ASTM Standard List - Structural and Constructional Steels Standards: Part One


Abstract:
ASTM specifications represent a consensus among producers, specifiers, fabricators, and users of steel mill products. ASTM’s designation system for metals consists of a letter (A for ferrous materials) followed by an arbitrary sequentially assigned number. These designations often apply to specific products, for example A548 is applicable to cold-heading quality carbon steel wire for tapping or sheet metal screws.

This article contains a list of standards that covers among other things:

  • Industry specific steel standards for applications in ships, cars and constructional reinforcement
  • A wide range of specific spring steels and their relevant applications
  • Numerous standards covering carbon steels

For more information on the ASTM designation system see our related article:
Introduction to the ASTM Standard Designation.



Structural and Constructional Steels: Part One

Standard
Number
Last
version
Description Status
A 1 2005 Carbon Steel Tee Rails /6/
A 2 2008 Carbon Steel Girder Rails of Plain, Grooved, and Guard Types /3/
A 3 2006 Steel Joint Bars, Low, Medium, and High Carbon (Non-Heat-Treated) /3/
A 4   Medium-Carbon-Steel Splice Bars /no materials/
A 5   High-Carbon Steel Joint Bars Replaced by A3 /no materials/
A 6/A 6M 2009 General Requirements for Rolled Structural Steel Bars, Plates, Shapes, and Sheet Piling /no materials/
A 7   Steel for Bridges and Building Replaced by A36/A36M /no materials/
A 8   Structural Nickel Steel Withdrawn 1963 /no materials/
A 9   Steel for Buildings Withdrawn 1940 /no materials/
A 10   Mild Steel Plates Withdrawn 1970 /no materials/
A 11   Structural Steel for Cars Replaced by A113 /no materials/
A 12   Structural Steel for Ships /no materials/
A 13   Rivet Steel for Ships Withdrawn 1934 /no materials/
A 14   Carbon-Steel Bars for Springs Withdrawn 1950 /no materials/
A 15   Billet-Steel Bars for Concrete Reinforcement Withdrawn 1969 /no materials/
A 16   Rail-Steel Bars of Concrete Reinforcement Replaced by A 616/A616M /no materials/
A 17   Carbon-Steel and Alloy-Steel Blooms, Billets and Slabs and Forms Replaced by A 273 /no materials/
A 18   Quenched-and-Tempered Carbon-Steel Axles, Shafts, and Other Forgings for Locomotives and Cars Replaced by A 236 /no materials/
A 20/A 20M 2007 General Requirements for Steel Plates for Pressure Vessels /no materials/
A 21 1999 Carbon Steel Axles, Non-Heat-Treated and Heat-Treated, for Railway Use Withdrawn 2003 /5/
A 22   Cold-Rolled Steel Axles Replaced by A 57 /no materials/
A 23   Forged and Rolled, or Rolled Solid Carbon-Steel Wheels for Engine-Truck, Tender, and Passenger Service Replaced by A 57 /no materials/
A 24   Forged and Rolled, or Rolled Solid Carbon-Steel Wheels for Freight-Car Service Replaced by A 57 /no materials/
A 25   Wrought Steel Wheels for Electric Railway Service Replaced by A 504 /5/
A 26   Steel Tires Replaced by A 551/A551M /no materials/
A 28   Lap-Welded and Seamless Steel Boiler Tubes for Locomotives Replaced by A 83 /no materials/
A 29/A 29M 2005 Steel Bars, Carbon and Alloy, Hot-Wrought, General Requirements for /273/
A 30   Boiler and Firebox Steel for Locomotives Withdrawn 1964 /no materials/
A 31   Steel Rivets and Bars for Rivets, Pressure Vessels /2/
A 32   Cold-Drawn Bessemer Steel Automotive Screw Stock Replaced by A 107 /no materials/
A 35   Recommended Practice for Annealing of Miscellaneous Rolled and Forged Carbon-Steel Objects Withdrawn 1937 /no materials/
