ASTM specifications represent a consensus among producers, specifiers, fabricators, and users of steel mill products. ASTM’s designation system for metals consists of a letter (A for ferrous materials) followed by an arbitrary sequentially assigned number. These designations often apply to specific products, for example A548 is applicable to cold-heading quality carbon steel wire for tapping or sheet metal screws.

This article contains a list of standards that covers among other things:

  • Metallic coated carbon steel wire coated at size for mechanical springs
  • Composite ribbed steel pipe, pre-coated and polyethylene lined sewer pipe application
  • Flexible poly (vinyl chloride) (PVC) gaskets used in connection of water closets to sanitary drainage system

For more information on the ASTM designation system see our related article:
Introduction to the ASTM Standard Designation.

Coated steels


Standard
Number
Last
version
Description Status
A 53/A 53M 2007 Pipe, Steel, Black and Hot-Dipped, Zinc-Coated, Welded and Seamless /5/
A 93   Zinc-Coated Galvanized Iron or Steel Sheets, Boils, and Butt Lengths Replaced by A 525 /no materials/
A 111 2004 Zinc-Coated (Galvanized) "Iron" Telephone and Telegraph Line Wire /no materials/
A 112   Zinc-Coated (Galvanized) Steel Tie wires Withdrawn 1990 /no materials/
A 116 2005 Metallic-Coated, Steel Woven Wire Fence Fabric /no materials/
A 117 1956 Zinc-Coated Iron or Steel Chain-Link Fence Fabric Galvanized After Wearing Replaced by A392 /no materials/
A 118   Zinc-Coated Iron or Steel Chain-Link Fence Fabric Galvanized Before Wearing Withdrawn 1933 /no materials/
A 120 1984 Pipe, Steel, Black and Hot-Dipped Zinc-Coated (Galvanized) Welded and Seamless for Ordinary Uses Withdrawn 1987 /no materials/
A 121 2007 Metallic-Coated Carbon Steel Barbed Wire /no materials/
A 122   Zinc-Coated Steel Wire Strand (Galvanized) and Class A Extra Galvanized Withdrawn 1963 /no materials/
A 123/A 123M 2009 Zinc (Hot-Dip Galvanized) Coatings on Iron and Steel Products /no materials/
A 143/A 143M 2007 Standard Practice for Safeguarding Against Embrittlement of Hot-Dip Galvanized Structural Steel Products and Procedure for Detecting Embrittlement /no materials/
A 153/A 153M 2009 Zinc Coating (Hot-Dip) on Iron and Steel Hardware /no materials/
A 163   Zinc-Coated (Galvanized) Wrought Iron Sheets Withdrawn 1972 /no materials/
A 164   Electrodeposited Coatings of Zinc on Steel Replaced by B 633 /no materials/
A 165   Electrodeposited Coatings of Cadmium on Steel Replaced by B 766 /no materials/
A 166   Electrodeposited Coatings of Nickel and Chromium on Steel Replaced by B 456 /no materials/
A 218   Zinc-Coated Steel Wire Strand (Class B and Class C Coatings) Replaced by A 475 /no materials/
A 239 2009 Standard Practice for Locating the Thinnest Spot in a Zinc (Galvanized) Coating on Iron or Steel Articles /no materials/
A 267   Lead Coating (Hot-Dip) on Iron or Steel Hardware Withdrawn 1954 /no materials/
A 308/A 308M 2006 Steel Sheet, Terne (Lead-Tin Alloy) Coated by the Hot-Dip Process /22/
A 326   Zinc-Coated (Galvanized) High Tensile Steel Telephone and Telegraph Line Wire Withdrawn 1990 /no materials/
A 337   Zinc-Coated Iron or Steel Chain-link Fence Fabric Galvanized before Weaving Replaced by A 392 /no materials/
