SAE AMS Standard List - Stainless Steels: Part Two

Abstract:

A numeral index system is used to identify the compositions of the SAE steels, which makes it possible to use numerals that are partially descriptive of the composition of material covered by such numbers. In the case of the simple alloy steels, the second digit generally indicates the approximate percentage of the predominant alloying element.

This article contains a list of standards that covers among other things:

  • Bars, wire and spring stainless steels
  • Heat and corrosion resistant welding tubing
  • Specialist seamless tubing for high pressure, hydraulic applications

For more information on the SAE AMS designation system see Introduction to the SAE AMS Standard Designation System.

Stainless Steel’s: Part Two

Standard
Number
Last
version
Description Status
SAE AMS 5584 2006 Steel, Corrosion and Heat Resistant, Seamless and Welded Hydraulic Tubing, 17Cr - 12Ni - 1.5Mo - 0.03C max, Cold Drawn, 1/8 Hard Temper /1/
SAE AMS 5585 2001 Alloy, Corrosion and Heat Resistant, Welded Tubing, 32Fe - 21Cr - 20Ni - 20Co - 3Mo - 2.5W - 1.0Cb - 0.15N, Solution Heat Treated /1/
SAE AMS 5591 2006 Steel, Corrosion and Heat-Resistant, Tubing, Seamless, 12.5Cr (SAE 51410), Annealed /1/
SAE AMS 5595 2008 Steel, Corrosion Resistant, Sheet, Strip, and Plate 9.0Mn - 20Cr - 6.5Ni - 0.28N Solution Heat Treated /1/
SAE AMS 5600 2007 Steel, Corrosion-Resistant, Sheet Laminated, Edge Bonded /1/
SAE AMS 5603   Sheet and strip 15Cr - 8,4Ni - 2,2Mo - 1,1Al, vac. Induct. Melted, solution heat treated Withdrawn 2001 /1/
SAE AMS 5604 2001 Steel, Corrosion Resistant, Sheet, Strip, and Plate, 16.5Cr - 4.0Ni - 4.0Cu - 0.30Cb, Solution Heat Treated, Precipitation Hardenable /1/
SAE AMS 5609 1999 Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Tubing, and Rings, 12Cr - 0.12Cb (SAE 51410 Modified), Ferrite Controlled, Annealed /1/
SAE AMS 5610 2006 Steel, Corrosion and Heat-Resistant, Bars, Wire, and Forgings 12.5Cr - Low Carbon (SAE 51416, 51416Se) Free-Machining /2/
SAE AMS 5611 2006 Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Tubing, and Rings, 12Cr, Ferrite Controlled, Consumable Electrode Melted /1/
SAE AMS 5612 2007 Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Tubing, and Rings 12Cr Ferrite Controlled, Annealed /1/
SAE AMS 5613 2001 Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Tubing, and Rings, 12.5Cr (SAE 51410), Annealed /1/
SAE AMS 5614 2001 Steel, Corrosion and Heat Resistant, Bars, Wire, and Forgings 12Cr - 0.50Mo Annealed /1/
SAE AMS 5616 2008 Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Tubing, and Rings 13Cr - 2.0Ni - 3.0W Annealed /1/
SAE AMS 5617 2006 Steel, Corrosion-Resistant, Bars, Wire, and Forgings 12Cr - 8.5Ni - 1.2Ti - 2.0Cu Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Precipitation Hardenable /2/
SAE AMS 5618 2006 Steel, Corrosion-Resistant, Bars, Wire, and Forgings 17Cr - 0.52Mo (0.95 - 1.20C) (SAE 51440C) Consumable Electrode Vacuum Melted /1/
SAE AMS 5619 1994 Bars and Forgings, 14Cr - 4,0Mo (1,00-1,10C) Withdrawn 2000 /1/
SAE AMS 5620 2006 Steel, Corrosion and Heat-Resistant, Bars, Wire, and Forgings 13Cr (0.30 - 0.40C) (SAE 51420F, 51420FSe) Free-Machining Grade /2/
SAE AMS 5621 2006 Steel, Corrosion Resistant, Bars, Wire, and Forgings 13Cr (0.30-0.40C) (SAE 51420) Annealed /1/
