Euronorm Standard List: Aerospace Series

Rezumat:

The creation of the EEC (European Economic Community) has made it necessary to establish common standards named "European Norms" (EN), therefore standardizing the common language across Europe. Since 1988 a new series of 'mandatory' European standards (EN) has been created, to replace national standards, such as BS, DIN, SS and NF, throughout 18 countries of Western Europe.

Aluminum is one of the most economical and structurally effective materials used for commercial and military equipment applications. Some of its attractive properties include: good appearance, easy of fabrication, good corrosion resistance, low density and high strength-to-weight ratio, high fracture toughness etc.

For more information on the EN designation system see Introduction to the Euronorm Standard Designation System.

The list of standards below cover among other things:

  • A range of aluminium alloys used for specialized aerospace applications
  • Plates, sheets and strip aluminium for various uses in the aerospace industry
  • Aluminium hand forgings

Click on the below links to see lists of Euronorm standards covering the following material categories:

Aluminium Wrought/Castings/Ingots/Remelting

Aluminium Materials


Aerospace Materials

Standard
Number
Last
version
Description Status
EN 2044 2001 Aerospace series - Round bars, drawn, in aluminium and aluminium alloys - Tolerance class h 11 - Diameter 4 mm <= D <= 63 mm - Dimensions  
EN 2045 2001 Aerospace series - Square bars, drawn in aluminium and aluminium alloys - Tolerance class h 11 - Thickness 6 mm <= a <= 50 mm - Dimensions  
EN 2046 2001 Aerospace series - Hexagonal bars, drawn in aluminium and aluminium alloys - Tolerance class h 11 - Width across flats 7 mm <= a <= 50 mm - Dimensions  
EN 2047 2001 Aerospace series - Beaded L-section extruded, in aluminium alloys - Dimensions  
EN 2048 2001 Aerospace series - Extruded L-section, in aluminium alloys - Dimensions  
EN 2049 2001 Aerospace series - Extruded channel section, in aluminium alloys - Dimensions  
EN 2050 2001 Aerospace series - Extruded T-section, in aluminium alloys - Dimensions  
EN 2066 2001 Aerospace series - Extruded section in aluminium alloys - General tolerances  
EN 2070-1 1989 Aerospace series - Aluminium and aluminium alloy wrought products - Technical specification - Part 1: General requirements  
EN 2070-2 1989 Aerospace series - Aluminium and aluminium alloy wrought products - Technical specification - Part 2: Sheet, strip formed profiles and plate  
EN 2070-3 1989 Aerospace series - Aluminium and aluminium alloy wrought products - Technical specification - Part 3: Bar and section  
EN 2070-4 1989 Aerospace series - Aluminium and aluminium alloy wrought products - Technical specification - Part 4: Tube for structures  
EN 2070-5 1989 Aerospace series - Aluminium and aluminium alloy wrought products - Technical specification - Part 5: Tube used under pressure  
EN 2070-6 1989 Aerospace series - Aluminium and aluminium alloy wrought products - Technical specification - Part 6: Rivet wire  
EN 2070-7 1989 Aerospace series - Aluminium and aluminium alloy wrought products - Technical specification - Part 7: Wrought forging stock  
EN 2071 2001 Aerospace series - Sheets in aluminium and aluminium alloys - Thickness 0,25 mm <= a <= 6 mm - Dimensions  
EN 2072 2005 Aerospace series - Aluminium AL-P1050A - H14 - Sheet and strip - 0,4 mm <= a <= 6 mm  
EN 2076-1 1989 Aerospace series - Aluminium and magnesium alloy ingots and castings - Technical specification - Part 1: General requirements  
EN 2076-2 1989 Aerospace series - Aluminium and magnesium alloy ingots and castings - Technical specification - Part 2: Ingots for remelting  
EN 2076-3 1989 Aerospace series - Aluminium and magnesium alloy ingots and castings - Technical specification - Part 3: Pre-production and production castings  
