Standard Number |
Last version |
Description |
Status |
| A 167 |
2009 |
Stainless and Heat-Resisting Chromium-Nickel Steel Plate, Sheet, and Strip |
/42/ |
| A 176 |
2009 |
Stainless and Heat-Resisting Chromium Steel Plate, Sheet, and Strip |
/31/ |
| A 177 |
|
High-Strength Stainless and Chromium-Nickel Steel Sheet and Strip |
Replaced by A 666 /1/ |
| A 193/A 193M |
2009 |
Alloy-Steel and Stainless Steel Bolting Materials for High Temperature or High Pressure Service and Other Special Purpose Applications |
/58/ |
| A 213/A 213M |
2009 |
Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes |
/86/ |
| A 225/A 225M |
2007 |
Pressure Vessel Plates, Alloy Steel, Manganese-Vanadium-Nickel |
/2/ |
| A 240/A 240M |
2009 |
Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications |
/208/ |
| A 249/A 249M |
2008 |
Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes |
/87/ |
| A 263 |
2009 |
Stainless Chromium Steel-Clad Plate |
/1/ |
| A 264 |
2009 |
Stainless Chromium-Nickel Steel-Clad Plate |
/1/ |
| A 270 |
2008 |
Seamless and Welded Austenitic Stainless Steel Sanitary Tubing |
/18/ |
| A 271 |
1996 |
Seamless Austenitic Chromium-Nickel Steel Still Tubes for Refinery Service |
Replaced by A 213/A 213M /9/ |
| A 276 |
2008 |
Stainless Steel Bars and Shapes |
/79/ |
| A 296 |
|
Corrosion-Resistant Iron-Chromium and Iron-Chromium Nickel and Nickel-B Alloy Castings |
Replaced by A 743/A 743M /no materials/ |
| A 298 |
|
Corrosion-Resistant Chromium and Chromium-Nickel Steel Covered Welding Electrodes |
Withdrawn 1970 /no materials/ |
| A 299/A 299M |
2004 |
Pressure Vessel Plates, Carbon Steel, Manganese-Silicon |
/2/ |
| A 312/A 312M |
2009 |
Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes |
/72/ |
| A 313/A 313M |
2008 |
Stainless Steel Spring Wire |
/20/ |
| A 314 |
2008 |
Stainless Steel Billets and Bars for Forging |
/103/ |
| A 320/A 320M |
2008 |
Alloy-Steel and Stainless Steel Bolting Materials for Low-Temperature Service |
/39/ |
| A 358/A 358M |
2008 |
Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications |
/67/ |
| A 368 |
2009 |
Stainless Steel Wire Strand |
/12/ |
| A 371 |
|
Corrosion-Resisting Chromium and Chromium-Nickel Steel Welding Rods and Bare Electrodes |
Withdrawn 1969 /no materials/ |
| A 376/A 376M |
2000 |
Seamless Austenitic Steel Pipe for High-Temperature Central-Station Service |
/19/ |
| A 380 |
2006 |
Standard Practice for Cleaning, Descaling, and Passivation of Stainless Steel Parts, Equipment, and Systems |
/no materials/ |
| A 403/A 403M |
2007 |
Wrought Austenitic Stainless Steel Piping Fittings |
/81/ |
| A 409/A 409M |
2008 |
Welded Large Diameter Austenitic Steel Pipe for Corrosive or High-Temperature Service |
/38/ |
| A 412 |
|
Stainless and Heat-Resisting Chromium-Nickel-Manganese Steel Plate, Sheet, and Strip |
Withdrawn 1989 /7/ |
| A 429 |
|
Hot- and Cold-Finished Bars of Stainless and Heat-Resisting Chromium-Nickel-Manganese Steel |
Replaced by A 276 /no materials/ |
| A 451/A 451M |
2006 |
Centrifugally Cast Austenitic Steel Pipe for High-Temperature Service |
/13/ |
| A 452 |
1988 |
Centrifugally Cast Austenitic Steel Cold-Wrought Pipe for High-Temperature Service |
Withdrawn 1995 /3/ |
| A 478 |
2008 |
Chromium-Nickel Stainless Steel Weaving and Knitting Wire |
/24/ |
