PN/H standards for steel materials

خلاصات:

This group of PN standard specifications covers carbon and alloy steels, plates and forgings used in boilers and pressure vessels, high-strength low-alloy steels, heat-treatable steels, sheets and strips. This article contains standards for various types of steel pipes which specify requirements for high-temperature service, and special applications such as fire protection use. Steel casting and high temperature cast steel specifications call out the standard properties for pressure purposes. The group of standards for tool steels, stainless and heat resisting steels is also presented.

Review of PH/N Standards for steel consists of 3 volumes. It contains formally approved PH/N standard classifications, guides, practices, specifications, test methods and terminology and related material such as proposals.

Covers:

The following data is given for each standard: standard number, grade, chemical composition and mechanical properties (yield point, tensile strength, notch toughness). When deemed useful, steel type, manufacturing method, thickness of plate, heat treatment and other data are described.

This group of PN standard specifications covers carbon and alloy steels, plates and forgings used in boilers and pressure vessels, high-strength low-alloy steels, heat-treatable steels, sheets and strips. This article contains standards for various types of steel pipes which specify requirements for high-temperature service, and special applications such as fire protection use. Steel casting and high temperature cast steel specifications call out the standard properties for pressure purposes. The group of standards for tool steels, stainless and heat resisting steels is also presented.

Group of standards for structural and constructional steels

PN/H 74231 Drill tubes (small gauges)
PN/H 74235 Drill tubes
PN/H 74244 Welded tubes
PN/H 83152 Unalloyed cast steel for construction
PN/H 83156 Alloyed cast steel
PN/H 83157 High temperature cast steel
PN/H 83160 Wear-resistant cast steel
PN/H 84016 Semi killed low alloy high strength steels
PN/H 84017 Steels resistant to weathering
PN/H 84018 High strength low alloy steels
PN/H 84019 Quality carbon steels for general use
PN/H 84020 Unalloyed steels for general use
PN/H 84023 Steels for special purposes
PN/H 84023/02 Low carbon soft magnetic steels
PN/H 84023/03 Low carbon steels for sheet and strip
PN/H 84023/04 Low carbon steels
PN/H 84023/05 Low alloy and alloyed high-quality steels
PN/H 84023/06 Concrete steels
PN/H 84023/07 Steels for tubes
PN/H 84023/08 Chainsteels
PN/H 84023/09 Steel for gas cylinders
PN/H 84024 High-temperature steels
PN/H 84026 Free-cutting
PN/H 84027 Railway steel
PN/H 84027/01 Wheel discs
PN/H 84027/02 Forged pieces
PN/H 84027/03 Axle-trees
PN/H 84027/04 Forged pieces
PN/H 84027/06 Railway tyres
PN/H 84027/07 Rails for normal width
PN/H 84027/08 Rolled section for railway equipment
PN/H 84028 Unalloyed wire rod for drawing
PN/H 84030/02 Alloyed case hardening steels
PN/H 84030/03 Nitriding steels
PN/H 84030/04 Heat-treatable steels
PN/H 84032 Spring steels
PN/H 84035 For highly stressed machine-parts
PN/H 84041 Roller bearing steels
PN/H 91042 Crude wheel tyres
PN/H 91044 Unmachined wheel tyres
PN/H 91046 Axle-trees for vehicles to be pulled
PN/H 92147 Shipbuilding plates
PN/H 92149 Steels resistant to weathering
PN/H 92602 Unalloyed wire rod for spring wire
PN/H 93027 Rolled bars and wire rod for mine-chains
PN/H 93028 Bars and wire rods for mine-chains
PN/H 93421 Railway rails (normal widths)
PN/H 93440 Steel for tramway rails
PN/H 94010 Forging steel for aviation
PN/H 69420 Filler rod
PN/H 69420 Filler rod

Group of standards for tool steels

PN/H 83161 Tool steel for castings
PN/H 85020 Carbon tool steels
PN/H 85021 Alloyed hot work tool steels
PN/H 85022 Carbon tool steels
PN/H 85023 Cold work tool steels

Group of standards for stainless and heat resisting steels

PN/H 83158 Corrosion-resisting cast steel
PN/H 83159 Heat-resisting cast steel
PN/H 84038 For hard magnetic bars
PN/H 86020 Stainless steels
PN/H 86022 Heat-resisting steels
PN/H 87045 Nickel alloys
PN/H 87047 Soft magnetic Ni-Fe and Co-Fe alloys
PN/H 92133 Soft magnetic steel, hot rolled sheet and strip
PN/H 92336 Strip of steel- and nickel alloys with high electric resistor
PN/H 92610 Steels and nickel alloys with high electric resistor

ابحث في قاعدة معلومات

ادخل عبارة لتبحث عنها:

بحث بِـ:

الوثيقة الكاملة
الكلمات المفاتيح

ترويسات
خلاصات

With Total Materia finding information about a metal standard specification, its current status and the materials it defines is one click away.

Within seconds it is also possible for you to find related detailed material property data or search equivalent materials starting from the Total Materia standard list.

To get started, click on the standard list button in the menu bar.

solution img

By simply selecting a Standard Development Organization (SDO) and/or typing the standard number, you receive immediate results from the multi-lingual database containing over 30,000 standards.

For example, you can review all metal standards from UNI by selecting this SDO from the popup.

solution img

The result list consists of over 1400 UNI metal standards. Information includes: standard description, year of last issue, current status (valid, replaced, etc.) and a hot link to the materials defined by this standard.

solution img

By simply clicking the materials hot link, you can see a list of metal materials defined by the selected standard.

solution img

From the list of materials, you can review detailed properties and equivalents of each material.

solution img

For you’re a chance to take a test drive of the Total Materia database, we invite you to join a community of over 150,000 registered users through the Total Materia Free Demo.