Euronorm Standard List: Wrought, Castings, Ingots, and Remelting


Abstract:
The creation of the EEC (European Economic Community) has made it necessary to establish common standards named "European Norms" (EN), therefore standardizing the common language across Europe. Since 1988 a new series of 'mandatory' European standards (EN) has been created, to replace national standards, such as BS, DIN, SS and NF, throughout 18 countries of Western Europe.

Aluminum is one of the most economical and structurally effective materials used for commercial and military equipment applications. Some of its attractive properties include: good appearance, easy of fabrication, good corrosion resistance, low density and high strength-to-weight ratio, high fracture toughness etc.

For more information on the EN designation system see Introduction to the Euronorm Standard Designation System.

The list of standards below cover among other things:

  • A range of aluminium alloys used for general use and for multiple applications
  • Aluminium used for drill pipes in the petroleum and natural gas industries
  • Various aluminium alloys used in general structural and constructional applications

Click on the below links to see lists of Euronorm standards covering the following material categories:

Aluminium Materials

Aluminium Aerospace Materials


Wrought/Castings/Ingots/Remelting

Standard
Number
Last
version
Description Status
EN 485-1 2008 Aluminium and aluminium alloys - Sheet, strip and plate - Part 1: Technical conditions for inspection and delivery  
EN 485-2 2008 Aluminium and aluminium alloys - Sheet, strip and plate - Part 2: Mechanical properties  
EN 485-3 2003 Aluminium and aluminium alloys - Sheet, strip and plate - Part 3: Tolerances on dimensions and form for hot-rolled products  
EN 485-4 1993 Aluminium and aluminium alloys - Sheet, strip and plate - Part 4: Tolerances on shape and dimensions for cold-rolled products  
EN 486 2009 Aluminium and aluminium alloys - Extrusion ingots - Specifications  
EN 487 2009 Aluminium and aluminium alloys - Rolling ingots - Specifications  
EN 541 2006 Aluminium and aluminium alloys - Rolled products for cans, closures and lids - Specifications  
EN 546-1 2006 Aluminium and aluminium alloys - Foil - Part 1: Technical conditions for inspection and delivery  
EN 546-2 2006 Aluminium and aluminium alloys - Foil - Part 2: Mechanical properties  
EN 546-3 2006 Aluminium and aluminium alloys - Foil - Part 3: Tolerances on dimensions  
EN 546-4 2006 Aluminium and aluminium alloys - Foil - Part 4: Special property requirements  
EN 570 2007 Aluminium and aluminium alloys - Impact extrusion slugs obtained from wrought products - Specification  
EN 573-1 2004 Aluminium and aluminium alloys - Chemical composition and form of wrought products - Part 1: Numerical designation system  
EN 573-3 2009 Aluminium and aluminium alloys - Chemical composition and form of wrought products - Part 3: Chemical composition  
EN 573-4 2007 Aluminium and aluminium alloys - Chemical composition and form of wrought products - Part 4: Forms of products  
EN 1301-1 2008 Aluminium and aluminium alloys - Drawn wire - Part 1: Technical conditions for inspection and delivery  
EN 1301-2 2008 Aluminium and aluminium alloys - Drawn wire - Part 2: Mechanical properties  
EN 1301-3 2008 Aluminium and aluminium alloys - Drawn wire - Part 3: Tolerances on dimensions  
EN 1386 2007 Aluminium and aluminium alloys - Tread plate - Specifications  
EN 1396 2007 Aluminium and aluminium alloys - Coil coated sheet and strip for general applications - Specifications  
EN 1592-1 1997 Aluminium and aluminium alloys - HF seam welded tubes - Part 1: Technical conditions for inspection and delivery  
EN 1592-2 2000 Aluminium and aluminium alloys - HF seam welded tubes - Part 2: Mechanical properties  
EN 1592-3 1997 Aluminium and aluminium alloys - HF seam welded tubes - Part 3: Tolerances on dimensions and form for circular tubes  
EN 1592-4 1999 Aluminium and aluminium alloys - HF seam welded tubes - Part 4: Tolerances on dimensions and form for square, rectangular and shaped tubes  