EN 2082-1 1989 Aerospace series - Aluminium alloy forging stock and forgings - Technical specification - Part 1: General requirements  
EN 2082-2 1993 Aerospace series - Aluminium alloy forging stock and forgings - Technical specification - Part 2: Forging stock  
EN 2082-3 1989 Aerospace series - Aluminium alloy forging stock and forgings - Technical specification - Part 3: Pre-production and production forgings  
EN 2085 2004 Aerospace series - Aluminium alloy AL-P2618A-T6 - Hand and die forgings - a <= 150 mm  
EN 2086 2004 Aerospace series - Aluminium alloy AL-P2618A-T851 - Hand and die forgings - a <= 150 mm  
EN 2087 2005 Aerospace series - Aluminium alloy AL-P2014A-T6 or T62 - Clad sheet and strip - 0,4 mm <= a <= 6 mm  
EN 2088 2005 Aerospace series - Aluminium alloy AL-P2014A-T4 or T42 - Clad sheet and strip - 0,4 mm <= a <= 6 mm  
EN 2089 2005 Aerospace series - Aluminium alloy AL-P2014A-T6 or T62 - Sheet and strip - 0,4 mm <= a <= 6 mm  
EN 2090 2005 Aerospace series - Aluminium alloy AL-P2024-T3 - Clad sheet and strip 0,3 mm <= a <= 6 mm  
EN 2092 2005 Aerospace series - Aluminium alloy AL-P7075-T6 or T62 - Clad sheet and strip - 0,4 mm <= a <= 6 mm  
EN 2093 1993 Aerospace series - Aluminium alloy AL-P7009-T74 - Hand forgings 20 mm <= a <= 150 mm  
EN 2094 1992 Aerospace series - Aluminium alloy AL-P7009-T74 - Die forgings 3 mm <= a <= 150 mm  
EN 2100 1992 Aerospace series - Aluminium alloy AL-P2014A-T4511 - Extruded bars and sections a or D <= 200 mm  
EN 2126 1992 Aerospace series - Aluminium alloy AL-P7075-T651 - Plates 6 mm < a <= 80 mm  
EN 2127 1992 Aerospace series - Aluminium alloy AL-P7075-T73511 - Extruded bars and sections a or D <= 100 mm  
EN 2128 1992 Aerospace series - Aluminium alloy AL-P7075-T7351 - Drawn bars 6 mm <= a or D <= 75 mm  
EN 2131 2001 Aerospace series - Plates in aluminium alloys - Thickness 6 mm < a <= 160 mm - Dimensions  
EN 2134 2001 Aerospace series - Round bars, extruded in aluminium and aluminium alloys - Diameter 10 mm <= D <= 220 mm - Dimensions  
EN 2256 2004 Aerospace series - Aluminium alloy AL-P2618A - T852 - Hand and die forgings - a <= 150 mm  
EN 2284 1991 Aerospace series - Sulphuric acid anodizing of aluminium and wrought aluminium alloys  
EN 2318 1992 Aerospace series - Aluminium alloy AL-P2024-T3511 - Extruded bars and sections 1,2 mm <= a or D <= 150 mm  
EN 2326 1992 Aerospace series - Aluminium alloy AL-P6082-T6 - Extruded bars and sections a or D <= 200 mm  
EN 2381 1992 Aerospace series - Aluminium alloy AL-P7009-T7452 - Hand forgings 40 mm <= a <= 150 mm  
EN 2384 1992 Aerospace series - Aluminium alloy AL-P2014A T6511 - Extruded bars and sections a or D <= 150 mm  
EN 2385 1992 Aerospace series - Aluminium alloy AL-P7009-T74511 - Extruded bars and sections a or D <= 125 mm  
EN 2395 2005 Aerospace series - Aluminium alloy AL-P2014A-T4 or T42 - Sheet and strip - 0,4 mm <= a <= 6 mm  
EN 2422 2005 Aerospace series - Aluminium alloy AL-P2124-T351 - Plate - 25 mm < a <= 120 mm  
EN 2486 2005 Aerospace series - Aluminium alloy AL-P2618A - Forging stock  
EN 2511 2005 Aerospace series - Aluminium alloy AL-P7075-T7351 - Plate - 6 mm < a <= 100 mm  
EN 2599 2001 Aerospace series - Strips in aluminium and aluminium alloys - Thickness 0,25 mm <= a <= 3,2 mm - Dimensions  
EN 2630 1993 Aerospace series - Aluminium alloy AL-P7009-T74511 - Extruded bars and sections a or D <= 125 mm with peripheral coarse grain control  
EN 2632 2005 Aerospace series - Aluminium alloy AL-P7075-T73511 - Extruded bar and section - a or D <= 100 mm with peripheral coarse grain control  
EN 2633 1993 Aerospace series - Aluminium alloy AL-P2024-T3511 - Extruded bars and sections 1,2 mm <= a or D <= 150 mm with peripheral coarse grain control  
EN 2635 2005 Aerospace series - Aluminium alloy AL-P2014A-T6511 - Extruded bar and section - a or D <= 200 mm with peripheral coarse grain control  