A 36/A 36M 2008 Carbon Structural Steel /1/
A 37   Recommended Practice for Carburizing and Heat-Treatment of Carburized Objects Withdrawn 1936 /no materials/
A 49 2006 Heat-Treated Carbon Steel Joint Bars, Microalloyed Joint Bars, and Forged Carbon Steel Compromise Joint Bars /1/
A 50   Quenched Carbon-Steel Track Bolts Replaced by A 183 /no materials/
A 51   Quenched Alloy-Steel Track Bolts Replaced by A 183 /no materials/
A 52   Lap-Welded and Seamless Steel and Wrought-Iron Boiler Tubes for Stationary Service Replaced by A 83 /no materials/
A 54   Cold-Drawn Open-Hearth Steel Automatic Screw Stock Replaced by A 107 /no materials/
A 57   Multiple-Wear Wrought Steel Wheels Replaced by A 504/A504M /no materials/
A 58   Carbon-Steel Bars for Vehicle and General Purpose Springs Replaced by A 689 /no materials/
A 59   Silicon-Manganese Steel Bars for Springs Replaced by A 689 /no materials/
A 60   Chromium-Vanadium Steel Bars for Springs Replaced by A 689 /no materials/
A 61   Deformed Rail Steel Bars for Concrete Reinforcement with 60,000 psi Minimum Yield Strength Replaced by A 616/A616M /no materials/
A 62   Steel Elliptical Springs Withdrawn 1949 /no materials/
A 65 2007 Steel Track Spikes /3/
A 66 2007 Steel Screw Spikes /1/
A 67 2005 Steel Tie Plates, Low-Carbon and High-Carbon Hot-Worked /2/
A 68   Carbon Steel Bars for Springs Replaced by A 689 /no materials/
A 69   Elliptical Steel Springs for Automobiles Withdrawn 1927 /no materials/
A 70   Low and Intermediate Tensile Strength Carbon-Steel Replaced by A 285/A285M /no materials/
A 72   Welded Wrought-Iron Pipe Withdrawn 1972 /no materials/
A 73   Wrought Iron Rolled or Forged Blooms and Forgings Withdrawn 1972 /no materials/
A 76   Low-Carbon Steel Track Bolts and Nuts Replaced by A183 /no materials/
A 78   Low Tensile Strength Carbon-Steel Plates of Structured Quality for Welding Replaced by A283/A283M /no materials/
A 80   Cold Finished Carbon-Steel Bars and Shafting Replaced by A107 /no materials/
A 82/A 82M 2007 Steel Wire, Plain, for Concrete Reinforcement /no materials/
A 83   Seamless Carbon Steel Boiler Tubes Replaced by A192/A192M /no materials/
A 89 1943 Low-Tensile Strength Steel Plates of Flange Carbon-Qualities and Firebox Replaced by A285/A285M /no materials/
A 92   High-Speed Tool Steel Withdrawn 1937 /no materials/
A 94   High Strength Structural steel Withdrawn 1966 /no materials/
A 96   Alloy-Steel Bolting Material for High-Temperature Service Replaced by A193/A193M /no materials/
A 98   Spiegeleisen Withdrawn 1992 /no materials/
A 113 1933 Structural Steel for Locomotives and Cars Withdrawn 1979;Replaced by E 44 /no materials/
A 114   Marine Boiler Steel Plates Withdrawn 1940 /no materials/
A 115   Alloy Tool Steel Withdrawn 1937 /no materials/
A 125 2007 Steel Springs, Helical, Heat-Treated /no materials/
A 131/A 131M 2008 Structural Steel for Ships /17/
A 134 2005 Pipe, Steel, Electric-Fusion (Arc)-Welded (Sizes NPS 16 and Over) /14/
A 135/A 135M 2006 Electric-Resistance-Welded Steel Pipe /2/
A 137   Lock-Bar Steel Pipe Withdrawn 1943 /no materials/
A 139/A 139M 2004 Electric-Fusion (Arc)-Welded Steel Pipe (NPS 4 and Over) /5/
A 140   Steel for Bridges and Buildings Withdrawn 1935 /no materials/
A 141   Structural Rivet Steel Withdrawn 1967 /no materials/
A 147   Heat-Treated Steel Leaf Springs Withdrawn 1987 /no materials/
A 149   High Tensile Strength Carbon-Steel Plates for Boilers and Other Pressure Vessel Plates (2 in.) Withdrawn 1940 /no materials/
