ASTM specifications represent a consensus among producers, specifiers, fabricators, and users of steel mill products. ASTM’s designation system for metals consists of a letter (A for ferrous materials) followed by an arbitrary sequentially assigned number. These designations often apply to specific products, for example A548 is applicable to cold-heading quality carbon steel wire for tapping or sheet metal screws.

This article contains a list of standards that covers among other things:

  • Centrifugally Cast Austenitic Steel Pipe for High-Temperature Service
  • Various stainless steels specifically designed for use as springs
  • Stainless Steel Bars for Compressor and Turbine Airfoils

For more information on the ASTM designation system see our related article:
Introduction to the ASTM Standard Designation.



Stainless Steel

Standard
Number
Last
version
Description Status
A 167 2009 Stainless and Heat-Resisting Chromium-Nickel Steel Plate, Sheet, and Strip /42/
A 176 2009 Stainless and Heat-Resisting Chromium Steel Plate, Sheet, and Strip /31/
A 177   High-Strength Stainless and Chromium-Nickel Steel Sheet and Strip Replaced by A 666 /1/
A 193/A 193M 2009 Alloy-Steel and Stainless Steel Bolting Materials for High Temperature or High Pressure Service and Other Special Purpose Applications /58/
A 213/A 213M 2009 Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes /86/
A 225/A 225M 2007 Pressure Vessel Plates, Alloy Steel, Manganese-Vanadium-Nickel /2/
A 240/A 240M 2009 Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications /208/
A 249/A 249M 2008 Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes /87/
A 263 2009 Stainless Chromium Steel-Clad Plate /1/
A 264 2009 Stainless Chromium-Nickel Steel-Clad Plate /1/
A 270 2008 Seamless and Welded Austenitic Stainless Steel Sanitary Tubing /18/
A 271 1996 Seamless Austenitic Chromium-Nickel Steel Still Tubes for Refinery Service Replaced by A 213/A 213M /9/
A 276 2008 Stainless Steel Bars and Shapes /79/
A 296   Corrosion-Resistant Iron-Chromium and Iron-Chromium Nickel and Nickel-B Alloy Castings Replaced by A 743/A 743M /no materials/
A 298   Corrosion-Resistant Chromium and Chromium-Nickel Steel Covered Welding Electrodes Withdrawn 1970 /no materials/
A 299/A 299M 2004 Pressure Vessel Plates, Carbon Steel, Manganese-Silicon /2/
A 312/A 312M 2009 Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes /72/
A 313/A 313M 2008 Stainless Steel Spring Wire /20/
A 314 2008 Stainless Steel Billets and Bars for Forging /103/
A 320/A 320M 2008 Alloy-Steel and Stainless Steel Bolting Materials for Low-Temperature Service /39/
A 358/A 358M 2008 Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications /67/
A 368 2009 Stainless Steel Wire Strand /12/
A 371   Corrosion-Resisting Chromium and Chromium-Nickel Steel Welding Rods and Bare Electrodes Withdrawn 1969 /no materials/
A 376/A 376M 2000 Seamless Austenitic Steel Pipe for High-Temperature Central-Station Service /19/
A 380 2006 Standard Practice for Cleaning, Descaling, and Passivation of Stainless Steel Parts, Equipment, and Systems /no materials/
A 403/A 403M 2007 Wrought Austenitic Stainless Steel Piping Fittings /81/
A 409/A 409M 2008 Welded Large Diameter Austenitic Steel Pipe for Corrosive or High-Temperature Service /38/
