Material designation: X 21 CrMoV 12 1
Numerical designation: 1.4926
Standard:  SEW
Country:  Germany

Subgroup

#SubgroupDetails
1 SEW 555
Steels for larger forgings for components in turbine and generator installations
Cross-Reference Table (1)
Composition (9)
Mechanical Properties (6)
Physical Properties *
Elevated Temperatures
Machinability
Heat Treatment
Metallography
Carbon Equivalent
Direct Suppliers (1)
Alternative Suppliers
Stress-Strain diagrams
Flow Stress Flow Strain
Fatigue Data
Fracture Mechanics
Creep Data
* No original data are present. Estimates are available.