EN 2636 1993 Aerospace series - Aluminium alloy AL-P6082-T6 - Extruded bars and sections a or D <= 200 mm with peripheral coarse grain control  
EN 2681 2004 Aerospace series - Aluminium alloy AL-P7010-T74 - Hand and die forgings - a <= 150 mm  
EN 2684 2004 Aerospace series - Aluminium alloy AL-P7010-T7651 - Plate - 6 mm < a <= 140 mm  
EN 2687 2004 Aerospace series - Aluminium alloy AL-P7010-T7451 - Plate - 6 mm < a <= 160 mm  
EN 2693 2005 Aerospace series - Aluminium alloy AL-P5086-H111 - Sheet and strip - 0,3 mm <= a <= 6 mm  
EN 2694 2005 Aerospace series - Aluminium alloy AL-P6061-T6 or T62 - Sheet and strip - 0,4 mm <= a <= 6 mm  
EN 2695 2005 Aerospace series - Aluminium alloy AL-P6081-T6 - Sheet and strip - 0,3 mm <= a <= 6 mm  
EN 2696 2005 Aerospace series - Aluminium alloy AL-P7075-T6 or T62 - Sheet and strip - 0,4 mm <= a <= 6 mm  
EN 2702 2005 Aerospace series - Aluminium alloy AL-P6061-T6 or T62 - Drawn or extruded bar and section - a or D <= 200 mm  
EN 2703 2005 Aerospace series - Aluminium alloy AL-P2024-T4 or T42 - Clad sheet and strip - 0,3 mm <= a <= 6 mm  
EN 2802 2005 Aerospace series - Aluminium alloy AL-P7475-T761 - Sheet and strip - 0,6 mm <= a <= 6 mm  
EN 2803 2005 Aerospace series - Aluminium alloy AL-P7475-T761 - Clad sheet and strip - 1,0 mm <= a <= 6 mm  
EN 3332 2005 Aerospace series - Aluminium alloy AL-P7475-T762 - Clad sheet and strip - 1,0 mm <= a <= 6 mm  
EN 3333 2005 Aerospace series - Aluminium alloy AL-P7475-T762 - Sheet and strip - 0,6 mm <= a <= 6 mm  
EN 3335 2005 Aerospace series - Aluminium alloy AL-P7475-O2 - Sheet for superplastic forming (SPF) - 0,8 mm <= a <= 6 mm  
EN 3338 2005 Aerospace series - Aluminium alloy AL-P7050 - T74511 - Extruded bar and section - a or D <= 150 mm with peripheral coarse grain control  
EN 3339 2006 Aerospace series - Aluminium alloy AL-P7010-T76 - Die forgings - a <= 200 mm  
EN 3341 2005 Aerospace series - Aluminium alloy AL-P6061-T4 or T42 - Sheet and strip - 0,4 mm <= a <= 6 mm  
EN 3342 2005 Aerospace series - Aluminium alloy AL-P6061-T4 or T42 - Drawn or extruded bar and section - a or D <= 150 mm  
EN 3344 2005 Aerospace series - Aluminium alloy AL-P7050-T76511 - Extruded bar and section - a or D <= 150 mm with peripheral coarse grain control  
EN 3347 2005 Aerospace series - Aluminium alloy AL-P2024-T8511 - Extruded bar and section - a or D <= 150 mm with peripheral coarse grain control  
EN 3474 2005 Aerospace series - Aluminium alloy AL-P2024-T81 - Sheet and strip - 0,25 mm <= a <= 6 mm  
EN 3552 2005 Aerospace series - Aluminium alloy AL-P2618A-T6 or T62 - Clad sheet and strip - 0,4 mm <= a <= 6 mm  
EN 3553 2004 Aerospace series - Aluminium alloy AL-P2618A - T6511 - Extruded bar and section - a or D <= 160 mm  
EN 3719 2005 Aerospace series - Aluminium or aluminium alloy conductors for electrical cables - Product standard  
EN 3872 2005 Aerospace series - Aluminium alloy AL-R39002-H112 - Die forgings - a <= 200 mm  
EN 3979 2005 Aerospace series - Aluminium alloy AL-P8090-O2 - Sheet for superplastic forming (SPF) - 0,8 mm <= a <= 6 mm  
EN 3997 2007 Aerospace series - Aluminium alloy AL-P2024-T3 - Sheet and strip 0,4 mm <= a <= 6 mm  
EN 3998 2007 Aerospace series - Aluminium alloy AL-P2024-T4 or T42 - Sheet and strip 0,3 mm <= a <= 6 mm  
EN 4001 2007 Aerospace series - Aluminium alloy AL-P2024-T351 - Clad sheet and strip with improved chemical milling capability 1,6 mm <= a <= 6 mm  
EN 4003 2006 Aerospace series - Aluminium alloy AL-P2219-T87 - Sheet and strip 0,5 mm <= a <= 6 mm  
EN 4004 2007 Aerospace series - Aluminium alloy AL-P3103-H16 - Sheet and strip 0,4 mm <= a <= 6 mm  
EN 4005 2007 Aerospace series - Aluminium alloy AL-P5052-O - Sheet and strip 0,3 mm <= a <= 6 mm  
EN 4006 2007 Aerospace series - Aluminium alloy AL-P6082-T4 or T42 - Sheet and strip 0,4 mm <= a <= 6 mm  