EN 1676 1996 Aluminium and aluminium alloys - Alloyed ingots for remelting - Specifications  
EN 1706 1998 Aluminium and aluminium alloys - Castings - Chemical composition and mechanical properties  
EN 1715-1 2008 Aluminium and aluminium alloys - Drawing stock - Part 1: General requirements and technical conditions for inspection and delivery  
EN 1715-2 2008 Aluminium and aluminium alloys - Drawing stock - Part 2: Specific requirements for electrical applications  
EN 1715-3 2008 Aluminium and aluminium alloys - Drawing stock - Part 3: Specific requirements for mechanical uses (excluding welding)  
EN 1715-4 2008 Aluminium and aluminium alloys - Drawing stock - Part 4: Specific requirements for welding applications  
EN 12020-1 2008 Aluminium and aluminium alloys - Extruded precision profiles in alloys EN AW-6060 and EN AW-6063 - Part 1: Technical conditions for inspection and delivery  
EN 12020-2 2008 Aluminium and aluminium alloys - Extruded precision profiles in alloys EN AW-6060 and EN AW-6063 - Part 2: Tolerances on dimensions and form  
EN 12392 2000 Aluminium and aluminium alloys - Wrought products - Special requirements for products intended for the production of pressure equipment  
EN 12482-1 1998 Aluminium and aluminium alloys - Reroll stock for general applications - Part 1: Specifications for hot rolled reroll stock  
EN 12482-2 1998 Aluminium and aluminium alloys - Reroll stock for general applications - Part 2: Specifications for cold rolled reroll stock  
EN 13195-1 2002 Aluminium and aluminium alloys - Wrought and cast products for marine applications (shipbuilding, marine and offshore) - Part 1: Specifications  
EN 13957 2008 Aluminium and aluminium alloys - Extruded round, coiled tube for general applications - Specification  
EN 13958 2008 Aluminium and aluminium alloys - Cold drawn, round, coiled tube for general applications - Specification  
EN 13981-1 2003 Aluminium and aluminium alloys - Products for structural railway applications - Technical conditions for inspection and delivery - Part 1: Extruded products  
EN 13981-2 2004 Aluminium and aluminium alloys - Products for structural railway applications - Technical conditions for inspection and delivery - Part 2: Plates and sheets  
EN 13981-3 2006 Aluminium and aluminium alloys - Products for structural railway applications - Technical conditions for inspection and delivery - Part 3: Castings  
EN 13981-4 2006 Aluminium and aluminium alloys - Products for structural railway applications - Technical conditions for inspection and delivery - Part 4: Forgings  
EN 14121 2009 Aluminium and aluminium alloys - Aluminium sheet, strip and plate for electrotechnical applications  
EN 14242 2004 Aluminium and aluminium alloys - Chemical analysis - Inductively coupled plasma optical emission spectral analysis  
EN 14286 2008 Aluminium and aluminium alloys - Weldable rolled products for tanks for the storage and transportation of dangerous goods  
EN 14287 2004 Aluminium and aluminium alloys - Specific requirements on the chemical composition of products intended to be used for the manufacture of packaging and packaging components  
EN 14361 2004 Aluminium and aluminium alloys - Chemical analysis - Sampling from metal melts  
EN 14726 2005 Aluminium and aluminium alloys - Chemical analysis - Guideline for spark optical emission spectrometric analysis  
EN 15088 2005 Aluminium and aluminium alloys - Structural products for construction works - Technical conditions for inspection and delivery  
EN ISO 15546 2007 Petroleum and natural gas industries - Aluminium alloy drill pipe  


Date Published: Apr-2011




The KEY to METALS database brings global metal properties together into one integrated and searchable database. Quick and easy access to the mechanical properties, chemical composition, cross-reference tables, and more provide users with an unprecedented wealth of information. Click the buttons below to learn more from the Guided Tour or to test drive the KEY to METALS database.