Review of JIS Standards for steel consists of 3 volumes. It contains formally
approved JIS standard classifications, guides, practices, specifications,
test methods and terminology and related material such as proposals.
The following data is given for each standard: standard number and year,
grade, chemical composition, and mechanical properties (yield point,
tensile strength, notch toughness). When deemed useful, steel type,
manufacturing method, thickness of plate, heat treatment and other data are described.
This group of JIS standard specifications covers carbon and alloy steel plates for boilers and other pressure vessels, sheets and strips, high-strength low-alloy steels, heat-treatable steels, hot and cold-rolled plates for cold forming and steel bars. This article also contains standards for various types of steel pipes which specify requirements for high-temperature service, ordinary use, and special applications such as fire protection use. Specifications for steel tubes list standard requirements for boiler and superheater tubes, general service tubes, steel tubes in refinery service, heat exchanger and condenser tubes, mechanical tubing, and structural tubing. Steel casting specifications call out the standard properties for pressure purposes. Group of standards for tool steels, stainless and heat resisting steels is also presented.
|
JIS G 3101
|
1987
|
Rolled steels for general structure
|
|
JIS G 3103
|
1987
|
Plates for boilers and other pressure vessels
|
|
JIS G 3104
|
1987
|
Steel bars for rivets
|
|
JIS G 3105
|
1987
|
Steel bars for chains
|
|
JIS G 3106
|
1988
|
Rolled steels for welded structure
|
|
JIS G 3108
|
1987
|
Carbon steels
|
|
JIS G 3114
|
1988
|
Atmospheric corrosion resisting steels
|
|
JIS G 3115
|
1990
|
Plates for pressure vessels
|
|
JIS G 3116
|
1990
|
Sheets, plates and strip for gas cylinders
|
|
JIS G 3118
|
1987
|
Plates for pressure vessels
|
|
JIS G 3119
|
1987
|
Alloyed plates for boilers and other pressure vessels
|
|
JIS G 3120
|
1987
|
Plates quenched and tempered for pressure vessels
|
|
JIS G 3124
|
1987
|
High strength and tempered for pressure vessels
|
|
JIS G 3125
|
1987
|
Atmospheritic corrosion pressure vessels
|
|
JIS G 3126
|
1990
|
Plates for pressure vessels
|
|
JIS G 3127
|
1990
|
Plates for pressure vessels
|
|
JIS G 3128
|
1987
|
Plates for welded structure
|
|
JIS G 3131
|
1990
|
Sheet and strip
|
|
JIS G 3132
|
1990
|
Strip for pipes and tubes
|
|
JIS G 3141
|
1990
|
Sheet and strip
|
|
JIS G 3202
|
1988
|
Forgings for pressure vessels
|
|
JIS G 3203
|
1988
|
Forgings for pressure vessels
|
|
JIS G 3204
|
1988
|
Quenched and tempered forgings for pressure vessels
|
|
JIS G 3205
|
1988
|
Forgings for pressure vessels
|
|
JIS G 3311
|
1988
|
Cold rolled special strip
|
|
JIS G 3441
|
1988
|
Tubes for machine purpose
|
|
JIS G 3445
|
1988
|
Tubes
|
|
JIS G 3454
|
1988
|
Pipes for pressure service
|
|
JIS G 3455
|
1988
|
Pipes for high pressure service
|
|
JIS G 3457
|
1988
|
Arc welded pipes
|
|
JIS G 3458
|
1988
|
Pipes
|
|
JIS G 3460
|
1988
|
Pipes for low temperature service
|
|
JIS G 3464
|
1988
|
Boiler and heat exchanger tubes
|
|
JIS G 3462
|
1988
|
Boiler and heat exchanger tubes
|
|
JIS G 3464
|
1988
|
Heat exchangers tubes for low temperature service
|
|
JIS G 3467
|
1988
|
Tubes for fired heater
|
|
JIS G 3444
|
1988
|
Tubes for general structural purposes
|
|
JIS G 3466
|
1988
|
Square pipes for general structural purpose
|
|
JIS G 3505
|
1980
|
Wire rods
|
|
JIS G 3506
|
1980
|
Wire rods
|
|
JIS G 3507
|
1991
|
Wire rods for cold heading and cold forging
|
|
JIS G 3508
|
1991
|
Boron wire rod for cold heading and cold forging
|
|
JIS G 3566
|
1988
|
|
|
JIS G 4051
|
1979
|
Carbon steels
|
|
JIS G 4052
|
1979
|
Structural steels with specified hardenability bands
|
|
JIS G 4102
|
1979
|
Ni-Cr steels
|
|
JIS G 4103
|
1979
|
Ni-Cr-Mo steels
|
|
JIS G 4104
|
1979
|
Cr steels
|
|
JIS G 4105
|
1979
|
Cr-Mo steels
|
|
JIS G 4106
|
1979
|
Mn and Mn-Cr steels
|
|
JIS G 4107
|
1988
|
Bolting material
|
|
JIS G 4108
|
1988
|
Bolting material
|
|
JIS G 4109
|
1987
|
Plates for pressure vessels
|
|
JIS G 4202
|
1979
|
Al-Cr-Mo steels
|
|
JIS G 4410
|
1984
|
Hollow drill steels
|
|
JIS G 4805
|
1990
|
Bearing steels
|
|
JIS G 3214
|
1991
|
Forgings for pressure vessels
|
|
JIS G 3446
|
1991
|
Tubes for machine and structural purpose
|
|
JIS G 3459
|
1988
|
Pipes
|
|
JIS G 4303
|
1991
|
Bars
|
|
JIS G 4304
|
1991
|
Hot rolled sheets and plates
|
|
JIS G 4305
|
1991
|
Cold rolled sheets and plates
|
|
JIS G 4308
|
1991
|
Steel wire rod
|
|
JIS G 4309
|
1988
|
Wire
|
|
JIS G 4311
|
1991
|
Heat resisting steel bars
|
|
JIS G 4312
|
1991
|
Heat resisting steel sheets and plates
|
|
JIS G 4313
|
1988
|
Cold rolled strip for springs
|
|
JIS G 4314
|
1988
|
Wires for springs
|
|
JIS G 4315
|
1988
|
Wire for cold heading
|
|
JIS G 4316
|
1991
|
Welding wire
|
|
JIS G 4318
|
1991
|
Cold drawn bars
|
|
JIS G 4901
|
1991
|
Superalloy bars
|
|
JIS G 4902
|
1991
|
Superalloy sheets
|
|
JIS G 4903
|
1991
|
Seamless pipes
|
|
JIS G 4904
|
1991
|
Seamless pipes
|
|
JIS G 4801
|
1984
|
Spring steels
|
|
JIS G 4802
|
1983
|
Cold-rolled strips for springs
|
|
JIS G 4804
|
1983
|
Free cutting steels
|
|
JIS G 5101
|
1991
|
Steel castings
|
|
JIS G 5102
|
1991
|
Steel castings
|
|
JIS G 5111
|
1991
|
Steel casting
|
|
JIS G 5131
|
1991
|
Steel castings
|
|
JIS G 5151
|
1991
|
Steel castings
|
|
JIS G 5152
|
1991
|
Steel casting
|
|
JIS G 5201
|
1991
|
Centrifugally cast steel pipes
|
|
JIS G 5202
|
1991
|
Centrifugally cast steel pipes
|