ASTM Standard List: Stainless Steels


Abstrakt:
ASTM specifications represent a consensus among producers, specifiers, fabricators, and users of steel mill products. ASTM’s designation system for metals consists of a letter (A for ferrous materials) followed by an arbitrary sequentially assigned number. These designations often apply to specific products, for example A548 is applicable to cold-heading quality carbon steel wire for tapping or sheet metal screws.

This article contains a list of standards that covers among other things:

  • Centrifugally Cast Austenitic Steel Pipe for High-Temperature Service
  • Various stainless steels specifically designed for use as springs
  • Stainless Steel Bars for Compressor and Turbine Airfoils

For more information on the ASTM designation system see our related article:
Introduction to the ASTM Standard Designation.



Stainless Steel

Standard
Number
Last
version
Description Status
A 167 2009 Stainless and Heat-Resisting Chromium-Nickel Steel Plate, Sheet, and Strip /42/
A 176 2009 Stainless and Heat-Resisting Chromium Steel Plate, Sheet, and Strip /31/
A 177   High-Strength Stainless and Chromium-Nickel Steel Sheet and Strip Replaced by A 666 /1/
A 193/A 193M 2009 Alloy-Steel and Stainless Steel Bolting Materials for High Temperature or High Pressure Service and Other Special Purpose Applications /58/
A 213/A 213M 2009 Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes /86/
A 225/A 225M 2007 Pressure Vessel Plates, Alloy Steel, Manganese-Vanadium-Nickel /2/
A 240/A 240M 2009 Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications /208/
A 249/A 249M 2008 Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes /87/
A 263 2009 Stainless Chromium Steel-Clad Plate /1/
A 264 2009 Stainless Chromium-Nickel Steel-Clad Plate /1/
A 270 2008 Seamless and Welded Austenitic Stainless Steel Sanitary Tubing /18/
A 271 1996 Seamless Austenitic Chromium-Nickel Steel Still Tubes for Refinery Service Replaced by A 213/A 213M /9/
A 276 2008 Stainless Steel Bars and Shapes /79/
A 296   Corrosion-Resistant Iron-Chromium and Iron-Chromium Nickel and Nickel-B Alloy Castings Replaced by A 743/A 743M /no materials/
A 298   Corrosion-Resistant Chromium and Chromium-Nickel Steel Covered Welding Electrodes Withdrawn 1970 /no materials/
A 299/A 299M 2004 Pressure Vessel Plates, Carbon Steel, Manganese-Silicon /2/
A 312/A 312M 2009 Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes /72/
A 313/A 313M 2008 Stainless Steel Spring Wire /20/
A 314 2008 Stainless Steel Billets and Bars for Forging /103/
A 320/A 320M 2008 Alloy-Steel and Stainless Steel Bolting Materials for Low-Temperature Service /39/
A 358/A 358M 2008 Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications /67/
A 368 2009 Stainless Steel Wire Strand /12/
A 371   Corrosion-Resisting Chromium and Chromium-Nickel Steel Welding Rods and Bare Electrodes Withdrawn 1969 /no materials/
A 376/A 376M 2000 Seamless Austenitic Steel Pipe for High-Temperature Central-Station Service /19/
A 380 2006 Standard Practice for Cleaning, Descaling, and Passivation of Stainless Steel Parts, Equipment, and Systems /no materials/
A 403/A 403M 2007 Wrought Austenitic Stainless Steel Piping Fittings /81/
A 409/A 409M 2008 Welded Large Diameter Austenitic Steel Pipe for Corrosive or High-Temperature Service /38/
A 412   Stainless and Heat-Resisting Chromium-Nickel-Manganese Steel Plate, Sheet, and Strip Withdrawn 1989 /7/