A 150   High Tensile Strength Carbon-Silicon Steel Plates for Boilers and Other Pressure Vessel Withdrawn 1940 /no materials/
A 151   Steel Suitable for Fusion Welding Withdrawn 1938 /no materials/
A 155   Electric-Fusion Welded Steel Pipe for High-Pressure Service Replaced by A 671 /no materials/
A 160   Axle-Steel Bars for Concrete Reinforcement Replaced by A 617/A617M /no materials/
A 161 1994 Seamless Low-Carbon and Carbon-Molybdenum Steel Still Tubes for Refinery Service /2/
A 162   Uncoated Wrought Iron Sheets Withdrawn 1973 /no materials/
A 178/A 178M 2008 Electric-Resistance-Welded Carbon Steel and Carbon-Manganese Steel Boiler and Superheater Tubes /3/
A 179/A 179M 2005 Seamless Cold-Drawn Low-Carbon Steel Heat-Exchanger and Condenser Tubes /1/
A 183 2009 Carbon Steel Track Bolts and Nuts /4/
A 185/A 185M 2007 Steel Welded Wire Reinforcement, Plain, for Concrete /1/
A 186   One-Wear Wrought Steel Wheels Replaced by A 504/A504M /no materials/
A 187   Seamless Cold-Drawn Alloy-Steel (4 to 6 Percent Chromium) Heat Exchanger and Condenser Tubes Withdrawn 1943 /no materials/
A 188   Seamless Alloy-Steel (4 to 6 Percent Chromium) Still tubes for refinery service Withdrawn 1943 /no materials/
A 189   Single and Double Refined Wrought Iron Bars Withdrawn 1972 /no materials/
A 192/A 192M 2007 Seamless Carbon Steel Boiler Tubes for High-Pressure Service /1/
A 194/A 194M 2009 Carbon and Alloy Steel Nuts for Bolts for High Pressure or High Temperature Service, or Both /42/
A 195 1959 High-Strength Structural Rivet Steel Replaced by A 502 /no materials/
A 200 1994 Seamless Intermediate Alloy-Steel Still Tubes for Refinery Service Replaced by A213/A213M /9/
A 201 1967 Carbon-Silicon Steel Plates of Intermediate Tensile Ranges for Fusion-Welded Boilers and Other Pressure Vessels Replaced by A515/A515M /no materials/
A 202/A 202M 2003 Pressure Vessel Plates, Alloy Steel, Chromium-Manganese-Silicon Withdrawn 2004 /2/
A 203/A 203M 2007 Pressure Vessel Plates, Alloy Steel, Nickel Withdrawn 1972 /5/
A 204/A 204M 2007 Pressure Vessel Plates, Alloy Steel, Molybdenum /3/
A 206   Seamless Ferritic Alloy-Steel Pipe for HIgh-Temperature Service Replaced by A 335/A335M /no materials/
A 207   Rolled Wrought Iron Shapes and Bars Withdrawn 1972 /no materials/
A 209/A 209M 2007 Seamless Carbon-Molybdenum Alloy-Steel Boiler and Superheater Tubes /3/
A 210/A 210M 2007 Seamless Medium-Carbon Steel Boiler and Superheater Tubes /2/
A 211   Spiral-Welded Steel or Iron Pipe Withdrawn 1993 /no materials/
A 212   High Tensile Strength Carbon-Silicon Steel Plates for Boilers and Other Pressure Vessels Withdrawn 1967 /no materials/
A 214/A 214M 2005 Electric-Resistance-Welded Carbon Steel Heat-Exchanger and Condenser Tubes /1/
A 226/A 226M 1995 Electric-Resistance-Welded Carbon Steel Boiler Superheater Tubes for High-Pressure Service Withdrawn 1997 /1/
A 227/A 227M 2006 Steel Wire, Cold-Drawn for Mechanical Springs  
A 228/A 228M 2007 Steel Wire, Music Spring Quality /1/
A 229/A 229M 2005 Steel Wire, Oil-Tempered for Mechanical Springs /2/


Date Published: Apr-2011




The KEY to METALS database brings global metal properties together into one integrated and searchable database. Quick and easy access to the mechanical properties, chemical composition, cross-reference tables, and more provide users with an unprecedented wealth of information. Click the buttons below to learn more from the Guided Tour or to test drive the KEY to METALS database.