UNE standards for steel materials

خلاصات:

This group of UNE standard specifications covers carbon and alloy steels, plates for boilers and other pressure vessels, sheets and strips, high-strength low-alloy steels, heat-treatable steels, hot and cold-rolled plates for cold forming, and non-alloy steels. Steel casting specifications call out the standard properties for pressure purposes. The group of standards for tool steels, stainless and heat resisting steels is also presented.

Review of UNE Standards for steel consists of 3 volumes. It contains formally approved UNE standard classifications, guides, practices, specifications, test methods and terminology and related material such as proposals.

Covers:

The following data is given for each standard: standard number, grade, chemical composition and mechanical properties (yield point, tensile strength, notch toughness). When deemed useful, steel type, manufacturing method, thickness of plate heat treatment and other data are described.

This group of UNE standard specifications covers carbon and alloy steels, plates for boilers and other pressure vessels, sheets and strips, high-strength low-alloy steels, heat-treatable steels, hot and cold-rolled plates for cold forming, and non-alloy steels. Steel casting specifications call out the standard properties for pressure purposes. The group of standards for tool steels, stainless and heat resisting steels is also presented.

Group of standards for structural and constructional steels

UNE 36013-76 Cementation steels
UNE 36014-75 Nitriding steels
UNE 36015-77 Spring steels
UNE 36021-80 Free-cutting steels
UNE 36027-86 Ball and roller bearing steels
UNE 36032-85 Steels for bolts
UNE 36034-85 Cold heading and cold extruding
UNE 36051-91(1) Heat-treatable steels
UNE 36051-91(2) Heat-treatable steels
UNE 36080-90 Non-alloy steels
UNE 36081-76 Fine grained structural steels
UNE 36082-84 Resistant to weathering
UNE 36084-79 Steels for shipbuilding
UNE 36086-91 Cold rolled flat products for cold forming
UNE 36087-74 Sheets
UNE 36087-76/78 Sheet and strip
UNE 36121-85 Cold rolled strip
UNE 36123-90 Hot rolled strip
UNE 36129-89(1) Steel plate for welded gas cylinders
UNE 36253-71 Steel casting
UNE 36254-79 Steel casting
UNE 36255-79 Steel casting
UNE 36256-73 Steel casting
UNE 36259-79 Steel casting

Group of standards for tool steels

UNE 36071 1975 Carbon tool steels
UNE 36072(1) 1975 Alloyed cold work steels
UNE 36072(2) 1975 Alloyed hot work steels
UNE 36073 1975 High speed steels

Group of standards for stainless and heat resisting steels

UNE 36016-89(1) Bars, wire and forged pieces
UNE 36016-89(2) Flat rolled products
UNE 36017-85 Heat-resisting steels
UNE 36022-91 Valve steels
UNE 36087-89/4 Sheet and strip
UNE 36257-74 Stainless steel castings
UNE 36258-74 Heat-resisting steel castings

ابحث في قاعدة معلومات

ادخل عبارة لتبحث عنها:

بحث بِـ:

الوثيقة الكاملة
الكلمات المفاتيح

ترويسات
خلاصات

With Total Materia finding information about a metal standard specification, its current status and the materials it defines is one click away.

Within seconds it is also possible for you to find related detailed material property data or search equivalent materials starting from the Total Materia standard list.

To get started, click on the standard list button in the menu bar.

solution img

By simply selecting a Standard Development Organization (SDO) and/or typing the standard number, you receive immediate results from the multi-lingual database containing over 30,000 standards.

For example, you can review all metal standards from UNI by selecting this SDO from the popup.

solution img

The result list consists of over 1400 UNI metal standards. Information includes: standard description, year of last issue, current status (valid, replaced, etc.) and a hot link to the materials defined by this standard.

solution img

By simply clicking the materials hot link, you can see a list of metal materials defined by the selected standard.

solution img

From the list of materials, you can review detailed properties and equivalents of each material.

solution img

For you’re a chance to take a test drive of the Total Materia database, we invite you to join a community of over 150,000 registered users through the Total Materia Free Demo.