Cross-reference tables for DIN aluminium wrought alloys: Part 2


Abstract:
Cross-reference tables between alphanumeric and numeric temper designations for wrought aluminum alloy according to DIN 1745, DIN 1746 and DIN 1747 standard specifications are given in this article. Here are described temper designations for plate, sheets and strips with thickness over 0.35mm, as well as rods, bars and tubes made of aluminum alloy.

DIN 1745

Plate, sheet and strip of wrought aluminum and aluminum alloys with thickness over 0,35mm

Alphanumeric designation (Kurzzeichen) Numeric designation
(Werkstoff-nummer)
Al99,8 W6 3.0285.10
F6 .07
F8 .24
G8 .25
F10 .26
F12 .30
F14 .32
Al99,7 W6 3.0275.10
F6 .07
F8 .24
G8 .25
F10 .26
F12 .30
F14 .32
Al99,5 W7 3.0255.10
W7 .10
F8 .07
F9 .24
G9 .25
F11 .26
G11 .27
F13 .30
G13 .31
F15 .32
Al99 W8 3.0205.10
W8 .10
F10 .24
G10 .25
F12 .26
F14 .30
F16 .32
AlRMg0,5 3.3309
Al99,9Mg0,5 3.3308
Al99,85Mg0,5 W8 3.3307.10
F10 .26
G10 .27
F12 .28
G12 .29
F14 .30
G14 .31
F16 .32
AlRMg1 3.3319
Al99,9Mg1 3.3318
Al99,85Mg1 W10 3.3317.10
F12 .24
G12 .25
F14 .26
G14 .27
F16 .30
G16 .31
F18 .32
AlFeSi W8 3.0915.10
F13 .26
G13 .27
F17 .30
F19 .32
AlMn W9 3.0515.10
F12 .24
F14 .26
F17 .30
F19 .32
F21 .34
AlMnCu W10 3.0517.10
F13 .24
F15 .26
F17 .28
F19 .30
AlMn1Mg1 W16 3.0526.10
F19 .24
G19 .25
F22 .26
G22 .27
F24 .28
G24 .29
F26 .30
G26 .31
AlMg1 W10 3.3315.10
F13 .24
G13 .25
F15 .26
G15 .27
F17 .28
G17 .29
F19 .30
G19 .31
F21 .32
AlMg1,5 W13 3.3316.10
F16 .24
G16 .25
F18 .26
G18 .27
F20 .28
G20 .29
F23 .30
G23 .31
F25 .32
AlMg2,5 W17 3.3523.10
F21 .24
G21 .25
F23 .26
G23 .27
F25 .28
G25 .29
F27 .30
G27 .31
AlMg3 W19 3.3535.10
W19 .10
F19 .07
F20 .07
F21 .07
F22 .24
G22 .25
F24 .26
G24 .27
F27 .28
G27 .29
F29 .30
G29 .31
AlMg2Mn0,3 W16 3.3525.10
F19 .24
G19 .25
F21 .26
G21 .27
F23 .28
G23 .29
F26 .30
G26 .31
AlMg2Mn0,8 W19 3.3527.10
W19 .10
F19 .07
F20 .07
F21 .07
F22 .24
G22 .25
F24 .26
G24 .27
F27 .28
G27 .29
F29 .30
G29 .31
AlMg2,7Mn F22 3.3537.07
F22 .07
G25 .25
G25 .25
G27 .27
G27 .27
AlMg4Mn W24 3.3545
W24 .10
F24 .07
F28 .24
G28 .25
F30 .26
G30 .27
F33 .28
G33 .29
F35 .30
AlMg4,5Mn W28 3.3547.10
F27 .07
G31 .25
G35 .27
AlMgSi0,8 F20 3.2316.51
F28 .71
AlMgSi1 W 3.2315.10
F21 .51
F21 .51
F28 .71
F28 .71
F32 .72
F30 .72
F30 .72
AlCu2Mg0,5 F27 3.1303.51
AlCuMg1 W 3.1325.10
F40 .51
F39 .51
F39 .51
AlCuMg2 W 3.1355.10
F44 .51
AlCuSiMn W 3.1255.10
F40 .51
F40 .51
F39 .51
F46 .71
AlZn4,5Mg1 F35 3.4335.71
F34 .71
AlZnMgCu0,5 F45 3.4345.71
F45 .71
F43 .71
F41 .71
AlZnMgCu1,5 F53 3.4365.71
F53 .71
F53 .71
F50 .71
F48 .71
F48 .71