A 412   Stainless and Heat-Resisting Chromium-Nickel-Manganese Steel Plate, Sheet, and Strip Withdrawn 1989 /7/
A 429   Hot- and Cold-Finished Bars of Stainless and Heat-Resisting Chromium-Nickel-Manganese Steel Replaced by A 276 /no materials/
A 451/A 451M 2006 Centrifugally Cast Austenitic Steel Pipe for High-Temperature Service /13/
A 452 1988 Centrifugally Cast Austenitic Steel Cold-Wrought Pipe for High-Temperature Service Withdrawn 1995 /3/
A 478 2008 Chromium-Nickel Stainless Steel Weaving and Knitting Wire /24/
A 479/A 479M 2008 Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels /80/
A 480/A 480M 2009 General Requirements for Flat-Rolled Stainless and Heat-Resisting Steel Plate, Sheet, and Strip /no materials/
A 484/A 484M 2009 General Requirements for Stainless Steel Bars, Billets, and Forgings /no materials/
A 492 2009 Stainless Steel Rope Wire /12/
A 493 2009 Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging /34/
A 511/A 511M 2008 Seamless Stainless Steel Mechanical Tubing /29/
A 554 2008 Welded Stainless Steel Mechanical Tubing /19/
A 555/A 555M 2009 General Requirements for Stainless Steel Wire and Wire Rods /no materials/
A 564/A 564M 2009 Hot-Rolled and Cold-Finished Age-Hardening Stainless Steel Bars and Shapes /21/
A 565/A 565M 2009 Martensitic Stainless Steel Bars for High-Temperature Service /11/
A 580/A 580M 2008 Stainless Steel Wire /79/
A 581/A 581M 2009 Free-Machining Stainless Steel Wire and Wire Rods /24/
A 582/A 582M 2005 Free-Machining Stainless Steel Bars /32/
A 632 2004 Seamless and Welded Austenitic Stainless Steel Tubing (Small-Diameter) for General Service /18/
A 651 1984 Stainless Steel Water-DWV Tube Withdrawn 1986 /7/
A 666 2003 Annealed or Cold-Worked Austenitic Stainless Steel Sheet, Strip, Plate, and Flat Bar /34/
A 669 1983 Seamless Ferritic-Austenitic Alloy Steel Tubes Replaced by A789/A789M /no materials/
A 688/A 688M 2008 Welded Austenitic Stainless Steel Feedwater Heater Tubes /22/
A 693 2006 Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip /25/
A 708 1979 Practice for Detection of Susceptibility to Intergranular Corrosion in Severely Sensitized Austenitic Stainless Steel Withdrawn 1988 /no materials/
A 731/A 731M   Seamless, Welded Ferritic, and Martensitic Stainless Steel Pipe Replaced by A268/A268M /7/
A 756 2009 Stainless Anti-Friction Bearing Steel /2/
A 771/A 771M 2001 Seamless Austenitic and Martensitic Stainless Steel Tubing for Liquid Metal-Cooled Reactor Core Components Withdrawn 2004 /3/
A 774/A 774M 2006 As-Welded Wrought Austenitic Stainless Steel Fittings for General Corrosive Service at Low and Moderate Temperatures /5/
A 778 2001 Welded, Unannealed Austenitic Stainless Steel Tubular Products /10/
A 789/A 789M 2008 Seamless and Welded Ferritic/Austenitic Stainless Steel Tubing for General Service /25/
A 790/A 790M 2009 Seamless and Welded Ferritic/Austenitic Stainless Steel Pipe /29/
A 793 2009 Rolled Floor Plate, Stainless Steel /4/
A 803/A 803M 2008 Welded Ferritic Stainless Steel Feedwater Heater Tubes /21/
A 813/A 813M 2009 Single- or Double-Welded Austenitic Stainless Steel Pipe /60/
A 814/A 814M 2008 Cold-Worked Welded Austenitic Stainless Steel Pipe /63/
