ASTM Standards for Steel Plates for Pressure Vessels

Abstract:

Standard designation A20-85 covers a group of common requirements which, unless otherwise specified in the individual material specification, shall apply to rolled steel plates for pressure vessels under each of the following specifications issued by ASTM quoted in this article.This specification also covers a group of supplementary requirements, which are applicable to several of the above specifications as indicated therein. These are provided for use when additional testing or inspection is desired and apply only when specified individually by the purchaser in the order.

Standard designation A20-85 covers a group of common requirements which, unless otherwise specified in the individual material specification, shall apply to rolled steel plates for pressure vessels under each of the following specifications issued by ASTM:

Title of Specification ASTM
Designation
Pressure Vessel Plates, Alloy Steel, Chromium-Manganese-Silicon A202
Pressure Vessel Plates, Alloy Steel, Nickel A203
Pressure Vessel Plates, Alloy Steel, Molybdenum A204
Pressure Vessel Plates, Alloy Steel, Manganese-Vanadium A225
Pressure Vessel Plates, Carbon Steel, Low and Intermediate-Tensile Strength A285
Pressure Vessel Plates, Carbon Steel, Manganese-Silicon A299
Pressure Vessel Plates, Alloy Steel, Manganese-Molybdenum and Manganese- Molybdenum-Nickel A302
Pressure Vessel Plates, Alloy Steel, 9 Percent Nickel Double-Normalized and Tempered A353
Pressure Vessel Plates, Alloy Steel, Chromium- Molybdenum A387
Pressure Vessel Plates, Carbon Steel, Improved Transition Properties A442
Pressure Vessel Plates, Carbon Steel, High Strength Manganese A455
Pressure Vessel Plates, Carbon Steel, for Intermediate-and Higher Temperature Service A515
Pressure Vessel Plates, Carbon Steel, Moderate-and Lower- Temperature Service A516
Pressure Vessel Plates, Alloy Steel, High Strength, Quenched and Tempered A517
Pressure Vessel Plates, Alloy Steel, Quenched and Tempered, Manganese-Molybdenum and Manganese- Molybdenum-Nickel A533
Pressure Vessel Plates, Heat-Treated, Carbon Manganese-Silicon Steel A537
Pressure Vessel Plates, Alloy Steel Precipitation Hardening 18 Percent Nickel A538
Pressure Vessel Plates, Alloy Steel, Quenched and Tempered Chromium-Molybdenum A542
Pressure Vessel Plates, Alloy Steel, Quenched and Tempered Nickel-Chromium-Molybdenum A543
Pressure Vessel Plates, Alloy Steel, Quenched and Tempered 8 and 9 Percent Nickel A553
Pressure Vessel Plates, Carbon steel, Manganese-Titanium for Glass or Diffused Metallic Coatings A562
Pressure Vessel Plates, Alloy Steel, Precipitation-Hardening 12 Percent Nickel A590
Pressure Vessel Plates, Alloy Steel, Quenched and Tempered Nickel-Cobalt- Molybdenum- Chromium A605
Pressure Vessel Plates, Carbon Steel, High Strength, for Moderate-and Lower- Temperature Service A612
Pressure Vessel Plates, Five Percent Nickel Alloy steel, Specially Heat Treated A645
Pressure Vessel Plates, Alloy Steel, 36 Percent Nickel A658
Pressure Vessel Plates, Carbon-Manganese, for Moderate and lower Temperature Service A662
Pressure Vessel Plates, Carbon Steel, Quenched and Tempered, for Welded Layered Pressure Vessels A724
Pressure Vessel Plates, Alloy Steel and High-Strength Low-Alloy Steel, Quenched and Tempered A734
Pressure Vessel Plates, Low-Carbon, Manganese-Molybdenum-Columbium Alloy Steel, for Moderate and Lower Temperature Service A735
Pressure Vessel Plates, Low-Carbon Age-Hardening Nickel-Copper-Chromium- Molybdenum-Columbium Alloy Steel A736
Pressure Vessel Plates, High-Strength Low-Alloy Steel A737
Pressure Vessel Plates, Heat-Treated, Carbon-Manganese-Silicon Steel, for Moderate and Lower Temperature Service A738
Pressure Vessel Plates, Quenched and Tempered, Manganese Chromium- Molybdenum-Silicon-Zirconium Alloy Steel A782

This specification also covers a group of supplementary requirements, which are applicable to several of the above specifications as indicated therein. These are provided for use when additional testing or inspection is desired and apply only when specified individually by the purchaser in the order.

