Cross-reference tables for DIN aluminium wrought alloys: Part 1 |
|
|
|
|
|
DIN 1788
Sheet and strip of wrought aluminum and aluminum alloys, with thickness from 0.021 to 0.350 mm,
mechanical properties
| Alphanumeric designation (Kurzzeichen)
|
Numeric designation (Werkstoff-nummer)
|
|
AI99,98R
|
W4
|
3.0385.10
|
|
|
F14
|
.32
|
|
Al99,5
|
W6
|
3.0255.10
|
|
|
W7
|
.10
|
|
|
F9
|
.24
|
|
|
F11
|
.26
|
|
|
G11
|
.27
|
|
|
F13
|
.30
|
|
|
G13
|
.31
|
|
|
F15
|
.32
|
|
|
F18
|
.34
|
|
Al99
|
W6
|
3.0205.10
|
|
|
W7
|
.10
|
|
|
W8
|
.10
|
|
|
F12
|
.26
|
|
|
F14
|
.30
|
|
|
F16
|
.32
|
|
|
F19
|
.34
|
|
AlFeSi
|
W8
|
3.0915.10
|
|
|
F11
|
.24
|
|
|
G11
|
.25
|
|
|
F13
|
.26
|
|
|
G13
|
.27
|
|
|
F15
|
.28
|
|
|
G15
|
.29
|
|
|
F17
|
.30
|
|
|
F20
|
.32
|
|
AlMnCu
|
W10
|
3.0517.10
|
|
|
G13
|
.25
|
|
|
F15
|
.26
|
|
|
G15
|
.27
|
|
|
F17
|
.28
|
|
|
G17
|
.29
|
|
|
F19
|
.30
|
|
AlMn0.5Mg0.5
|
W11
|
3.0505.10
|
|
|
G16
|
.25
|
|
|
F17
|
.26
|
|
|
G17
|
.27
|
|
|
F20
|
.28
|
|
|
G20
|
.29
|
|
|
F22
|
.30
|
|
|
F24
|
.32
|
|
AlMn1Mg0,5
|
W13
|
3.0525.10
|
|
|
G17
|
.25
|
|
|
G21
|
.31
|
|
|
F25
|
.32
|
|
AlMn1Mg1
|
W16
|
3.0526.10
|
|
|
F19
|
.24
|
|
|
G19
|
.25
|
|
|
F21
|
.26
|
|
|
G21
|
.27
|
|
|
F23
|
.28
|
|
|
G23
|
.29
|
|
|
F25
|
.30
|
|
|
G25
|
.31
|
|
|
F28
|
.32
|
|
AlMg1
|
W11
|
3.3315.10
|
|
|
G12
|
.25
|
|
|
F15
|
.26
|
|
|
G15
|
.27
|
|
|
F17
|
.28
|
|
|
F19
|
.30
|
|
|
F22
|
.32
|
|
AlMg2,5
|
W18
|
3.3523.10
|
|
|
G26
|
.29
|
|
|
F32
|
.34
|
|
AlMg3
|
W19
|
3.3535.10
|
|
|
F24
|
.26
|
|
|
G24
|
.27
|
|
|
F27
|
.28
|
|
|
G27
|
.29
|
|
|
F29
|
.30
|
|
|
G29
|
.31
|
|
|
F32
|
.32
|
|
AlMg4,5
|
G34
|
3.3345.31
|
|
|
F37
|
.32
|
|
|
G37
|
.33
|
DIN 1790
Wire of wrought aluminum and aluminum alloys; mechanical properties
|
Alphanumeric designation (Kurzzeichen)
|
Numeric designation (Werkstoff-nummer)
|
|
Al99,8R
|
W4
|
3.0385.10
|
|
|
F7
|
.26
|
|
|
F11
|
.30
|
|
Al99,9
|
W4
|
3.0305.10
|
|
|
F7
|
.26
|
|
|
F11
|
.30
|
|
Al99,8
|
W6
|
3.0285.10
|
|
|
F9
|
.26
|
|
|
F12
|
.30
|
|
Al99,5
|
W7
|
3.0255.10
|
|
|
F10
|
.26
|
|
|
F14
|
.30
|
|
Al99
|
W8
|
3.0205.10
|
|
|
F11
|
.26
|
|
|
F15
|
.30
|
|
Al99,9Mg0,5
|
W7
|
3.3308.10
|
|
|
F10
|
.26
|
|
|
F13
|
.30
|
|
Al99,9Mg1
|
W10
|
3.3318.10
|
|
|
F13
|
.26
|
|
|
F16
|
.30
|
|
Al99,85Mg0,5
|
W7
|
3.3307.10
|
|
|
F10
|
.26
|
|
|
F13
|
.30
|
|
Al99,85Mg1
|
W10
|
3.3317.10
|
|
|
F13
|
.26
|
|
|
F16
|
.30
|
|
AlMn
|
W10
|
3.0515.10
|
|
|
F13
|
.26
|
|
|
F16
|
.30
|
|
AlMg1
|
W10
|
3.3315.10
|
|
|
F14
|
.26
|
|
|
F19
|
.30
|
|
AlMg2Mn0,3
|
W15
|
3.3525.10
|
|
|
F19
|
.24
|
|
|
F23
|
.28
|
|
|
G22
|
.29
|
|
AlMg2,5
|
W17
|
3.3523.10
|
|
|
F21
|
.24
|
|
|
F25
|
.28
|
|
|
G24
|
.29
|
|
AlMg3
|
W18
|
3.3535.10
|
|
|
F23
|
.24
|
|
|
F27
|
.28
|
|
|
G26
|
.29
|
|
AlMg5
|
W27
|
3.3555.10
|
|
|
F31
|
.26
|
|
|
F35
|
.30
|
|
|
G34
|
.31
|
|
AlMgsSi0,5
|
W9
|
3.3206.10
|
|
|
F12
|
.26
|
|
|
F15
|
.41
|
|
|
F20
|
.53
|
|
|
F22
|
.61
|
|
|
F27
|
.56
|
|
|
F30
|
.73
|
|
AlMgSi1
|
W11
|
3.2315.10
|
|
|
F15
|
.26
|
|
|
F20
|
.41
|
|
|
F25
|
.53
|
|
|
F28
|
.61
|
|
|
F32
|
73
|
|
AlCu2,5Mg0,5
|
F18
|
3.1305.26
|
|
|
F27
|
.41
|
|
|
F31
|
.53
|
|
AlCuMg1
|
F22
|
3.1325.26
|
|
|
F38
|
.41
|
|
|
F42
|
.53
|
|
AlCuMg2
|
F26
|
3.1355.26
|
|
|
F42
|
.41
|
|
|
F48
|
.53
|
|
AlZn4,5Mg1
|
F35
|
3.4335.61
|
|
AlZnMgCu0,5
|
F20
|
3.4345.26
|
|
|
F46
|
.46
|
|
AlZnMgCu1,5
|
F25
|
3.4365.26
|
|
|
F51
|
.61
|
|
|
F55
|
.73
|
|