A 429   Hot- and Cold-Finished Bars of Stainless and Heat-Resisting Chromium-Nickel-Manganese Steel Replaced by A 276 /no materials/
A 451/A 451M 2006 Centrifugally Cast Austenitic Steel Pipe for High-Temperature Service /13/
A 452 1988 Centrifugally Cast Austenitic Steel Cold-Wrought Pipe for High-Temperature Service Withdrawn 1995 /3/
A 478 2008 Chromium-Nickel Stainless Steel Weaving and Knitting Wire /24/
A 479/A 479M 2008 Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels /80/
A 480/A 480M 2009 General Requirements for Flat-Rolled Stainless and Heat-Resisting Steel Plate, Sheet, and Strip /no materials/
A 484/A 484M 2009 General Requirements for Stainless Steel Bars, Billets, and Forgings /no materials/
A 492 2009 Stainless Steel Rope Wire /12/
A 493 2009 Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging /34/
A 511/A 511M 2008 Seamless Stainless Steel Mechanical Tubing /29/
A 554 2008 Welded Stainless Steel Mechanical Tubing /19/
A 555/A 555M 2009 General Requirements for Stainless Steel Wire and Wire Rods /no materials/
A 564/A 564M 2009 Hot-Rolled and Cold-Finished Age-Hardening Stainless Steel Bars and Shapes /21/
A 565/A 565M 2009 Martensitic Stainless Steel Bars for High-Temperature Service /11/
A 580/A 580M 2008 Stainless Steel Wire /79/
A 581/A 581M 2009 Free-Machining Stainless Steel Wire and Wire Rods /24/
A 582/A 582M 2005 Free-Machining Stainless Steel Bars /32/
A 632 2004 Seamless and Welded Austenitic Stainless Steel Tubing (Small-Diameter) for General Service /18/
A 651 1984 Stainless Steel Water-DWV Tube Withdrawn 1986 /7/
A 666 2003 Annealed or Cold-Worked Austenitic Stainless Steel Sheet, Strip, Plate, and Flat Bar /34/
A 669 1983 Seamless Ferritic-Austenitic Alloy Steel Tubes Replaced by A789/A789M /no materials/
A 688/A 688M 2008 Welded Austenitic Stainless Steel Feedwater Heater Tubes /22/
A 693 2006 Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip /25/
A 708 1979 Practice for Detection of Susceptibility to Intergranular Corrosion in Severely Sensitized Austenitic Stainless Steel Withdrawn 1988 /no materials/
A 731/A 731M   Seamless, Welded Ferritic, and Martensitic Stainless Steel Pipe Replaced by A268/A268M /7/
A 756 2009 Stainless Anti-Friction Bearing Steel /2/
A 771/A 771M 2001 Seamless Austenitic and Martensitic Stainless Steel Tubing for Liquid Metal-Cooled Reactor Core Components Withdrawn 2004 /3/
A 774/A 774M 2006 As-Welded Wrought Austenitic Stainless Steel Fittings for General Corrosive Service at Low and Moderate Temperatures /5/
A 778 2001 Welded, Unannealed Austenitic Stainless Steel Tubular Products /10/
A 789/A 789M 2008 Seamless and Welded Ferritic/Austenitic Stainless Steel Tubing for General Service /25/
A 790/A 790M 2009 Seamless and Welded Ferritic/Austenitic Stainless Steel Pipe /29/
A 793 2009 Rolled Floor Plate, Stainless Steel /4/
A 803/A 803M 2008 Welded Ferritic Stainless Steel Feedwater Heater Tubes /21/
A 813/A 813M 2009 Single- or Double-Welded Austenitic Stainless Steel Pipe /60/
A 814/A 814M 2008 Cold-Worked Welded Austenitic Stainless Steel Pipe /63/
A 815/A 815M 2009 Wrought Ferritic, Ferritic/Austenitic, and Martensitic Stainless Steel Piping Fittings /54/
A 826/A 826M 2001 Seamless Austenitic and Martensitic Stainless Steel Duct Tubes for Liquid Metal-Cooled Reactor Core Components Withdrawn 2004 /4/
A 831/A 831M 2000 Austenitic and Martensitic Stainless Steel Bars, Billets, and Forgings for Liquid Metal Cooled Reactor Core Components /4/
