Euronorm Standard List: Electrical Steels, Coated Steels, Castings and Forgings


Abstract:
The creation of the EEC (European Economic Community) has made it necessary to establish common standards named "European Norms" (EN), therefore standardizing the common language across Europe. Since 1988 a new series of 'mandatory' European standards (EN) has been created, to replace national standards, such as BS, DIN, SS and NF, throughout 18 countries of Western Europe.

The EN Designation System uses an alpha-numerical index to denote the key information about the material including mechanical properties, tensile strength and potential usage.

For more information on the EN designation system see Introduction to the Euronorm Standard Designation System.

The list of standards below cover among other things:

  • Hot-dipped coated steels for multiple uses
  • Various examples of organically coated steel wires
  • Zinc or zinc alloy coated non-alloy steel wire for armouring either power cables or telecommunication cables


Electrical steels

Standard
Number
Last
version
Description Status
EN 10106 2007 Cold rolled non-oriented electrical steel sheet and strip delivered in the fully processed state  
EN 10107 2005 Grain-oriented electrical steel sheet and strip delivered in the fully processed state  

Coated steels

Standard
Number
Last
version
Description Status
EN 10142 2000 Continuously hot-dip zinc coated low carbon steels strip and sheet for cold forming - Technical delivery conditions Replaced by EN10327:2004
EN 10143 2006 Continuously hot-dip coated steel sheet and strip - Tolerances on dimensions and shape  
EN 10147 2000 Continuously hot-dip zinc coated structural steels strip and sheet - Technical delivery conditions Replaced by EN10326:2004
EN 10152 2009 Electrolytically zinc coated cold rolled steel flat products for cold forming - Technical delivery conditions  
EN 10154 2002 Continuously hot-dip aluminium-silicon (AS) coated steel strip and sheet - Technical delivery conditions Replaced by EN10326:2004; EN 10327:2004
EN 10169-1 2003 Continuously organic coated (coil coated) steel flat products - Part 1: General information (definitions, materials, tolerances, test methods)  
EN 10169-2 2006 Continuously organic coated (coil coated) steel flat products - Part 2: Products for building exterior applications  
EN 10169-3 2003 Continuously organic coated (coil coated) steel flat products - Part 3: Products for building interior applications  
EN 10202 2001 Cold reduced tinmill products - Electrolytic tinplate and electrolytic chromium/chromium oxide coated steel  
EN 10203 1991 Cold reduced electrolytic tinplate Replaced by EN10202:2001
EN 10205 1991 Cold reduced blackplate in coil form for the production of tinplate or electrolytic chromium/chromium oxide coated steel  
EN 10214 1995 Continuously hot-dip zinc-aluminium (ZA) coated steel strip and sheet - Technical delivery conditions Replaced by EN10326:2004; EN 10327:2004
EN 10215 1995 Continuously hot-dip aluminium-zinc (AZ) coated steel strip and sheet - Technical delivery conditions Replaced by EN10326:2004; EN 10327:2004
EN 10223-1 1997 Steel wire and wire products for fences - Part 1: Zinc and zinc-alloy coated steel barbed wire  
EN 10240 1997 Internal and/or external protective coatings for steel tubes - Specification for hot dip galvanized coatings applied in automatic plants  
EN 10244-1 2009 Steel wire and wire products - Non-ferrous metallic coatings on steel wire - Part 1: General principles  
EN 10244-2 2009 Steel wire and wire products - Non-ferrous metallic coatings on steel wire - Part 2: Zinc or zinc alloy coatings  
EN 10244-3 2001 Steel wire and wire products -Non-ferrous metallic coatings on steel wire - Part 3: Aluminium coatings  
EN 10244-4 2001 Steel wire and wire products - Non-ferrous metallic coatings on steel wire - Part 4: Tin coatings  
EN 10244-5 2001 Steel wire and wire products - Non-ferrous metallic coatings on steel wire - Part 5: Nickel coatings  
EN 10244-6 2001 Steel wire and wire products - Non-ferrous metallic coatings on steel wire - Part 6: Copper, bronze or brass coatings  
EN 10245-1 2001 Steel wire and wire products - Organic coatings on steel wire - Part 1: General rules  
EN 10245-2 2001 Steel wire and wire products - Organic coatings on steel wire - Part 2: PVC finished wire  
EN 10245-3 2001 Steel wire and wire products - Organic coatings on steel wire - Part 3: PE coated wire  
EN 10245-4 2001 Steel wire and wire products - Organic coatings on steel wire - Part 4: Polyester coated wire  
EN 10257-1 1998 Zinc or zinc alloy coated non-alloy steel wire for armouring either power cables or telecommunication cables - Part 1: Land cables  
EN 10257-2 1998 Zinc or zinc alloy coated non-alloy steel wire for armouring either power cables or telecommunication cables - Part 2: Submarine cables  
EN 10271 1998 Electrolytically zinc-nickel (ZN) coated steel flat products - Technical delivery conditions  
EN 10292 2007 Continuously hot-dip coated strip and sheet of steels with high yield strength for cold forming - Technical delivery conditions  
EN 10326 2004 Continuously hot-dip coated strip and sheet of structural steels - Technical delivery conditions  
EN 10327 2004 Continuously hot-dip coated strip and sheet of low carbon steels for cold forming - Technical delivery conditions  
EN 10336 2007 Continuously hot-dip coated and electrolytically coated strip and sheet of multiphase steels for cold forming  
EN 10346 2009 Continuously hot-dip coated steel flat products - Technical delivery conditions  

