Standard Number |
Last version |
Description |
Status |
| EN 10216-1 |
2002 |
Seamless steel tubes for pressure purposes - Technical delivery conditions - Part 1: Non-alloy steel tubes with specified room temperature properties |
|
| EN 10216-2 |
2002 |
Seamless steel tubes for pressure purposes - Technical delivery conditions - Part 2: Non-alloy and alloy steel tubes with specified elevated temperature properties |
|
| EN 10216-3 |
2002 |
Seamless steel tubes for pressure purposes - Technical delivery conditions - Part 3: Alloy fine grain steel tubes |
|
| EN 10216-4 |
2002 |
Seamless steel tubes for pressure purposes - Technical delivery conditions - Part 4: Non-alloy and alloy steel tubes with specified low temperature properties |
|
| EN 10216-5 |
2004 |
Seamless steel tubes for pressure purposes - Technical delivery conditions - Part 5: Stainless steel tubes |
|
| EN 10217-1 |
2002 |
Welded steel tubes for pressure purposes - Technical delivery conditions - Part 1: Non-alloy steel tubes with specified room temperature properties |
|
| EN 10217-2 |
2002 |
Welded steel tubes for pressure purposes - Technical delivery conditions - Part 2: Electric welded non-alloy and alloy steel tubes with specified elevated temperature properties |
|
| EN 10217-3 |
2002 |
Welded steel tubes for pressure purposes - Technical delivery conditions - Part 3: Alloy fine grain steel tubes |
|
| EN 10217-4 |
2002 |
Welded steel tubes for pressure purposes - Technical delivery conditions - Part 4: Electric welded non-alloy steel tubes with specified low temperature properties |
|
| EN 10217-5 |
2002 |
Welded steel tubes for pressure purposes - Technical delivery conditions - Part 5: Submerged arc welded non-alloy and alloy steel tubes with specified elevated temperature properties |
|
| EN 10217-6 |
2002 |
Welded steel tubes for pressure purposes - Technical delivery conditions - Part 6: Submerged arc welded non-alloy steel tubes with specified low temperature properties |
|
| EN 10217-7 |
2005 |
Welded steel tubes for pressure purposes - Technical delivery conditions - Part 7: Stainless steel tubes |
|
| EN 10219-1 |
2006 |
Cold formed welded structural hollow sections of non-alloy and fine grain steels - Part 1: Technical delivery conditions |
|
| EN 10219-2 |
2006 |
Cold formed welded structural hollow sections of non-alloy and fine grain steels - Part 2: Tolerances, dimensions and sectional properties |
|
| EN 10220 |
2002 |
Seamless and welded steel tubes - Dimensions and masses per unit length |
|
| EN 10221 |
1995 |
Surface quality classes for hot-rolled bars and rods - Technical delivery conditions |
|
| EN 10223-2 |
1997 |
Steel wire and wire products for fences - Part 2: Hexagonal steel wire netting for agricultural, insulation and fencing purposes |
|
| EN 10223-3 |
1997 |
Steel wire and wire products for fences - Part 3: Hexagonal steel wire netting for engineering purposes |
|
| EN 10223-4 |
1998 |
Steel wire and wire products for fences - Part 4: Steel wire welded mesh fencing |
|
| EN 10223-5 |
1998 |
Steel wire and wire products for fences - Part 5: Steel wire woven hinged joint and knotted mesh fencing |
|
| EN 10223-6 |
1998 |
Steel wire and wire products for fences - Part 6: Steel wire chain link fencing |
|
| EN 10223-7 |
2002 |
Steel wire and wire products for fences - Part 7: Steel wire welded panels - For fencing |
|
| EN 10224 |
2002 |
Non-alloy steel tubes and fittings for the conveyance of water and other aqueous liquids - Technical delivery conditions |
|
| EN 10225 |
2001 |
Weldable structural steels for fixed offshore structures - Technical delivery conditions |
|
| EN 10229 |
1998 |
Evaluation of resistance of steel products to hydrogen induced cracking (HIC) |
|
| EN 10238 |
2009 |
Automatically blast-cleaned and automatically prefabricated primed structural steel products |
|
| EN 10248-1 |
1995 |
Hot rolled sheet piling of non alloy steels - Part 1: Technical delivery conditions |
|
| EN 10248-2 |
1995 |
Hot rolled sheet piling of non alloy steels - Part 2: Tolerances on shape and dimensions |
|
| EN 10249-1 |
1995 |
Cold formed sheet piling of non alloy steels - Part 1: Technical delivery conditions |
|
| EN 10249-2 |
1995 |
Cold formed sheet piling of non alloy steels - Part 2: Tolerances on shape and dimensions |
|
| EN 10255 |
2004 |
Non-alloy steel tubes suitable for welding and threading - Technical delivery conditions |
|
| EN 10263-1 |
2001 |
Steel rod, bars and wire for cold heading and cold extrusion - Part 1: General technical delivery conditions |
|
| EN 10263-2 |
2001 |
Steel rod, bars and wire for cold heading and cold extrusion - Part 2: Technical delivery conditions for steels not intended for heat treatment after cold working |
|
| EN 10263-3 |
2001 |
Steel rod, bars and wire for cold heading and cold extrusion - Part 3: Technical delivery conditions for case hardening steels |
|
| EN 10263-4 |
2001 |
Steel rod, bars and wire for cold heading and cold extrusion - Part 4: Technical delivery conditions for steels for quenching and tempering |
|
| EN 10263-5 |
2001 |
Steel rod, bars and steel wire for cold heading and cold extrusion - Part 5: Technical delivery conditions for stainless steels |