A 838 2007 Free-Machining Ferritic Stainless Soft Magnetic Alloy Bar for Relay Applications /5/
A 860/A 860M 2009 Wrought High-Strength Low-Alloy Steel Butt-Welding Fittings /6/
A 872/A 872M 2007 Centrifugally Cast Ferritic/Austenitic Stainless Steel Pipe for Corrosive Environments /4/
A 873/A 873M 1993 Steel Sheet and Strip, Chromium-Molybdenum Alloy, for Pressure Vessels Withdrawn 1997 /no materials/
A 887 2009 Borated Stainless Steel Plate, Sheet, and Strip for Nuclear Application /16/
A 895 2009 Free-Machining Stainless Steel Plate, Sheet, and Strip /16/
A 908 2008 Stainless Steel Needle Tubing /1/
A 928/A 928M 2008 Ferritic/Austenitic (Duplex) Stainless Steel Pipe Electric Fusion Welded with Addition of Filler Metal /15/
A 943/A 943M 2005 Spray-Formed Seamless Austenitic Stainless Steel Pipes /40/
A 947M 2004 Textured Stainless Steel Sheet [Metric] /no materials/
A 949/A 949M 2005 Spray-Formed Seamless Ferritic/Austenitic Stainless Steel Pipe /9/
A 953 2002 Austenitic Chromium-Nickel-Silicon Alloy Steel Seamless and Welded Tubing Withdrawn 2004 /1/
A 954 2002 Austenitic Chromium-Nickel-Silicon Alloy Steel Seamless and Welded Pipe Withdrawn 2005 /1/
A 955/A 955M 2009 Deformed and Plain Stainless-Steel Bars for Concrete Reinforcement /41/
A 959 2009 Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels /219/
A 967 2005 Chemical Passivation Treatments for Stainless Steel Parts /no materials/
A 988/A 988M 2007 Hot Isostatically-Pressed Stainless Steel Flanges, Fittings, Valves, and Parts for High Temperature Service /28/
A 989/A 989M 2007 Hot Isostatically-Pressed Alloy Steel Flanges, Fittings, Valves, and Parts for High Temperature Service /5/
A 999/A 999M 2004 General Requirements for Alloy and Stainless Steel Pipe /no materials/
A 1010/A 1010M 2009 Higher-Strength Martensitic Stainless Steel Plate, Sheet , and Strip /4/
A 1011/A 1011M 2009 Steel, Sheet and Strip, Hot-Rolled, Carbon, Structural, High-Strength Low-Alloy, High-Strength Low-Alloy with Improved Formability, and Ultra-High Strength /35/
A 1012 2007 Seamless and Welded Ferritic, Austenitic and Duplex Alloy Steel Condenser and Heat Exchanger Tubes With Integral Fins Withdrawn 2007 /no materials/
A 1016/A 1016M 2008 General Requirements for Ferritic Alloy Steel, Austenitic Alloy Steel, and Stainless Steel Tubes /no materials/
A 1022/A 1022M 2007 Deformed and Plain Stainless Steel Wire and Welded Wire for Concrete Reinforcement /1/
A 1023/A 1023M 2007 Stranded Carbon Steel Wire Ropes for General Purposes /no materials/
A 1024/A 1024M 2007 Steel Line Pipe, Black, Plain-End, Seamless /5/
A 1026 2003 Alloy Steel Structural Shapes for Use in Building Framing /2/
A 1028 2008 Stainless Steel Bars for Compressor and Turbine Airfoils /12/
A 1053/A 1053M 2006 Welded Ferritic-Martensitic Stainless Steel Pipe /1/
B 625 2005 Plate, sheet, and strip in the annealed temper /6/


Date Published: Apr-2011




Die KEY to METALS Datenbank vereinigt internationale Werkstoffspezifikationen und Metalleigenschaften in einem einzigen Datenbanksystem mit Suchfunktion. Anwender erhalten Hilfe durch einen schnellen und einfachen Zugang zu Informationen über mechanische Eigenschaften und chemische Zusammensetzungen, Querverweistabellen und vielem mehr.

Erfahren Sie mehr auf unserer geführten Tour oder testen Sie die komplette KEY to METALS Datenbank durch kostenlose Trial-Zugriffe, indem sie den Links unten folgen.