EN 4007 2005 Aerospace series - Aluminium alloy AL-P6082-T6 or T62 - Sheet and strip - 0,4 mm <= a <= 6 mm  
EN 4099 2005 Aerospace series - Aluminium alloy AL-P2219-T6 or T62 - Clad sheet and strip - 0,5 mm <= a <= 6 mm  
EN 4100 2005 Aerospace series - Aluminium alloy AL-P2219-T6 or T62 - Sheet and strip - 0,5 mm <= a <= 6 mm  
EN 4101 2005 Aerospace series - Aluminium alloy AL-P2024-T4 - Sheet and strip with improved stretch forming capability - 0,4 mm <= a <= 6 mm  
EN 4102 2005 Aerospace series - Aluminium alloy AL-P2219-T81 - Clad sheet and strip - 0,5 mm <= a <= 6 mm  
EN 4202 2005 Aerospace series - Aluminium alloy AL-P6082-T651 - Plate - 6 mm < a <= 25 mm  
EN 4203 2005 Aerospace series - Aluminium alloy AL-P8090-T89 - Sheet - 0,6 mm <= a <= 6 mm  
EN 4204 2005 Aerospace series - Aluminium alloy AL-P8090 - T841 - Sheet - 0,6 mm <= a <= 6 mm  
EN 4209 2005 Aerospace series - Aluminium alloy AL-P2219-T851 - Plate - 6 mm < a <= 50 mm  
EN 4211 2005 Aerospace series - Aluminium alloy AL-P2024-T42 - Clad plate - 6 mm < a <= 25 mm  
EN 4212 2005 Aerospace series - Aluminium alloy AL-P5086-H111 - Plate - 6 mm < a <= 80 mm  
EN 4213 2005 Aerospace series - Aluminium alloy AL-P6061-T651 - Plate - 6 mm < a <= 80 mm  
EN 4214 2005 Aerospace series - Aluminium alloy AL-P7010-T651 - Plate - 6 mm < a <= 20 mm  
EN 4215 2005 Aerospace series - Aluminium alloy AL-P7175-T651 - Plate - 6 mm < a <= 80 mm  
EN 4247 2005 Aerospace series - Aluminium alloy AL-P2024-T42 - Plate - 6 mm < a <= 140 mm  
EN 4283 2005 Aerospace series - Aluminium alloy AL-P2219-T87 - Plate - 6 mm < a <= 40 mm  
EN 4286 2005 Aerospace series - Aluminium alloy AL-P8090-T89 - Die forgings - a <= 125 mm  
EN 4287 2005 Aerospace series - Aluminium alloy AL-P7010 - Forging stock  
EN 4291 2005 Aerospace series - Aluminium alloy AL-P8090 - Forging stock  
EN 4292 2005 Aerospace series - Aluminium alloy AL-R39002 - Forging stock  
EN 4313 2005 Aerospace series - Aluminium alloy AL-P6013-T6 - Sheet and strip - 0,5 mm <= a <= 6 mm  
EN 4324 2001 Aerospace series - Aluminium alloy AL-W42201 - Filler metal for welding - Rod  
EN 4341 2001 Aerospace series - Aluminium alloy AL-W46431 - Filler metal for welding - Wire and rod  
EN 4449 2005 Aerospace series - Aluminium alloy AL-P7050 - T76 - Sheet - 0,8 mm < = a < = 6 mm  
EN 4450 2005 Aerospace series - Aluminium alloy AL-P7050-T762 - Sheet - 0,8 mm <= a <= 6 mm  

Caută în baza de date

Introduceţi frază de căutare pentru:

Caută după

Text complet
Cuvinte cheie

Titlu
Rezumate

With Total Materia finding information about a metal standard specification, its current status and the materials it defines is one click away.

Within seconds it is also possible for you to find related detailed material property data or search equivalent materials starting from the Total Materia standard list.

To get started, click on the standard list button in the menu bar.

solution img

By simply selecting a Standard Development Organization (SDO) and/or typing the standard number, you receive immediate results from the multi-lingual database containing over 30,000 standards.

For example, you can review all metal standards from EN by selecting this SDO from the popup.

solution img

The result list consists of over 1000 EN metal standards. Information includes: standard description, year of last issue, current status (valid, replaced, etc.) and a hot link to the materials defined by this standard.

solution img

By simply clicking the materials hot link, you can see a list of metal materials defined by the selected standard.

solution img

From the list of materials, you can review detailed properties and equivalents of each material.

solution img

For you’re a chance to take a test drive of the Total Materia database, we invite you to join a community of over 150,000 registered users through the Total Materia Free Demo.