SAE AMS 5622 2008 Steel, Corrosion-Resistant, Bars, Wire, Forgings, Tubing, and Rings, 16Cr - 4.0Ni - 0.30Cb - 4.0Cu, Solution Heat Treated, Precipitation Hardenable, Consumable Electrode Remelted /1/
SAE AMS 5627 2007 Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Tubing, and Rings 17Cr (SAE 51430) Annealed /1/
SAE AMS 5628 2006 Steel, Corrosion-Resistant, Bars, Wire, Forgings, and Tubing 16Cr - 2.5Ni (SAE 51431) /1/
SAE AMS 5629 2006 Steel, Corrosion-Resistant, Bars, Wire, Forgings, Rings, and Extrusions, 13Cr - 8.0Ni - 2.2Mo - 1.1Al, Vacuum Induction Plus Consumable Electrode Melted, Solution Heat Treated, Precipitation Hardenable /1/
SAE AMS 5630 2007 Steel, Corrosion-Resistant, Bars, Wire, and Forgings, 17Cr - 0.52Mo (0.95 - 1.20C) (SAE 51440C) /1/
SAE AMS 5631 2006 Steel, Corrosion-Resistant, Bars and Forgings 17Cr (0.60 - 0.75C) (SAE 51440A) /1/
SAE AMS 5632 2006 Steel, Corrosion-Resistant, Bars, Wire, and Forgings 17Cr - 0.50Mo (0.95 - 1.20C) (SAE 51440F) Free-Machining, Annealed /2/
SAE AMS 5635 2006 Steel, Corrosion-Resistant, Bars, Wire, and Forgings 18Cr - 9Ni - 0.21Pb (303Pb) Free-Machining, Solution Heat Treated /1/
SAE AMS 5636 2006 Steel, Corrosion-Resistant, Bars and Wire, 18Cr - 9.0Ni (SAE 30302), Solution Heat Treated and Cold Drawn, 100 ksi (689 MPa) Tensile Strength /1/
SAE AMS 5637 2001 Steel, Corrosion Resistant, Bars and Wire, 18Cr - 9.0Ni (SAE 30302) Solution Heat Treated and Cold Drawn, 125 ksi (862 Mpa) Tensile Strength /1/
SAE AMS 5638 2005 Steel, Corrosion-Resistant, Bars and Forgings 0.14S - 18Cr - 9.5Ni - 0.50Mo - 0.80Al (303MA) Free-Machining; Swaging or Upsetting Solution Heat Treated /1/
SAE AMS 5639 2002 Steel, Corrosion-Resistant, Bars, Wire, Forgings, Tubing and Rings (19Cr-10Ni) Solution Heat Treated /1/
SAE AMS 5640 2007 Steel, Corrosion-Resistant, Bars, Wire, and Forgings 18Cr - 9.0Ni Free Machining /3/
SAE AMS 5642 2006 Steel, Corrosion and Heat-Resistant, Bars, Wire, and Forgings 18Cr - 10.5Ni - 0.60Cb Free-Machining, Solution Heat Treated /2/
SAE AMS 5643 2008 Steel, Corrosion-Resistant, Bars, Wire, Forgings, Tubing, and Rings 16Cr - 4.0Ni - 0.30Cb - 4.0Cu Solution Heat Treated, Precipitation Hardenable /1/
SAE AMS 5644 1964 Steel Bars and Forgings, Corrosion Heat Resistant 17Cr - 7Ni - 1Al Withdrawn 2001 /1/
SAE AMS 5645 2006 Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Tubing, and Rings 18Cr - 10Ni - 0.40Ti (SAE 30321) Solution Heat Treated /1/
SAE AMS 5646 2002 Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Tubing, and Rings 18Cr - 11 Ni - 0.60Cb (SAE 30347) Solution Heat Treated /1/
SAE AMS 5647 2007 Steel, Corrosion-Resistant, Bars, Wire, Forgings, Tubing, And Rings 19Cr - 9.5Ni Solution Heat Treated /1/
SAE AMS 5648 2007 Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Tubing, and Rings, 17Cr - 12Ni - 2.5Mo, Solution Heat Treated /1/
SAE AMS 5649 2007 Steel, Corrosion and Heat-Resistant, Bars, Wire, and Forgings 18Cr - 13Ni - 2.1Mo Free Machining Solution Heat Treated /1/
SAE AMS 5650 2006 Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Tubing, and Rings 23Cr - 13.5Ni (SAE 30309S) Solution Heat Treated /1/
SAE AMS 5651 2007 Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Tubing, and Rings 25Cr - 20Ni (SAE 30310) Solution Heat Treated /1/
SAE AMS 5652 2006 Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Tubing, and Rings 25Cr - 20Ni - 2.0Si (SAE 30314) Solution Heat Treated /1/
