Material designation: 3.1354
Standard:  WL
Country:  Germany

Subgroup

#SubgroupDetails
1 WL 3.1354-1 (1987)
Aerospace; wrought aluminium alloy with approx. 4, 4Cu-1, 5Mg-0, 6Mn; sheet and plate
2 WL 3.1354-2 (1987)
Aerospace; wrought aluminium alloy with approx. 4, 4Cu-1, 5Mg-0, 6Mn; bars
3 WL 3.1354-3 (1987)
Aerospace; wrought aluminium alloy with approx. 4, 4Cu-1, 5Mg-0, 6Mn; extruded sections
4 WL 3.1354-4 (1990)
Aerospace; wrought aluminium alloy with approx. 4, 4Cu-1, 5Mg-0, 6Mn; structural tubes
* No original data are present. Estimates are available.