|
| EN 10264-1 |
2002 |
Steel wire and wire products - Steel wire for ropes - Part 1: General requirements |
|
| EN 10264-2 |
2002 |
Steel wire and wire products - Steel wire for ropes - Part 2: Cold drawn non alloy steel wire for ropes for general applications |
|
| EN 10264-3 |
2002 |
Steel wire and wire products - Steel wire for ropes - Part 3: Round and shaped non alloyed steel wire for high duty applications |
|
| EN 10264-4 |
2002 |
Steel wire and wire products - Steel wire for ropes - Part 4: Stainless steel wire |
|
| EN 10266 |
2003 |
Steel tubes, fittings and structural hollow sections - Symbols and definitions of terms for use in product standards |
|
| EN 10267 |
1998 |
Ferritic-pearlitic steels for precipitation hardening from hot-working temperatures |
|
| EN 10268 |
2006 |
Cold rolled steel flat products with high yield strength for cold forming - Technical delivery conditions |
|
| EN 10269 |
2008 |
Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties |
|
| EN 10270-1 |
2001 |
Steel wire for mechanical springs - Part 1: Patented cold drawn unalloyed spring steel wire |
|
| EN 10270-2 |
2001 |
Steel wire for mechanical springs - Part 2: Oil hardened and tempered spring steel wire |
|
| EN 10273 |
2007 |
Hot rolled weldable steel bars for pressure purposes with specified elevated temperature properties |
|
| EN 10277-1 |
2008 |
Bright steel products - Technical delivery conditions - Part 1: General |
|
| EN 10277-2 |
2008 |
Bright steel products - Technical delivery conditions - Part 2: Steels for general engineering purposes |
|
| EN 10277-3 |
2008 |
Bright steel products - Technical delivery conditions - Part 3: Free-cutting steels |
|
| EN 10277-4 |
2008 |
Bright steel products - Technical delivery conditions - Part 4: Case-hardening steels |
|
| EN 10277-5 |
2008 |
Bright steel products - Technical delivery conditions - Part 5: Steels for quenching and tempering |
|
| EN 10278 |
1999 |
Dimensions and tolerances of bright steel products |
|
| EN 10279 |
2000 |
Hot rolled steel channels - Tolerances on shape, dimensions and mass |
|
| EN 10294-1 |
2005 |
Hollow bars for machining - Technical delivery conditions - Part 1: Non alloy and alloy steels |
|
| EN 10296-1 |
2003 |
Welded circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 1: Non-alloy and alloy steel tubes |
|
| EN 10297-1 |
2003 |
Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 1: Non-alloy and alloy steel tubes |
|
| EN 10305-1 |
2002 |
Steel tubes for precision applications - Technical delivery conditions - Part 1: Seamless cold drawn tubes |
|
| EN 10305-2 |
2002 |
Steel tubes for precision applications - Technical delivery conditions - Part 2: Welded cold drawn tubes |
|
| EN 10305-3 |
2002 |
Steel tubes for precision applications - Technical delivery conditions - Part 3: Welded cold sized tubes |
|
| EN 10305-4 |
2003 |
Steel tubes for precision applications - Technical delivery conditions - Part 4: Seamless cold drawn tubes for hydraulic and pneumatic power systems |
|
| EN 10305-5 |
2003 |
Steel tubes for precision applications - Technical delivery conditions - Part 5: Welded and cold sized square and rectangular tubes |
|
| EN 10305-6 |
2005 |
Steel tubes for precision applications - Technical delivery conditions - Part 6: Welded cold drawn tubes for hydraulic and pneumatic power systems |
|
| EN 10323 |
2004 |
Steel wire and wire products - Bead wire |
|
| EN 10324 |
2004 |
Steel wire and wire products - Hose reinforcement wire |
|
| EN 10341 |
2006 |
Cold rolled electrical non-alloy and alloy steel sheet and strip delivered in the semi-processed state |
|
| EN 12385-1 |
2002 |
Steel wire ropes - Safety - Part 1: General requirements |
|
| EN 12385-10 |
2003 |
Steel wire ropes - Safety - Part 10: Spiral ropes for general structural applications |
|
| EN 12385-2 |
2002 |
Steel wire ropes - Safety - Part 2: Definitions, designation and classification |
|
| EN 12385-3 |
2004 |
Steel wire ropes - Safety - Part 3: Information for use and maintenance |
|
| EN 12385-5 |
2002 |
Steel wire ropes - Safety - Part 5: Stranded ropes for lifts |
|
| EN 12385-6 |
2004 |
Steel wire ropes - Safety - Part 6: Stranded ropes for mine shafts |
|
| EN 12385-7 |
2002 |
Steel wire ropes - Safety - Part 7: Locked coil ropes for mine shafts |
|
| EN 12385-8 |
2002 |
Steel wire ropes - Safety - Part 8: Stranded hauling and carrying-hauling ropes for cableway installations designed to carry persons |
|
| EN 12385-9 |
2002 |
Steel wire ropes - Safety - Part 9: Locked coil carrying ropes for cableway installations designed to carry persons |
|
| EN 12952-2 |
2001 |
Water-tube boilers and auxiliary installations - Part 2: Materials for pressure parts of boilers and accessories |
|
| EN 13173 |
2001 |
Cathodic protection for steel offshore floating structures |
|
| EN 13174 |
2001 |
Cathodic protection for harbour installations |
|
| ENV 10080 |
1995 |
Steel for the reinforcement of concrete - Weldable ribbed reinforcing steel B 500 - Technical delivery conditions for bars, coils and welded fabric |
Replaced by EN 10080:2005 |