A 361/A 361M 1994 Steel Sheet, Zinc-Coated (Galvanized) by the Hot-Dip Process for Roofing and Siding Withdrawn 1995 /no materials/
A 363 2003 Zinc-Coated (Galvanized) Steel Overhead Ground Wire Strand /no materials/
A 384/A 384M 2007 Standard Practice for Safeguarding Against Warpage and Distortion During Hot-Dip Galvanizing of Steel Assemblies /no materials/
A 385 2009 Standard Practice for Providing High-Quality Zinc Coatings (Hot-Dip) /no materials/
A 386   Zinc Coating (Hot-Dip) on Assembled Steel Products Replaced by A 123/A123M /no materials/
A 387/A 387M 2006 Pressure Vessel Plates, Alloy Steel, Chromium-Molybdenum /18/
A 390 2006 Zinc-Coated (Galvanized) Steel Poultry Fence Fabric (Hexagonal and Straight Line) /no materials/
A 392 2007 Zinc-Coated Steel Chain-Link Fence Fabric /no materials/
A 394 2008 Steel Transmission Tower Bolts, Zinc-Coated and Bare /1/
A 411 2008 Standard Specification for Zinc-Coated (Galvanized) Low-Carbon Steel Armor Wire /no materials/
A 444/A 444M 1989 Steel Sheet, Zinc-Coated (Galvanized) by the Hot-Dip Process for Storm Sewer and Drainage Pipe Replaced by A 929/A 929M /no materials/
A 446/A 446M 1993 Steel Sheet, Zinc-Coated (Galvanized) by the Hot-Dip Process, Structural (Physical) Quality Replaced by A 653/A 653M /7/
A 459 2008 Zinc-Coated Flat Steel Armoring Tape /1/
A 463/A 463M 2009 Steel Sheet, Aluminum-Coated, by the Hot-Dip Process /27/
A 464   Recommended Practice for Use of Magnetic Type Instruments for Measurement of Thickness of Hot-Dip Zinc Coatings on Iron and Steel Replaced by A 376/A 376M /no materials/
A 474 2008 Aluminum-Coated Steel Wire Strand /no materials/
A 475 2003 Zinc-Coated Steel Wire Strand /no materials/
A 491 2007 Aluminum-Coated Steel Chain-Link Fence Fabric /no materials/
A 525 1993 General Requirements for Steel Sheet, Zinc-Coated (Galvanized) by the Hot-Dip Process Replaced by A 653/A 653M /no materials/
A 525M 1991 General Requirements for Steel Sheet, Zinc-Coated (Galvanized) by the Hot-Dip Process (Metric) Replaced by A 653/A 924 /no materials/
A 526/A 526M 1990 Steel Sheet, Zinc-Coated (Galvanized) by the Hot-Dip Process, Commercial Quality Replaced by A 653/A 653M /1/
A 527/A 527M 2001 Steel Sheet, Zinc-Coated (Galvanized) by the Hot-Dip Process, Lock-Forming Quality Replaced by A 653/A 653M
A 528/A 528M 1990 Steel Sheet, Zinc-Coated (Galvanized) by the Hot-Dip Process Drawing Quality Replaced by A 653/A 653M /1/
A 562/A 562M 2006 Pressure Vessel Plates, Carbon Steel, Manganese-Titanium for Glass or Diffused Metallic Coatings /1/
A 584 1997 Aluminum-Coated Steel Woven Wire Fence Fabric Replaced by A 116 /no materials/
A 585 2002 Aluminum-Coated Steel Barbed Wire /no materials/
A 586 2009 Zinc-Coated Parallel and Helical Steel Wire Structural Strand /3/
A 591/A 591M 1998 Steel Sheet, Electrolytic Zinc-Coated, for Light Coating Weight [Mass] Applications Replaced by A 879 /60/
A 599/A 599M 2007 Tin Mill Products, Electrolytic Tin-Coated, Cold-Rolled Sheet /no materials/
A 603 2009 Zinc-Coated Steel Structural Wire Rope /3/
A 623 2008 Tin Mill Products, General Requirements /no materials/
A 623M 2009 Tin Mill Products, General Requirements [Metric] /3/
A 624/A 624M 2008 Tin Mill Products, Electrolytic Tin Plate, Single Reduced /no materials/
A 625/A 625M 2008 Tin Mill Products, Black Plate, Single Reduced /no materials/