| A 479/A 479M |
2008 |
Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels |
/80/ |
| A 480/A 480M |
2009 |
General Requirements for Flat-Rolled Stainless and Heat-Resisting Steel Plate, Sheet, and Strip |
/no materials/ |
| A 484/A 484M |
2009 |
General Requirements for Stainless Steel Bars, Billets, and Forgings |
/no materials/ |
| A 492 |
2009 |
Stainless Steel Rope Wire |
/12/ |
| A 493 |
2009 |
Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging |
/34/ |
| A 511/A 511M |
2008 |
Seamless Stainless Steel Mechanical Tubing |
/29/ |
| A 554 |
2008 |
Welded Stainless Steel Mechanical Tubing |
/19/ |
| A 555/A 555M |
2009 |
General Requirements for Stainless Steel Wire and Wire Rods |
/no materials/ |
| A 564/A 564M |
2009 |
Hot-Rolled and Cold-Finished Age-Hardening Stainless Steel Bars and Shapes |
/21/ |
| A 565/A 565M |
2009 |
Martensitic Stainless Steel Bars for High-Temperature Service |
/11/ |
| A 580/A 580M |
2008 |
Stainless Steel Wire |
/79/ |
| A 581/A 581M |
2009 |
Free-Machining Stainless Steel Wire and Wire Rods |
/24/ |
| A 582/A 582M |
2005 |
Free-Machining Stainless Steel Bars |
/32/ |
| A 632 |
2004 |
Seamless and Welded Austenitic Stainless Steel Tubing (Small-Diameter) for General Service |
/18/ |
| A 651 |
1984 |
Stainless Steel Water-DWV Tube |
Withdrawn 1986 /7/ |
| A 666 |
2003 |
Annealed or Cold-Worked Austenitic Stainless Steel Sheet, Strip, Plate, and Flat Bar |
/34/ |
| A 669 |
1983 |
Seamless Ferritic-Austenitic Alloy Steel Tubes |
Replaced by A789/A789M /no materials/ |
| A 688/A 688M |
2008 |
Welded Austenitic Stainless Steel Feedwater Heater Tubes |
/22/ |
| A 693 |
2006 |
Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip |
/25/ |
| A 708 |
1979 |
Practice for Detection of Susceptibility to Intergranular Corrosion in Severely Sensitized Austenitic Stainless Steel |
Withdrawn 1988 /no materials/ |
| A 731/A 731M |
|
Seamless, Welded Ferritic, and Martensitic Stainless Steel Pipe |
Replaced by A268/A268M /7/ |
| A 756 |
2009 |
Stainless Anti-Friction Bearing Steel |
/2/ |
| A 771/A 771M |
2001 |
Seamless Austenitic and Martensitic Stainless Steel Tubing for Liquid Metal-Cooled Reactor Core Components |
Withdrawn 2004 /3/ |
| A 774/A 774M |
2006 |
As-Welded Wrought Austenitic Stainless Steel Fittings for General Corrosive Service at Low and Moderate Temperatures |
/5/ |
| A 778 |
2001 |
Welded, Unannealed Austenitic Stainless Steel Tubular Products |
/10/ |
| A 789/A 789M |
2008 |
Seamless and Welded Ferritic/Austenitic Stainless Steel Tubing for General Service |
/25/ |
| A 790/A 790M |
2009 |
Seamless and Welded Ferritic/Austenitic Stainless Steel Pipe |
/29/ |
| A 793 |
2009 |
Rolled Floor Plate, Stainless Steel |
/4/ |
| A 803/A 803M |
2008 |
Welded Ferritic Stainless Steel Feedwater Heater Tubes |
/21/ |
| A 813/A 813M |
2009 |
Single- or Double-Welded Austenitic Stainless Steel Pipe |
/60/ |
| A 814/A 814M |
2008 |
Cold-Worked Welded Austenitic Stainless Steel Pipe |
/63/ |
| A 815/A 815M |
2009 |
Wrought Ferritic, Ferritic/Austenitic, and Martensitic Stainless Steel Piping Fittings |
/54/ |
| A 826/A 826M |
2001 |
Seamless Austenitic and Martensitic Stainless Steel Duct Tubes for Liquid Metal-Cooled Reactor Core Components |
Withdrawn 2004 /4/ |
| A 831/A 831M |
2000 |
