ASTM Standard List: Castings


Abstract:
ASTM specifications represent a consensus among producers, specifiers, fabricators, and users of steel mill products. ASTM’s designation system for metals consists of a letter (A for ferrous materials) followed by an arbitrary sequentially assigned number. These designations often apply to specific products, for example A548 is applicable to cold-heading quality carbon steel wire for tapping or sheet metal screws.

This article contains a list of standards that covers among other things:

  • Multiple standards for corrosion resistant iron for general application
  • Automotive Malleable Iron Castings
  • Steel Castings for Highway Bridges

For more information on the ASTM designation system see our related article:
Introduction to the ASTM Standard Designation.



Stainless Steel

Standard
Number
Last
version
Description Status
A 44   Engine Bolt Iron Cast Iron Pit-Cast Pipe for Water Other Liquids Replaced by A 377 /no materials/
A 45   Cast-Iron Locomotive Cylinders Replaced by A 377 /no materials/
A 46   Chilled-Tread Cast-Iron Wheels Withdrawn 1943 /no materials/
A 47/A 47M 2009 Ferritic Malleable Iron Castings /2/
A 47M 1996 Ferritic Malleable Iron Castings [Metric] Replaced by A 47/A47M /no materials/
A 48/A 48M 2008 Gray Iron Castings /20/
A 56   Wrought Iron Crane Chain Withdrawn 1972 /no materials/
A 75   Malleable Iron Castings Replaced by A 47/A47M /no materials/
A 77   Electric Cast-Steel Stud-Link Anchor Chain Withdrawn 1935 /no materials/
A 87   Mild to Medium-Strength Carbon-Steel Castings for General Application Replaced by A27/A27M /no materials/
A 95   Carbon-Steel Castings for Valves, Flanges, and Fittings for High-Temperature Service Replaced by A 216/A216M /no materials/
A 128/A 128M 2007 Steel Castings, Austenitic Manganese /11/
A 148/A 148M 2008 Steel Castings, High Strength, for Structural Purposes /30/
A 154   Mild-to-Medium-Strength Carbon-Steel Castings for General Application Replaced by A 27 /no materials/
A 157   Alloy-Steel Castings for Pressure Containing Parts Suitable for High-Temperature Service Replaced by A 217/A217M /no materials/
A 158   Seamless Ferritic Alloy-Steel Pipe for High-Temperature Service /no materials/
A 159 2006 Automotive Gray Iron Castings /9/
A 168   Corrosion-Resistant Iron-Chromium and Iron-Chromium-Nickel Alloy Castings for General Application Replaced by A 296 /no materials/
A 169   Corrosion-Resistant Iron-Chromium and Iron-Chromium-Nickel Alloy Castings for General Application Replaced by A 296 /no materials/
A 170   Corrosion-Resistant Iron-Chromium and Iron-Chromium-Nickel Alloy Castings for General Application Replaced by A 296 /no materials/
A 171   Corrosion-Resistant Iron-Chromium and Iron-Chromium-Nickel Alloy Castings for General Application Replaced by A 296 /no materials/
A 173   Corrosion-Resistant Iron-Chromium and Iron-Chromium-Nickel Alloy Castings for General Application Replaced by A 296 /no materials/
A 174   Corrosion-Resistant Iron-Chromium and Iron-Chromium-Nickel Alloy Castings for General Application Replaced by A 296 /no materials/
A 175   Corrosion-Resistant Iron-Chromium and Iron-Chromium-Nickel Alloy Castings for General Application Replaced by A 296 /no materials/
A 180   Mild-to-Medium-Strength Carbon-Steel Castings for General Application Replaced by A 27/A27M /no materials/
A 198   Corrosion-Resistant Iron-Chromium and Iron-Chromium-Nickel Alloy Castings for General Application /no materials/