DIN 1746

Tubes of wrought aluminium and aluminium alloy; mechanical properties

Alphanumeric designation (Kurzzeichen) Numeric designation
(Werkstoff-nummer)
Al99,8 F6 3.0285.08
W6 .10
F9 .26
F11 .30
Al99,5 F7 3.0255.08
W7 .10
F10 .26
F13 .30
Al99 F8 3.0205.08
W8 .10
F11 .26
F14 .30
Al99,85Mg0,5 F7 3.3307.08
Al99,85Mg1 F10 3.3317.08
AlMn F10 3.0515.08
W10 .10
F13 .26
F16 .28
AlMg1 F10 3.3315.08
W10 .10
F14 .26
F19 .30
AlMg1,8 F15 3.3326.08
W15 .10
F18 .26
F22 .30
AlMg3 F18 3.3535.08
W18 .10
F25 .26
AlMg5 F25 3.555.08
W25 .10
F28 .26
AlMg2Mn0,3 F15 3.3525.08
W15 .10
F20 .26
F24 .30
AlMg2Mn0,8 F20 3.3527.08
W18 .10
F25 .26
AlMg4,5Mn F27 3.3547.08
W27 .10
AlMgSi0,5 F13 3.206.51
F22 .71
F25 .72
AlMgSi0,8 F28 3.2316.71
AlMgSi1 F21 2.2315.51
F28 .71
F31 .72
AlMgSiPb F20 3.0615.51
F28 .71
AlCuBiPb F31 3.1655.51
F29 .51
F37 .71
AlCuMgPb F37 3.1645.51
F36 .51
AlCuMg1 F38 3.1325.51
F39 .51
F37 .51
AlCuMg2 F41 3.1355.51
F43 .51
F42 .51
AlCuSiMn F45 3.1255.71
AlZn4,5Mg1 F35 3.4335.71
AlZnMgCu0,5 F47 3.4345.71
AlZnMgCu1,5 F51 3.4365.71

DIN 1747

Rods and bars of wrought aluminium and aluminium alloys; mechanical properties

Alphanumeric designation (Kurzzeichen) Numeric designation
(Werkstoff-nummer)
Al99,8 F6 3.0285.08
W6 .10
F9 .26
F11 .30
Al99,5 F7 3.0255.08
W7 .10
F10 .26
F13 .30
Al99 F8 3.0205.08
W8 .10
F11 .26
F14 .30
AlMn F10 3.0515.08
W10 .10
F13 .26
F16 .28
AlMg1 F10 3.3315.08
W10 .10
F14 .26
F19 .30
AlMg3 F18 3.3535.08
W18 .10
F25 .26
AlMg5 F25 3.555.08
W25 .10
F26 .24
F28 .26
AlMg2Mn0,3 F15 3.3525.08
W15 .10
F20 .26
F24 .30
AlMg2Mn0,8 F20 3.3527.08
W18 .10
F25 .26
AlMg4,5Mn F27 3.3547.08
W27 .10
AlMgSi0,5 F13 3.206.51
F22 .71
F25 .72
AlMgSi0,8 F28 3.2316.71
AlMgSi1 F21 2.2315.51
F28 .71
F31 .72
F30 .72
F27 .72
AlMgSiPb F20 3.0615.51
F28 .71
AlCuBiPb F32 3.1655.51
F30 .51
F28 .51
F37 .71
AlCuMgPb F37 3.1645.51
F34 .51
AlCuMg1 F38 3.1325.51
F40 .51
F36 .51
F33 .51
AlCuMg2 F44 3.1355.51
F47 .51
F40 .51
AlCuSiMn F45 3.1255.71
F46 .71
F43 .71
AlZn4,5Mg1 F35 3.4335.71
AlZnMgCu0,5 F46 3.4345.71
F49 .71
F47 .71
AlZnMgCu1,5 F51 3.4365.71
F52 .71
F51 .71
F50 .71


Date Published: Jul-2002




The KEY to METALS database brings global metal properties together into one integrated and searchable database. Quick and easy access to the mechanical properties, chemical composition, cross-reference tables, and more provide users with an unprecedented wealth of information. Click the buttons below to learn more from the Guided Tour or to test drive the KEY to METALS database.