Castings

Standard
Number
Last
version
Description Status
EN 10213 2008 Steel castings for pressure purposes  
EN 10213-1 1995 Technical delivery conditions for steel castings for pressure purposes - Part 1: General  
EN 10213-2 1995 Technical delivery conditions for steel castings for pressure purposes - Part 2: Steel grades for use at room temperature and elevated temperatures  
EN 10213-3 1995 Technical delivery conditions for steel castings for pressure purposes - Part 3: Steel grades for use at low temperatures  
EN 10213-4 1995 Technical delivery conditions for steel castings for pressure purposes - Part 4: Austenitic and austenitic-ferritic steel grades  
EN 10283 1998 Corrosion resistant steel castings  
EN 10293 2008 Steel castings for general engineering uses  
EN 10295 2002 Heat resistant steel castings  
EN 10340 2007 Steel castings for structural uses  
EN 12454 1998 Founding - Visual examination of surface discontinuities - Steel sand castings  
EN 12513 2000 Founding - Abrasion resistant cast irons  
EN 12680-1 2003 Founding - Ultrasonic examination - Part 1: Steel castings for general purposes  
EN 12680-2 2003 Founding - Ultrasonic examination - Part 2: Steel castings for highly stressed components  
EN 12680-3 2003 Founding - Ultrasonic examination - Part 3: Spheroidal graphite cast iron castings  
EN 1369 1996 Founding - Magnetic particle inspection  
EN 1371-1 1997 Founding - Liquid penetrant inspection - Part 1: Sand, gravity die and low pressure die castings  
EN 1371-2 1998 Founding - Liquid penetrant inspection - Part 2: Investment castings  
EN 13835 2002 Founding - Austenitic cast irons  
EN 1503-3 2000 Valves - Materials for bodies, bonnets and covers - Part 3: Cast irons specified in European Standards  
EN 1559-1 1997 Founding - Technical conditions of delivery - Part 1: General  
EN 1559-2 2000 Founding - Technical conditions of delivery - Part 2: Additional requirements for steel castings  
EN 1559-3 1997 Founding - Technical conditions of delivery - Part 3: Additional requirements for iron castings  
EN 1560 1997 Founding - Designation system for cast iron - Material symbols and material numbers  
EN 1561 1997 Founding - Grey cast irons  
EN 1562 2006 Founding - Malleable cast irons  
EN 1563 2005 Founding - Spheroidal graphite cast irons  
EN 1564 2006 Founding - Austempered ductile cast irons  
EN ISO 945 1994 Cast iron - Designation of microstructure of graphite  

Forgings

Standard
Number
Last
version
Description Status
EN 10222-1 1998 Steel forgings for pressure purposes - Part 1 : General requirements for open die forgings  
EN 10222-2 1999 Steel forgings for pressure purposes - Part 2: Ferritic and martensitic steels with specified elevated temperature properties  
EN 10222-3 1998 Steel forgings for pressure purposes - Part 3: Nickel steels with specified low temperature properties  
EN 10222-4 1998 Steel forgings for pressure purposes - Part 4: Weldable fine grain steels with high proof strength  
EN 10222-5 1999 Steel forgings for pressure purposes - Part 5: Martensitic, austenitic and austenitic-ferritic stainless steels  
EN 10243-1 1999 Steel die forgings - Tolerances on dimensions - Part 1: Drop and vertical press forgings  
EN 10243-2 1999 Steel die forgings - Tolerances on dimensions - Part 2: Upset forging made on horizontal forging machines  
EN 10250-1 1999 Open die steel forgings for general engineering purposes - Part 1: General requirements  
EN 10250-2 1999 Open die steel forgings for general engineering purposes - Part 2: Non-alloy quality and special steels  
EN 10250-3 1999 Open die steel forgings for general engineering purposes - Part 3: Alloy special steels  
EN 10250-4 1999 Open die steel forgings for general engineering purposes - Part 4: Stainless steels  
EN 10254 1999 Steel closed die forgings - General technical delivery conditions  


Date Published: Apr-2011




The KEY to METALS database brings global metal properties together into one integrated and searchable database. Quick and easy access to the mechanical properties, chemical composition, cross-reference tables, and more provide users with an unprecedented wealth of information. Click the buttons below to learn more from the Guided Tour or to test drive the KEY to METALS database.