A 625M 1985 Tin Mill Products, Black Plate, Single Reduced. (Metric) Replaced by A 625/A 625M /no materials/
A 626/A 626M 2008 Tin Mill Products, Electrolytic Tin Plate, Double Reduced /no materials/
A 640 2009 Zinc-Coated Steel Strand for Messenger Support of Figure 8 Cable /no materials/
A 641/A 641M 2009 Zinc-Coated (Galvanized) Carbon Steel Wire /3/
A 642/A 642M   Steel Sheet, Zinc-Coated (Galvanized) by the Hot Dip Process, Drawing Quality, Special Killed Replaced by A 653/A 653M /no materials/
A 650/A 650M 2008 Tin Mill Products, Black Plate, Double Reduced /no materials/
A 653/A 653M 2009 Steel Sheet, Zinc-Coated (Galvanized) or Zinc-Iron Alloy-Coated (Galvannealed) by the Hot-Dip Process /72/
A 657/A 657M 2008 Tin Mill Products, Black Plate Electrolytic Chromium-Coated, Single and Double Reduced /no materials/
A 676 1972 Hot-Dipped Aluminum Coatings on Ferrous Articles Withdrawn 1987 /no materials/
A 741 2009 Zinc-Coated Steel Wire Rope and Fittings for Highway Guardrail /no materials/
A 742/A 742M 2008 Steel Sheet, Metallic Coated and Polymer Precoated for Corrugated Steel Pipe /no materials/
A 755/A 755M 2008 Steel Sheet, Metallic Coated by the Hot-Dip Process and Prepainted by the Coil-Coating Process for Exterior Exposed Building Products /no materials/
A 760/A 760M 2009 Corrugated Steel Pipe, Metallic-Coated for Sewers and Drains /no materials/
A 761/A 761M 2009 Corrugated Steel Structural Plate, Zinc-Coated, for Field-Bolted Pipe, Pipe-Arches, and Arches /no materials/
A 762/A 762M 2008 Corrugated Steel Pipe, Polymer Precoated for Sewers and Drains /no materials/
A 764 2007 Metallic Coated Carbon Steel Wire, Coated at Size and Drawn to Size for Mechanical Springs /1/
A 767/A 767M 2009 Zinc-Coated (Galvanized) Steel Bars for Concrete Reinforcement /no materials/
A 775/A 775M 2007 Epoxy-Coated Steel Reinforcing Bars /no materials/
A 780 2009 Standard Practice for Repair of Damaged and Uncoated Areas of Hot-Dip Galvanized Coatings /no materials/
A 783 1981 Aluminum-Zinc-Alloy-Coated Steel Chain Link Fence Fabric Withdrawn 1986 /no materials/
A 784 1981 Aluminum-Zinc Alloy-Coated Steel Wire Rope and Fittings for Highway Guard Rail Withdrawn 1987 /no materials/
A 785 1981 Aluminum-Zinc Alloy-Coated Wire Strand Withdrawn 1987 /no materials/
A 787 2009 Electric-Resistance-Welded Metallic-Coated Carbon Steel Mechanical Tubing /13/
A 791/A 791M 1994 Aluminum-Zinc Alloy-Coated Wire Strand Replaced by A268/A268M /10/
A 792/A 792M 2009 Steel Sheet, 55 % Aluminum-Zinc Alloy-Coated by the Hot-Dip Process /28/
A 792M 1993 Steel Sheet, 55% Aluminum-Zinc Alloy-Coated by the Hot Dip Process, General Requirements (Metric) Replaced by A792/A792M /no materials/
A 795/A 795M 2008 Black and Hot-Dipped Zinc-Coated (Galvanized) Welded and Seamless Steel Pipe for Fire Protection Use /2/
A 797 1982 Aluminum-Zinc Alloy-Coated Steel Overhead Ground Wire Strand Withdrawn 1990 /no materials/
A 809 2008 Aluminum-Coated (Aluminized) Carbon Steel Wire /1/
A 810 2009 Zinc-Coated (Galvanized) Steel Pipe Winding Mesh /no materials/
A 816/A 816M 1991 Steel Sheet, Zinc-Coated (Galvanized) by the Hot-Dip Process, High-Strength, Low Alloy Replaced by A653/A654M /no materials/
A 817 2007 Metallic-Coated Steel Wire for Chain-Link Fence Fabric and Marcelled Tension Wire /no materials/