A 815/A 815M 2009 Wrought Ferritic, Ferritic/Austenitic, and Martensitic Stainless Steel Piping Fittings /54/
A 826/A 826M 2001 Seamless Austenitic and Martensitic Stainless Steel Duct Tubes for Liquid Metal-Cooled Reactor Core Components Withdrawn 2004 /4/
A 831/A 831M 2000 Austenitic and Martensitic Stainless Steel Bars, Billets, and Forgings for Liquid Metal Cooled Reactor Core Components /4/
A 838 2007 Free-Machining Ferritic Stainless Soft Magnetic Alloy Bar for Relay Applications /5/
A 860/A 860M 2009 Wrought High-Strength Low-Alloy Steel Butt-Welding Fittings /6/
A 872/A 872M 2007 Centrifugally Cast Ferritic/Austenitic Stainless Steel Pipe for Corrosive Environments /4/
A 873/A 873M 1993 Steel Sheet and Strip, Chromium-Molybdenum Alloy, for Pressure Vessels Withdrawn 1997 /no materials/
A 887 2009 Borated Stainless Steel Plate, Sheet, and Strip for Nuclear Application /16/
A 895 2009 Free-Machining Stainless Steel Plate, Sheet, and Strip /16/
A 908 2008 Stainless Steel Needle Tubing /1/
A 928/A 928M 2008 Ferritic/Austenitic (Duplex) Stainless Steel Pipe Electric Fusion Welded with Addition of Filler Metal /15/
A 943/A 943M 2005 Spray-Formed Seamless Austenitic Stainless Steel Pipes /40/
A 947M 2004 Textured Stainless Steel Sheet [Metric] /no materials/
A 949/A 949M 2005 Spray-Formed Seamless Ferritic/Austenitic Stainless Steel Pipe /9/
A 953 2002 Austenitic Chromium-Nickel-Silicon Alloy Steel Seamless and Welded Tubing Withdrawn 2004 /1/
A 954 2002 Austenitic Chromium-Nickel-Silicon Alloy Steel Seamless and Welded Pipe Withdrawn 2005 /1/
A 955/A 955M 2009 Deformed and Plain Stainless-Steel Bars for Concrete Reinforcement /41/
A 959 2009 Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels /219/
A 967 2005 Chemical Passivation Treatments for Stainless Steel Parts /no materials/
A 988/A 988M 2007 Hot Isostatically-Pressed Stainless Steel Flanges, Fittings, Valves, and Parts for High Temperature Service /28/
A 989/A 989M 2007 Hot Isostatically-Pressed Alloy Steel Flanges, Fittings, Valves, and Parts for High Temperature Service /5/
A 999/A 999M 2004 General Requirements for Alloy and Stainless Steel Pipe /no materials/
A 1010/A 1010M 2009 Higher-Strength Martensitic Stainless Steel Plate, Sheet , and Strip /4/
A 1011/A 1011M 2009 Steel, Sheet and Strip, Hot-Rolled, Carbon, Structural, High-Strength Low-Alloy, High-Strength Low-Alloy with Improved Formability, and Ultra-High Strength /35/
A 1012 2007 Seamless and Welded Ferritic, Austenitic and Duplex Alloy Steel Condenser and Heat Exchanger Tubes With Integral Fins Withdrawn 2007 /no materials/
A 1016/A 1016M 2008 General Requirements for Ferritic Alloy Steel, Austenitic Alloy Steel, and Stainless Steel Tubes /no materials/
A 1022/A 1022M 2007 Deformed and Plain Stainless Steel Wire and Welded Wire for Concrete Reinforcement /1/
A 1023/A 1023M 2007 Stranded Carbon Steel Wire Ropes for General Purposes /no materials/
A 1024/A 1024M 2007 Steel Line Pipe, Black, Plain-End, Seamless /5/
A 1026 2003 Alloy Steel Structural Shapes for Use in Building Framing /2/
A 1028 2008 Stainless Steel Bars for Compressor and Turbine Airfoils /12/
A 1053/A 1053M 2006 Welded Ferritic-Martensitic Stainless Steel Pipe /1/
B 625 2005 Plate, sheet, and strip in the annealed temper /6/


Date Published: Apr-2011