A 199/A 199M 1992 Seamless Cold-Drawn Intermediate Alloy-Steel Heat-Exchanger and Condenser Tubes Replaced by A 200 /9/
A 215   Mild-to-Medium-Strength Carbon-Steel Castings for General Application Replaced by A 27/A27M /no materials/
A 216/A 216M 2008 Steel Castings, Carbon, Suitable for Fusion Welding, for High-Temperature Service /3/
A 217/A 217M 2008 Steel Castings, Martensitic Stainless and Alloy, for Pressure-Containing Parts, Suitable for High-Temperature Service /20/
A 221   Corrosion-Resistant Iron-Chromium and Iron-Chromium-Nickel Alloy Castings for General Application Replaced by A 296 /no materials/
A 222   Corrosion-Resistant Iron-Chromium and Iron-Chromium-Nickel Alloy Castings for General Application Replaced by A 296 /no materials/
A 223   Corrosion-Resistant Iron-Chromium and Iron-Chromium-Nickel Alloy Castings for General Application Replaced by A 296 /no materials/
A 27/A 27M 2008 Steel Castings, Carbon, for General Application /12/
A 282   High-Strength Steel Castings for Structural Purposes Replaced by A 148/A148M /no materials/
A 297/A 297M 2008 Steel Castings, Iron-Chromium and Iron-Chromium-Nickel, Heat Resistant, for General Application /15/
A 351/A 351M 2006 Castings, Austenitic, for Pressure-Containing Parts /31/
A 352/A 352M   Steel Castings, Ferritic and Martensitic, for Pressure-Containing Parts, Suitable for Low-Temperature Service /20/
A 356/A 356M 2007 Steel Castings, Carbon, Low Alloy, and Stainless Steel, Heavy-Walled for Steam Turbines /9/
A 362   Iron-Chromium and Iron-Chromium-Nickel Alloy Tubular Centrifugal Castings for General Applications Withdrawn 1997 /no materials/
A 389/A 389M 2008 Steel Castings, Alloy, Specially Heat-Treated, for Pressure-Containing Parts, Suitable for High-Temperature Service /2/
A 396   High-Strength Ductile Iron Castings Replaced by A 536 /no materials/
A 436 2006 Austenitic Gray Iron Castings /8/
A 437/A 437M 2006 Alloy-Steel Turbine-Type Bolting Material Specially Heat Treated for High-Temperature Service /3/
A 439 2004 Austenitic Ductile Iron Castings /9/
A 445 1974 Ferritic Iron Castings for Valves, Flanges, Pipe Fittings, and Other Piping Components Replaced by A 395/A395M /no materials/
A 447/A 447M 2007 Steel Castings, Chromium-Nickel-Iron Alloy (25-12 Class), for High-Temperature Service /1/
A 448   Nickel-Chromium-Iron Alloy Castings (35-15 Class) for High-Temperature Service Withdrawn 1976 /no materials/
A 476/A 476M 2009 Ductile Iron Castings for Paper Mill Dryer Rolls /1/
A 476M 1993 Ductile Iron Castings for Paper Mill Dryer Rolls [Metric] Replaced by A 476/A476M /no materials/
A 486/A 486M   Steel Castings for Highway Bridges Withdrawn 1998 /3/
A 487/A 487M 2007 Steel Castings Suitable for Pressure Service /39/
A 488/A 488M 2007 Standard Practice for Steel Castings, Welding, Qualifications of Procedures and Personnel /no materials/
A 518/A 518M 2008 Corrosion-Resistant High-Silicon Iron Castings /3/
A 518M 1997 Corrosion-Resistant High-Silicon Iron Castings [Metric] Replaced by A 518/A518M /no materials/
A 536 2004 Ductile Iron Castings /8/
A 560/A 560M 2005 Castings, Chromium-Nickel Alloy /3/
A 567/A 567M   Castings, Iron, Cobalt, and Nickel-Base Alloy, for High Strength at Elevated Temperatures Withdrawn 1985 /19/
A 571/A 571M 2006 Austenitic Ductile Iron Castings for Pressure-Containing Parts Suitable for Low-Temperature Service /4/
A 571M 1997 Austenitic Ductile Iron Castings for Pressure-Containing Parts Suitable for Low-Temperature Service [Metric] Replaced by A 571/A571M /no materials/
A 597 2004 Cast Tool Steel /9/