Appendix X2 describes the production and some of the characteristics of coiled product from which pressure vessel plates may be produced.

In case of any conflict in requirements, the requirements of the individual material specification shall prevail over those of this general specification.

The purchaser may specify additional requirements which do not negate any the provisions of this general specification or of the individual material specifications. Such additional requirements, the acceptance of which is subject to negotiation with the supplier, must be included in the order information.

In general, all these materials are intended to be suitable for fusion welding.

Manufacture

Unless otherwise specified in the material specification, the steel may be made by any of the following processes: open-hearth, basic-oxygen, electric-furnace, vacuum arc remelt (VAR) or electroslag remelt (ESR).

The steel may be cast in ingots or may be strand cast. If more than one heat is consecutively strand cast at one time, the heats must be melted to the same steelmaking composition range. When such continuous strand casting is employed, the heat number assigned to the cast product (slab) may remain unchanged until all of the steel in the slab is from the following heat.

The ratio of reduction of thickness from a strand-cast slab to plate shall be a minimum of 3 to 1. Plates are produced in either discrete cut lengths of flat product or from coils. Plates produced from coil means plates that have been leveled or flattened and cut to length from a coiled product and that are furnished without heat treatment. Plates that are annealed, normalized, normalized-and-tempered, or quenched-and-tempered after decoiling shall be considered to discrete cut lengths of flat products.

Heat Treatment

When material is required to be heat treated, the heat treatment may be performed either by the manufacturer or processor or by the fabricator unless otherwise specified in the material specification.

When the heat treatment required by the material specification is to be performed by the purchaser or his agent, and the material is to be supplied by the material producer in a condition other than that required by the material specification, the order shall so state.

When plates are ordered without the heat treatment required by the material specification, heat treatment of the plates to conform to the requirements of the material specification shall be responsibility of the purchaser.

When heat treatment is to be performed, the material shall be heat treated as specified in the material specification. The purchaser may specify the heat treatment to be used provided it is not in conflict with the requirements of the material specification.

When normalizing is to be performed by the fabricator, it may be accomplished by heating uniformly for hot forming. The temperature to which the plates are heated for hot forming shall not significantly exceed the normalizing temperature.

When no heat treatment is required, the manufacturer or processor at his option may heat treat the plates by normalizing and then stress relieving to meet the material specification.

If approved by the purchaser, cooling rates faster than those obtained by cooling in air are permissible for improvement of the toughness, provided the plates are subsequently tempered in the temperature range from 595 to 705oC.

Search Knowledge Base

Enter a phrase to search for:

Search by

Full text
Keywords

Headings
Abstracts

With Total Materia finding information about a metal standard specification, its current status and the materials it defines is one click away.

Within seconds it is also possible for you to find related detailed material property data or search equivalent materials starting from the Total Materia standard list.

To get started, click on the standard list button in the menu bar.


By simply selecting a Standard Development Organization (SDO) and/or typing the standard number, you receive immediate results from the multi-lingual database containing over 30,000 standards.

For example, you can review all metal standards from ASTM by selecting this SDO from the popup.


The result list consists of over 3000 ASTM metal standards. Information includes: standard description, year of last issue, current status (valid, replaced, etc.) and a hot link to the materials defined by this standard.


By simply clicking the materials hot link, you can see a list of metal materials defined by the selected standard.


From the list of materials, you can review detailed properties and equivalents of each material.


For you’re a chance to take a test drive of the Total Materia database, we invite you to join a community of over 150,000 registered users through the Total Materia Free Demo.