JIS-standards for steel materials


Abstract:
This group of JIS standard specifications covers carbon and alloy steel plates for boilers and other pressure vessels, sheets and strips, high-strength low-alloy steels, heat-treatable steels, hot and cold-rolled plates for cold forming and steel bars. This article also contains standards for various types of steel pipes which specify requirements for high-temperature service, ordinary use, and special applications such as fire protection use. Specifications for steel tubes list standard requirements for boiler and superheater tubes, general service tubes, steel tubes in refinery service, heat exchanger and condenser tubes, mechanical tubing, and structural tubing. Steel casting specifications call out the standard properties for pressure purposes. Group of standards for tool steels, stainless and heat resisting steels is also presented.

Review of JIS Standards for steel consists of 3 volumes. It contains formally approved JIS standard classifications, guides, practices, specifications, test methods and terminology and related material such as proposals.

Covers:

The following data is given for each standard: standard number and year, grade, chemical composition, and mechanical properties (yield point, tensile strength, notch toughness). When deemed useful, steel type, manufacturing method, thickness of plate, heat treatment and other data are described.

This group of JIS standard specifications covers carbon and alloy steel plates for boilers and other pressure vessels, sheets and strips, high-strength low-alloy steels, heat-treatable steels, hot and cold-rolled plates for cold forming and steel bars. This article also contains standards for various types of steel pipes which specify requirements for high-temperature service, ordinary use, and special applications such as fire protection use. Specifications for steel tubes list standard requirements for boiler and superheater tubes, general service tubes, steel tubes in refinery service, heat exchanger and condenser tubes, mechanical tubing, and structural tubing. Steel casting specifications call out the standard properties for pressure purposes. Group of standards for tool steels, stainless and heat resisting steels is also presented.

Group of standards for structural and constructional steels

JIS G 3101 1987 Rolled steels for general structure
JIS G 3103 1987 Plates for boilers and other pressure vessels
JIS G 3104 1987 Steel bars for rivets
JIS G 3105 1987 Steel bars for chains
JIS G 3106 1988 Rolled steels for welded structure
JIS G 3108 1987 Carbon steels
JIS G 3114 1988 Atmospheric corrosion resisting steels
JIS G 3115 1990 Plates for pressure vessels
JIS G 3116 1990 Sheets, plates and strip for gas cylinders
JIS G 3118 1987 Plates for pressure vessels
JIS G 3119 1987 Alloyed plates for boilers and other pressure vessels
JIS G 3120 1987 Plates quenched and tempered for pressure vessels
JIS G 3124 1987 High strength and tempered for pressure vessels
JIS G 3125 1987 Atmospheritic corrosion pressure vessels
JIS G 3126 1990 Plates for pressure vessels
JIS G 3127 1990 Plates for pressure vessels
JIS G 3128 1987 Plates for welded structure
JIS G 3131 1990 Sheet and strip
JIS G 3132 1990 Strip for pipes and tubes
JIS G 3141 1990 Sheet and strip
JIS G 3202 1988 Forgings for pressure vessels
JIS G 3203 1988 Forgings for pressure vessels
JIS G 3204 1988 Quenched and tempered forgings for pressure vessels
JIS G 3205 1988 Forgings for pressure vessels
JIS G 3311 1988 Cold rolled special strip
JIS G 3441 1988 Tubes for machine purpose
JIS G 3445 1988 Tubes
JIS G 3454 1988 Pipes for pressure service
JIS G 3455 1988 Pipes for high pressure service
JIS G 3457 1988 Arc welded pipes
JIS G 3458 1988 Pipes
JIS G 3460 1988 Pipes for low temperature service
JIS G 3464 1988 Boiler and heat exchanger tubes
JIS G 3462 1988 Boiler and heat exchanger tubes
JIS G 3464 1988 Heat exchangers tubes for low temperature service
JIS G 3467 1988 Tubes for fired heater
JIS G 3444 1988 Tubes for general structural purposes
JIS G 3466 1988 Square pipes for general structural purpose
JIS G 3505 1980 Wire rods
JIS G 3506 1980 Wire rods
JIS G 3507 1991 Wire rods for cold heading and cold forging
JIS G 3508 1991 Boron wire rod for cold heading and cold forging
JIS G 3566 1988
JIS G 4051 1979 Carbon steels
JIS G 4052 1979 Structural steels with specified hardenability bands
JIS G 4102 1979 Ni-Cr steels
JIS G 4103 1979 Ni-Cr-Mo steels
JIS G 4104 1979 Cr steels
JIS G 4105 1979 Cr-Mo steels
JIS G 4106 1979 Mn and Mn-Cr steels
JIS G 4107 1988 Bolting material
JIS G 4108 1988 Bolting material
JIS G 4109 1987 Plates for pressure vessels
JIS G 4202 1979 Al-Cr-Mo steels
JIS G 4410 1984 Hollow drill steels
JIS G 4805 1990 Bearing steels
JIS G 3214 1991 Forgings for pressure vessels
JIS G 3446 1991 Tubes for machine and structural purpose
JIS G 3459 1988 Pipes
JIS G 4303 1991 Bars
JIS G 4304 1991 Hot rolled sheets and plates
JIS G 4305 1991 Cold rolled sheets and plates
JIS G 4308 1991 Steel wire rod
JIS G 4309 1988 Wire
JIS G 4311 1991 Heat resisting steel bars
JIS G 4312 1991 Heat resisting steel sheets and plates
JIS G 4313 1988 Cold rolled strip for springs
JIS G 4314 1988 Wires for springs
JIS G 4315 1988 Wire for cold heading
JIS G 4316 1991 Welding wire
JIS G 4318 1991 Cold drawn bars
JIS G 4901 1991 Superalloy bars
JIS G 4902 1991 Superalloy sheets
JIS G 4903 1991 Seamless pipes
JIS G 4904 1991 Seamless pipes
JIS G 4801 1984 Spring steels
JIS G 4802 1983 Cold-rolled strips for springs
JIS G 4804 1983 Free cutting steels
JIS G 5101 1991 Steel castings
JIS G 5102 1991 Steel castings
JIS G 5111 1991 Steel casting
JIS G 5131 1991 Steel castings
JIS G 5151 1991 Steel castings
JIS G 5152 1991 Steel casting
JIS G 5201 1991 Centrifugally cast steel pipes
JIS G 5202 1991 Centrifugally cast steel pipes

Group of standards for tool steels

JIS G 3311 1988 Cold rolled special strip
JIS G 4401 1983 Carbon tool steels
JIS G 4403 1983 High speed tool steels
JIS G 4404 1983 Alloy tool steels

Group of standards for stainless and heat resisting steels

JIS G 5121 1991 Stainless steel casting
JIS G 5122 1991 Heat resisting casting


Date Published: Mar-2001




The KEY to METALS database brings global metal properties together into one integrated and searchable database. Quick and easy access to the mechanical properties, chemical composition, cross-reference tables, and more provide users with an unprecedented wealth of information. Click the buttons below to learn more from the Guided Tour or to test drive the KEY to METALS database.