A 602 2004 Automotive Malleable Iron Castings /6/
A 613   Special Requirements for Steel Castings for Nuclear and Other Special Applications Withdrawn 1985 /no materials/
A 643   Steel Castings, Heavy-Walled, Carbon and Alloy for Pressure Vessels /no materials/
A 703/A 703M 2008 Steel Castings, General Requirements, for Pressure-Containing Parts /no materials/
A 743/A 743M 2006 Castings, Iron-Chromium, Iron-Chromium-Nickel, Corrosion Resistant, for General Application /72/
A 744/A 744M 2006 Castings, Iron-Chromium-Nickel, Corrosion Resistant, for Severe Service /29/
A 747/A 747M 2007 Steel Castings, Stainless, Precipitation Hardening /2/
A 748/A 748M 2008 Statically Cast Chilled White Iron-Gray Iron Dual Metal Rolls for Pressure Vessel Use /4/
A 750 1994 Steel Air Ventilating Grille Units for Detention Areas Withdrawn 2004 /no materials/
A 757/A 757M 2004 Steel Castings, Ferritic and Martensitic, for Pressure-Containing and Other Applications, for Low-Temperature Service /23/
A 781/A 781M 2008 Castings, Steel and Alloy, Common Requirements, for General Industrial Use /no materials/
A 799/A 799M 2004 Standard Practice for Steel Castings, Stainless, Instrument Calibration, for Estimating Ferrite Content /no materials/
A 800/A 800M 2006 Standard Practice for Steel Casting, Austenitic Alloy, Estimating Ferrite Content Thereof /no materials/
A 802/A 802M 2006 Standard Practice for Steel Castings, Surface Acceptance Standards, Visual Examination /no materials/
A 874/A 874M 2009 Ferritic Ductile Iron Castings Suitable for Low-Temperature Service /1/
A 874M 1989 Ferritic Ductile Iron Castings Suitable for Low-Temperature Service [Metric] Replaced by 874/A874M /no materials/
A 890/A 890M 2007 Castings, Iron-Chromium-Nickel-Molybdenum Corrosion-Resistant, Duplex (Austenitic/Ferritic) for General Application /24/
A 903/A 903M 2007 Steel Castings, Surface Acceptance Standards, Magnetic Particle and Liquid Penetrant Inspection /no materials/
A 915/A 915M 2008 Steel Castings, Carbon, and Alloy, Chemical Requirements Similar to Standard Wrought Grades /24/
A 957/A 957M 2009 Investment Castings, Steel and Alloy, Common Requirements, for General Industrial Use /no materials/
A 958 2006 Steel Castings, Carbon and Alloy, with Tensile Requirements, Chemical Requirements Similar to Standard Wrought Grades /94/
A 985/A 985M 2008 Steel Investment Castings General Requirements, for Pressure-Containing Parts /no materials/
A 990 2008 Castings, Iron-Nickel-Chromium and Nickel Alloys, Specially Controlled for Pressure Retaining Parts for Corrosive Service /3/
A 995/A 995M 2009 Castings, Austenitic-Ferritic (Duplex) Stainless Steel, for Pressure-Containing Parts /23/
A 997 2008 Standard Practice for Investment Castings, Surface Acceptance Standards, Visual Examination /no materials/
A 998/A 998M 2008 Standard Practice for Structural Design of Reinforcements for Fittings in FactoryMade Corrugated Steel Pipe for Sewers and Other Applications /no materials/
A 1001 2006 High Strength Steel Castings in Heavy Sections /3/
A 1002 2003 Castings, Nickel-Aluminum Ordered Alloy /1/


Date Published: Apr-2011




The KEY to METALS database brings global metal properties together into one integrated and searchable database. Quick and easy access to the mechanical properties, chemical composition, cross-reference tables, and more provide users with an unprecedented wealth of information. Click the buttons below to learn more from the Guided Tour or to test drive the KEY to METALS database.