A 819 1990 Steel Sheet, Aluminum-Coated Type 2 for Storm Sewer and Drainage Pipe Replaced by A929/A929M /no materials/
A 824 2007 Metallic-Coated Steel Marcelled Tension Wire for Use With Chain Link Fence /no materials/
A 825 1984 Steel Sheet, Composite Coated for Corrugated Steel Sewer Pipe and Bin Type Retaining Walls Withdrawn 1990
A 849 2005 Post-Applied Coatings, Pavings, and Linings for Corrugated Steel Sewer and Drainage Pipe /no materials/
A 854/A 854M 2008 Metallic-Coated Steel Smooth High-Tensile Fence and Trellis Wire /no materials/
A 855/A 855M 2009 Zinc-5% Aluminum-Mischmetal Alloy-Coated Steel Wire Strand /no materials/
A 856/A 856M 2003 Zinc-5% Aluminum-Mischmetal Alloy-Coated Carbon Steel Wire /3/
A 862/A 862M 2008 Standard Practice for Application of Asphalt Coatings to Corrugated Steel Sewer and Drainage Pipe /no materials/
A 863 1986 Corrugated Steel Pipe with Smooth PVC Liner for Seweres and Drains Withdrawn 1990 /no materials/
A 865/A 865M 2006 Threaded Couplings, Steel, Black or Zinc-Coated (Galvanized) Welded or Seamless, for Use in Steel Pipe Joints /1/
A 875/A 875M 2009 Steel Sheet, Zinc-5 % Aluminum Alloy-Coated by the Hot-Dip Process /22/
A 879/A 879M 2006 Steel Sheet, Zinc Coated by the Electrolytic Process for Applications Requiring Designation of the Coating Mass on Each Surface /no materials/
A 882/A 882M 2004 Filled Epoxy-Coated Seven-Wire Prestressing Steel Strand /no materials/
A 884/A 884M 2006 Epoxy-Coated Steel Wire and Welded Wire Reinforcement /no materials/
A 885/A 885M 2002 Steel Sheet, Zinc and Aramid Fiber Composite Coated for Corrugated Steel Sewer, Culvert, and Underdrain Pipe Withdrawn 2005 /no materials/
A 899 2007 Steel Wire, Epoxy-Coated /no materials/
A 916 1993 Steel Sheet, Zinc-5% Aluminum-Mischmetal Alloy-Coated by Hot-Dip Process for Storm Sewer and Drainage Pipe Replaced by A929/A929M /no materials/
A 917 2008 Steel Sheet, Coated by the Electrolytic Process for Applications Requiring Designation of the Coating Mass on Each Surface (General Requirements) /no materials/
A 918 2006 Steel Sheet, Zinc-Nickel Alloy Coated by the Electrolytic Process for Applications Requiring Designation of the Coating Mass on Each Surface /no materials/
A 924/A 924M 2009 General Requirements for Steel Sheet, Metallic-Coated by the Hot-Dip Process /no materials/
A 925 2009 Zinc-5% Aluminum-Mischmetal Alloy-Coated Steel Overhead Ground Wire Strand /no materials/
A 929/A 929M 2007 Steel Sheet, Metallic-Coated by the Hot-Dip Process for Corrugated Steel Pipe /1/
A 933/A 933M 2007 Vinyl (PVC) Coated Steel Wire and Welded Wire Fabric for Reinforcement /no materials/
A 934/A 934M 2007 Epoxy-Coated Prefabricated Steel Reinforcing Bars /no materials/
A 950/A 950M 2007 Fusion Bonded Epoxy-Coated Structural Steel H-Piles and Sheet Piling /no materials/
A 972/A 972M 2004 Fusion Bonded Epoxy-Coated Pipe Piles /no materials/
A 974 2003 Welded Wire Fabric Gabions and Gabion Mattresses (Metallic Coated or Polyvinyl Chloride (PVC) Coated) /no materials/
A 975 2003 Double-Twisted Hexagonal Mesh Gabions and Revet Mattresses (Metallic-Coated Steel Wire or Metallic-Coated Steel Wire With Poly(Vinyl Chloride) (PVC) Coating) /no materials/