Austenitic and Martensitic Stainless Steel Bars, Billets, and Forgings for Liquid Metal Cooled Reactor Core Components |
/4/ |
| A 838 |
2007 |
Free-Machining Ferritic Stainless Soft Magnetic Alloy Bar for Relay Applications |
/5/ |
| A 860/A 860M |
2009 |
Wrought High-Strength Low-Alloy Steel Butt-Welding Fittings |
/6/ |
| A 872/A 872M |
2007 |
Centrifugally Cast Ferritic/Austenitic Stainless Steel Pipe for Corrosive Environments |
/4/ |
| A 873/A 873M |
1993 |
Steel Sheet and Strip, Chromium-Molybdenum Alloy, for Pressure Vessels |
Withdrawn 1997 /no materials/ |
| A 887 |
2009 |
Borated Stainless Steel Plate, Sheet, and Strip for Nuclear Application |
/16/ |
| A 895 |
2009 |
Free-Machining Stainless Steel Plate, Sheet, and Strip |
/16/ |
| A 908 |
2008 |
Stainless Steel Needle Tubing |
/1/ |
| A 928/A 928M |
2008 |
Ferritic/Austenitic (Duplex) Stainless Steel Pipe Electric Fusion Welded with Addition of Filler Metal |
/15/ |
| A 943/A 943M |
2005 |
Spray-Formed Seamless Austenitic Stainless Steel Pipes |
/40/ |
| A 947M |
2004 |
Textured Stainless Steel Sheet [Metric] |
/no materials/ |
| A 949/A 949M |
2005 |
Spray-Formed Seamless Ferritic/Austenitic Stainless Steel Pipe |
/9/ |
| A 953 |
2002 |
Austenitic Chromium-Nickel-Silicon Alloy Steel Seamless and Welded Tubing |
Withdrawn 2004 /1/ |
| A 954 |
2002 |
Austenitic Chromium-Nickel-Silicon Alloy Steel Seamless and Welded Pipe |
Withdrawn 2005 /1/ |
| A 955/A 955M |
2009 |
Deformed and Plain Stainless-Steel Bars for Concrete Reinforcement |
/41/ |
| A 959 |
2009 |
Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels |
/219/ |
| A 967 |
2005 |
Chemical Passivation Treatments for Stainless Steel Parts |
/no materials/ |
| A 988/A 988M |
2007 |
Hot Isostatically-Pressed Stainless Steel Flanges, Fittings, Valves, and Parts for High Temperature Service |
/28/ |
| A 989/A 989M |
2007 |
Hot Isostatically-Pressed Alloy Steel Flanges, Fittings, Valves, and Parts for High Temperature Service |
/5/ |
| A 999/A 999M |
2004 |
General Requirements for Alloy and Stainless Steel Pipe |
/no materials/ |
| A 1010/A 1010M |
2009 |
Higher-Strength Martensitic Stainless Steel Plate, Sheet , and Strip |
/4/ |
| A 1011/A 1011M |
2009 |
Steel, Sheet and Strip, Hot-Rolled, Carbon, Structural, High-Strength Low-Alloy, High-Strength Low-Alloy with Improved Formability, and Ultra-High Strength |
/35/ |
| A 1012 |
2007 |
Seamless and Welded Ferritic, Austenitic and Duplex Alloy Steel Condenser and Heat Exchanger Tubes With Integral Fins |
Withdrawn 2007 /no materials/ |
| A 1016/A 1016M |
2008 |
General Requirements for Ferritic Alloy Steel, Austenitic Alloy Steel, and Stainless Steel Tubes |
/no materials/ |
| A 1022/A 1022M |
2007 |
Deformed and Plain Stainless Steel Wire and Welded Wire for Concrete Reinforcement |
/1/ |
| A 1023/A 1023M |
2007 |
Stranded Carbon Steel Wire Ropes for General Purposes |
/no materials/ |
| A 1024/A 1024M |
2007 |
Steel Line Pipe, Black, Plain-End, Seamless |
/5/ |
| A 1026 |
2003 |
Alloy Steel Structural Shapes for Use in Building Framing |
/2/ |
| A 1028 |
2008 |
Stainless Steel Bars for Compressor and Turbine Airfoils |
/12/ |
| A 1053/A 1053M |
2006 |
Welded Ferritic-Martensitic Stainless Steel Pipe |
/1/ |
| B 625 |
2005 |
Plate, sheet, and strip in the annealed temper |
/6/ |