Material designation: 6061
Numerical designation: 6061
Standard:  SAE
Country:  USA

Subgroup

#SubgroupDetails
1 SAE AMS T 7081A (1999)
Tube, aluminum alloy, seamless, round, drawn, 6061, aircraft hydraulic quality

Standard Replaced
2 SAE AMS 4113E (2008)
Aluminum Alloy, Extruded Profiles 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061-T6) Solution and Precipitation Heat Treated
3 SAE AMS 4127J (2005)
Aluminum Alloy, Forgings and Rolled or Forged Rings (6061-T6) Solution and Precipitation Heat Treated
4 SAE AMS 4150M (2013)
Aluminum Alloy, Extrusions and Rings 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr - (6061-T6) Solution and Precipitation Heat Treated
5 SAE AMS A 22771C (2012)
Aluminum Alloy Forgings, Heat Treated
6 SAE AMS 4080N (2009)
Aluminum Alloy, Drawn Seamless Tubing 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061-O) Annealed
7 SAE AMS 4115H (2009)
Aluminum Alloy, Rolled or Cold-Finished, Bars, Rods, Wire, and Flash Welded Rings Annealed 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061-O)
8 SAE AMS 4160H (2013)
Aluminum Alloy, Extrusions 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061-O) Annealed
9 SAE AMS 4079G (2009)
Aluminum Alloy, Drawn, Round, Seamless, Tubing 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061-O) Close Tolerance, Annealed
10 SAE AMS 4026M (2005)
Aluminum Alloy, Sheet and Plate 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061; -T4 Sheet, -T451 Plate) Solution Heat Treated and Naturally Aged
11 SAE AMS 4116H (2009)
Aluminum Alloy, Bars, Rods, and Wire 1.0Mg - 0.60Si - 0.30Cu - 0.20Cr (6061-T4) Cold Finished, Solution Heat Treated
12 SAE AMS 4161H (2013)
Aluminum Alloy, Extrusions 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061-T4) Solution Heat Treated and Naturally Aged
13 SAE AMS 4172F (2013)
Aluminum Alloy, Extrusions 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061-T4511) Solution Heat Treated and Stress Relieved by Stretching
14 SAE AMS QQ A 200 16 (1997)
Aluminum Alloy, Structural Shapes, Extruded, 6061

Standard Replaced
15 SAE AMS 4027N (2008)
Aluminum Alloy, Sheet and Plate 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061; -T6 Sheet, -T651 Plate) Solution and Precipitation Heat Treated
16 SAE AMS 4173F (2013)
Aluminum Alloy, Extrusions 1.0Mg - 0.60Si - 0.30Cu - 0.20Cr (6061-T6511) Solution Heat Treated, Stress Relieved by Stretching, Straightened, and Precipitation Heat Treated
17 SAE AMS 4248C (2012)
Aluminum Alloy Hand Forgings and Rolled Rings 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061-T652) Solution Heat Treated, Stress Relief Compressed, and Precipitation Heat Treated
18 SAE AMS 4312D (2008)
Aluminum Alloy, Rolled or Forged Rings 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061-T651, 6061-T652) Solution Heat Treated, Mechanically Stress Relieved, and Precipitation Heat Treated
19 SAE AMS QQ A 200 8 (1997)
Aluminum Alloy 6061, Bar, Rod, Shapes, Tube, and Wire, Extruded
20 SAE AMS QQ A 225 8A (2007)
Aluminum Alloy 6061, Bar, Rod, Wire, and Special Shapes; Rolled, Drawn, or Cold Finished

Standard Withdrawn
21 SAE AMS QQ A 250 11A (1997)
Aluminum alloy 6061 - plate and sheet

Standard Withdrawn
22 SAE AMS QQ A 367D (2012)
Aluminum alloy forgings
23 SAE AMS WW T 700/6B (2011)
Tube, Aluminum Alloy, Drawn, Seamless, 6061
24 SAE AMS 4025L (2008)
Aluminum Alloy, Sheet and Plate 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061-O) Annealed
25 SAE AMS 4083L (2012)
Aluminum Alloy Tubing, Hydraulic, Seamless, Drawn, Round 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061-T6) Solution and Precipitation Heat Treated
26 SAE AMS 4082P (2008)
Aluminum Alloy, Seamless Drawn Tubing 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061-T6) Solution and Precipitation Heat Treated
27 SAE AMS 4081J (2008)
Aluminum Alloy Tubing, Hydraulic, Seamless, Drawn, Round 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061-T4) Solution Heat Treated and Naturally Aged
28 SAE AMS 4117J (2009)
Aluminum Alloy, Rolled or Cold Finished Bars, Rods, and Wire and Flash Welded Rings 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061; -T6, -T651) Solution and Precipitation Heat Treated
29 SAE AMS 4128D (2007)
Aluminum Alloy Bars, Rolled or Cold Finished 1.0Mg - 0.60Si - 0.30Cu - 0.20Cr (6061-T451) Solution Heat Treated and Stress Relieved by Stretching
30 SAE AMS 4146G (2008)
Aluminum Alloy Forgings and Rolled or Forged Rings 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061 - T4) Solution Heat Treated and Naturally Aged
31 SAE J 454 (1991)
Wrought aluminum alloys
32 SAE AMS 4009B (1995)
Aluminum Alloy Foil 1.0Mg - 0.6Si - 0.30Cu - 0.20Cr (6061-O) Annealed

Standard Withdrawn
33 SAE AMS 4294 (2010)
Aluminum Alloy Extrusions 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061-T5511) Press Heat Treated, Stress Relieved by Stretching, Straightened, and Artificially Aged
34 SAE AMS 4300C (2006)
Boron-Aluminum Composite Sheet 50 v/o 5.6B, 6061-O, For Diffusion Bonding