Euronorm Standard List: Stainless Steels and Welding and Filler Materials

Abstract:

The creation of the EEC (European Economic Community) has made it necessary to establish common standards named "European Norms" (EN), therefore standardizing the common language across Europe. Since 1988 a new series of 'mandatory' European standards (EN) has been created, to replace national standards, such as BS, DIN, SS and NF, throughout 18 countries of Western Europe.

The EN Designation System uses an alpha-numerical index to denote the key information about the material including mechanical properties, tensile strength and potential usage.

For more information on the EN designation system see Introduction to the Euronorm Standard Designation System.

The list of standards below cover among other things:

  • A range of stainless steels used for general use and for multiple applications such as surgical tool production
  • A range of stainless steel rods, tubes, and spring wires
  • Various materials used in the production of welding consumables
  • Electrode production for multiple welding processes


Stainless Steel

Standard
Number
Last
version
Description Status
EN 10088-1 2005 Stainless steels - Part 1: List of stainless steels  
EN 10088-2 2005 Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes  
EN 10088-3 2005 Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes  
EN 10088-4 2009 Stainless steels - Part 4: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for construction purposes  
EN 10088-5 2009 Stainless steels - Part 5: Technical delivery conditions for bars, rods, wire, sections and bright products of corrosion resisting steels for construction purposes  
EN 10095 1999 Heat resisting steels and nickel alloys  
EN 10151 2002 Stainless steel strip for springs - Technical delivery conditions  
EN 10269 2008 Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties  
EN 10270-3 2001 Steel wire for mechanical springs - Part 3: Stainless spring steel wire  
EN 10272 2007 Stainless steel bars for pressure purposes  
EN 10296-2 2005 Welded circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel  
EN 10297-2 2005 Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel  
EN ISO 7153-1 2000 Surgical instruments - Metallic materials - Part 1: Stainless steel  
EN ISO 9445 2006 Continuously cold-rolled stainless steel narrow strip, wide strip, plate/sheet and cut lengths - Tolerances on dimensions and form  
EN ISO 11960 2004 Petroleum and natural gas industries - Steel pipes for use as casing or tubing for wells  
EN ISO 11961 2008 Petroleum and natural gas industries - Steel pipes for use as drill pipe - Specification  
EN ISO 13680 2001 Petroleum and natural gas industries - Corrosion-resistant alloy seamless tubes for use as casing, tubing and coupling stock - Technical delivery conditions  
ENV 1090-6 1999 Execution of steel structures - Part 6: Supplementary rules for stainless steel  

Welding and Filler materials

Standard
Number
Last
version
Description Status
EN ISO 2560 2005 Welding consumables - Covered electrodes for manual metal arc welding of non-alloy and fine grain steels  
EN ISO 18276 2006 Welding consumables - Tubular cored electrodes for gas-shielded and non-gas-shielded metal arc welding of high-strength steels - Classification  
EN ISO 17634 2006 Welding consumables - Tubular cored electrodes for gas shielded metal arc welding of creep-resisting steels - Classification  
EN ISO 14343 2007 Welding consumables - Wire electrodes, strip electrodes, wires and rods for fusion welding of stainless and heat resisting steels - Classification  
EN 758 1997 Welding consumables - Tubular cored electrodes for metal arc welding with and without a gas shield of non alloy and fine grain steels  
EN 757 1997 Welding consumables - Covered electrodes for manual metal arc welding of high strength steels  
EN 10253-1 1999 Butt-welding pipe fittings - Part 1: Wrought carbon steel for general use and without specific inspection requirements  
EN 10253-2 2007 Butt-welding pipe fittings - Part 2: Non alloy and ferritic alloy steels with specific inspection requirements  
EN 10253-3 2008 Butt-welding pipe fittings - Part 3: Wrought austenitic and austenitic-ferritic (duplex) stainless steels without specific inspection requirements  
EN 10253-4 2008 Butt-welding pipe fittings - Part 4: Wrought austenitic and austenitic-ferritic (duplex) stainless steels with specific inspection requirements  
EN 12070 1999 Welding consumables - Wire electrodes, wires and rods for arc welding of creep-resisting steels  
EN 12071 1999 Welding consumables - Tubular cored electrodes for gas shielded metal arc welding of creep-resisting steels  
EN 12072 1999 Welding consumables - Wire electrodes, wires and rods for arc welding of stainless and heat-resisting steels  
EN 12535 2000 Welding consumables - Tubular cored electrodes for gas shielded metal arc welding of high strength steels  
EN 12536 2000 Welding consumables - Rods for gas welding of non alloy and creep-resisting steels  
EN 1599 1997 Welding consumables - Covered electrodes for manual metal arc welding of creep-resisting steels  
EN 1600 1997 Welding consumables - Covered electrodes for manual metal arc welding of stainless and heat resisting steels  
EN 1668   Welding consumables - Rods, wires and deposits for tungsten inert gas welding of non alloy and fine grain steels  
EN 27963 1992 Welds in steel; calibration block no. 2 for ultrasonic examination of welds  
EN 440 1994 Welding consumables - Wire electrodes and deposits for gas shielded metal arc welding of non alloy and fine grain steels  
EN 756 2004 Welding consumables - Solid wire, solid wire-flux and tubular cored electrode-flux combinations for submerged arc welding of non alloy and fine grain steels  
EN 757 1997 Welding consumables - Covered electrodes for manual metal arc welding of high strength steels  
EN 758 1997 Welding consumables - Tubular cored electrodes for metal arc welding with and without a gas shield of non alloy and fine grain steels  
EN ISO 14343 2007 Welding consumables - Wire electrodes, strip electrodes, wires and rods for fusion welding of stainless and heat resisting steels - Classification  
EN ISO 17634 2006 Welding consumables - Tubular cored electrodes for gas shielded metal arc welding of creep-resisting steels - Classification  
EN ISO 18276 2006 Welding consumables - Tubular cored electrodes for gas-shielded and non-gas-shielded metal arc welding of high-strength steels - Classification  
EN ISO 2560 2005 Welding consumables - Covered electrodes for manual metal arc welding of non-alloy and fine grain steels  
EN ISO 3580 2008 Welding consumables - Covered electrodes for manual metal arc welding of creep-resisting steels - Classification (ISO 3580:2004)  

Doorzoek Kennisbank

Geef een zoekterm in:

Zoeken op

Volledige tekst
Kernwoorden

Titels
Abstract:

With Total Materia finding information about a metal standard specification, its current status and the materials it defines is one click away.

Within seconds it is also possible for you to find related detailed material property data or search equivalent materials starting from the Total Materia standard list.

To get started, click on the standard list button in the menu bar.


By simply selecting a Standard Development Organization (SDO) and/or typing the standard number, you receive immediate results from the multi-lingual database containing over 30,000 standards.

For example, you can review all metal standards from EN by selecting this SDO from the popup.


The result list consists of over 1000 EN metal standards. Information includes: standard description, year of last issue, current status (valid, replaced, etc.) and a hot link to the materials defined by this standard.


By simply clicking the materials hot link, you can see a list of metal materials defined by the selected standard.


From the list of materials, you can review detailed properties and equivalents of each material.


For you’re a chance to take a test drive of the Total Materia database, we invite you to join a community of over 150,000 registered users through the Total Materia Free Demo.