SAE AMS 5653 2007 Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Tubing, and Rings 17Cr - 12Ni - 2.5Mo (0.030 Max C) Solution Heat Treated /1/
SAE AMS 5654 2006 Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Tubing and Rings (18Cr - 11Ni - 0.60(Cb + Ta)) Premium Aircraft Quality, Consumable Electrode Melted Solution Heat Treated /1/
SAE AMS 5655 2006 Steel, Corrosion and Heat Resistant, Bars, Wire, and Forgings, 12.5Cr - 0.75Ni - 1.0Mo - 1.0W - 0.24V (0.20-0.25C), Hardened and Tempered /1/
SAE AMS 5656 2006 Steel, Corrosion Resistant, Bars, Wire, Forgings, Extrusions, and Rings 9.0Mn - 20Cr - 6.5Ni - 0.27N Solution Heat Treated /1/
SAE AMS 5657 1960 Steel Bars and Forgings, Corrosion and Moderate Heat-Resistant 15Cr - 7.1Ni - 2.5Mo - 1.1Al Withdrawn 1982 /1/
SAE AMS 5659 2008 Steel, Corrosion-Resistant, Bars, Wire, Forgings, Rings, and Extrusions 15Cr - 4.5Ni - 0.30CB (Nb) - 3.5Cu Consumable Electrode Melted Solution Heat Treated, Precipitation Hardenable /1/
SAE AMS 5672 2000 Steel Wire, Corrosion Resistant, 11.8Cr - 8.5Ni - 0.30(Cb + Ta) - 1.1Ti - 2.0Cu, Precipitation Hardenable, Spring Temper Withdrawn 2001 /1/
SAE AMS 5674 2001 Steel, Corrosion and Heat Resistant, Wire 18Cr - 11.5Ni - 0.70Cb (SAE 30347) Solution Heat Treated /1/
SAE AMS 5678 2007 Steel, Corrosion Resistant, Wire 17Cr - 7.1Ni - 1.1Al Cold Drawn, Precipitation-Hardenable /1/
SAE AMS 5680 2006 Steel, Corrosion and Heat-Resistant, Welding Wire 18.5Cr - 11Ni - 0.40Cb (Nb) (SAE 30347) /1/
SAE AMS-QQ-S-763 1998 Steel, Corrosion Resistant, Bars, Wire, Shapes, and Forgings Withdrawn 2003 /47/
SAE AMS-S-7720 1997 Steel, Corrosion-Resistant (18-8) Bars, Wire and Forging Stock (Aircraft Quality) /2/
SAE J 217 1994 Stainless Steel 17-7 Ph Spring Wire and Springs /1/
SAE J 230 1994 Stainless Steel, SAE 30302, Spring Wire and Springs /1/
SAE J 405 1998 Chemical Compositions of SAE Wrought Stainless Steels /115/

Search Knowledge Base

Enter a phrase to search for:

Search by

Full text
Keywords

Headings
Abstracts

This article belongs to a series of articles. You can click the links below to read more on this topic.

With Total Materia finding information about a metal standard specification, its current status and the materials it defines is one click away.

Within seconds it is also possible for you to find related detailed material property data or search equivalent materials starting from the Total Materia standard list.

To get started, click on the standard list button in the menu bar.


By simply selecting a Standard Development Organization (SDO) and/or typing the standard number, you receive immediate results from the multi-lingual database containing over 30,000 standards.

For example, you can review all metal standards from SAE by selecting this SDO from the popup.


The result list consists of over 1600 SAE metal standards. Information includes: standard description, year of last issue, current status (valid, replaced, etc.) and a hot link to the materials defined by this standard.


By simply clicking the materials hot link, you can see a list of metal materials defined by the selected standard.


From the list of materials, you can review detailed properties and equivalents of each material.


For you’re a chance to take a test drive of the Total Materia database, we invite you to join a community of over 150,000 registered users through the Total Materia Free Demo.