A 976 2008 Standard Classification of Insulating Coatings by Composition, Relative Insulating Ability and Application /no materials/
A 978/A 978M 2008 Composite Ribbed Steel Pipe, Precoated and Polyethylene Lined for Gravity Flow Sanitary Sewers, Storm Sewers, and Other Special Applications /no materials/
A 1003/A 1003M 2009 Steel Sheet, Carbon, Metallic- and Nonmetallic-Coated for Cold-Formed Framing Members /3/
A 1004/A 1004M 2004 Standard Practice for Establishing Conformance to the Minimum Expected Corrosion Characteristics of Metallic, Painted-Metallic, and Nonmetallic-Coated Steel Sheet Intended for Use as Cold Formed Framing Members /no materials/
A 1019/A 1019M 2007 Closed Rib Steel Pipe with Diameter of 36 in. [900 mm] or Less, Polymer Precoated for Sewers and Drains /1/
A 1045 2008 Flexible Poly (Vinyl Chloride) (PVC) Gaskets used in Connection of Water Closets to Sanitary Drainage System /no materials/
A 1046/A 1046M 2006 Steel Sheet, Zinc-Aluminum-Magnesium Alloy-Coated by the Hot-Dip Process /25/
A 1055 2008 Standard Specification for Zinc and Epoxy Dual-Coated Steel Reinforcing Bars /no materials/
A 1057/A 1057M 2008 Standard Specification for Steel, Structural Tubing, Cold Formed, Welded, Carbon, Zinc-Coated (Galvanized) by the Hot-Dip Process /no materials/
A 1059/A 1059M 2008 Standard Specification for Zinc Alloy Thermo-Diffusion Coatings (TDC) on Steel Fasteners, Hardware, and Other Products /no materials/
B 606 2008 Standard Specification for High-Strength Zinc-Coated (Galvanized) Steel Core Wire for Aluminum and Aluminum-Alloy Conductors, Steel Reinforced  
B 802/B 802M 2008 Standard Specification for Zinc–5 % Aluminum-Mischmetal Alloy-Coated Steel Core Wire for Aluminum Conductors, Steel Reinforced (ACSR)  
B 803 2008 Standard Specification for High-Strength Zinc–5 % Aluminum-Mischmetal Alloy-Coated Steel Core Wire for Use in Overhead Electrical Conductors  

ابحث في قاعدة معلومات

ادخل عبارة لتبحث عنها:

بحث بِـ:

الوثيقة الكاملة
الكلمات المفاتيح

ترويسات
خلاصات

With Total Materia finding information about a metal standard specification, its current status and the materials it defines is one click away.

Within seconds it is also possible for you to find related detailed material property data or search equivalent materials starting from the Total Materia standard list.

To get started, click on the standard list button in the menu bar.

solution img

By simply selecting a Standard Development Organization (SDO) and/or typing the standard number, you receive immediate results from the multi-lingual database containing over 30,000 standards.

For example, you can review all metal standards from ASTM by selecting this SDO from the popup.

solution img

The result list consists of over 3000 ASTM metal standards. Information includes: standard description, year of last issue, current status (valid, replaced, etc.) and a hot link to the materials defined by this standard.

solution img

By simply clicking the materials hot link, you can see a list of metal materials defined by the selected standard.

solution img

From the list of materials, you can review detailed properties and equivalents of each material.

solution img

For you’re a chance to take a test drive of the Total Materia database, we invite you to join a community of over 150,000 registered users through the Total Materia Free Demo.