This group of ASTM specifications covers standard properties of steel
and iron castings and forgings for valves, flanges, fittings, and other
pressure containing parts for high-temperature and low-temperature service.
Additionally, in the table below standards for evaluating the microstructure
of graphite in iron castings and methods for mechanical testing of cast
irons are presented.
|
A27
|
A27/A27M-95
|
Specification for Steel Castings, Carbon, for General Application
|
|
A47
|
A47/A47M-99
|
Specification for Ferritic Malleable Iron Castings
|
|
A48M
|
A48M-94e1
|
Specification for Gray Iron Castings [Metric]
|
|
A48
|
A48-94ae1
|
Specification for Gray Iron Castings
|
|
A74
|
A74-98
|
Specification for Cast Iron Soil Pipe and Fittings
|
|
A126
|
A126-95e1
|
Specification for Gray Iron Castings for Valves, Flanges, and Pipe Fittings
|
|
A128
|
A128/A128M-93 (1998)
|
Specification for Steel Castings, Austenitic Manganese
|
|
A148
|
A148/A148M-93b (1998)
|
Specification for Steel Castings, High Strength, for Structural Purposes
|
|
A159
|
A159-83 (1993)
|
Specification for Automotive Gray Iron Castings
|
|
A216
|
A216/A216M-93 (1998)
|
Specification for Steel Castings, Carbon, Suitable for Fusion Welding, for High- Temperature Service
|
|
A217
|
A217/A217M-99
|
Specification for Steel Castings, Martensitic Stainless and Alloy, for Pressure- Containing Parts, Suitable for High-Temperature Service
|
|
A247
|
A247-67 (1998)
|
Test Method for Evaluating the Microstructure of Graphite in Iron Castings
|
|
A278M
|
A278M-93e1
|
Specification for Gray Iron Castings for Pressure-Containing Parts for Temperatures Up to 350°C
|
|
A278
|
A278-93
|
Specification for Gray Iron Castings for Pressure-Containing Parts for Temperatures Up to 650°F
|
|
A297
|
A297/A297M-97 (1998)
|
Specification for Steel Castings, Iron-Chromium and Iron-Chromium-Nickel, Heat Resistant, for General Application
|
|
A319
|
A319-71 (1995)
|
Specification for Gray Iron Castings for Elevated Temperatures for Non-Pressure Containing Parts
|
|
A327M
|
A327M-91 (1997)
|
Test Methods for Impact Testing of Cast Irons (Metric)
|
|
A327
|
A327-91 (1997)
|
Test Methods for Impact Testing of Cast Irons
|
|
A351
|
A351/A351M-94a (1999)
|
Specification for Castings, Austenitic, Austenitic-Ferritic (Duplex), for Pressure-Containing Parts
|
|
A352
|
A352/A352M-93 (1998)
|
Specification for Steel Castings, Ferritic and Martensitic, for Pressure-Containing Parts, Suitable for Low-Temperature Service
|
|
A356
|
A356/A356M-98e1
|
Specification for Steel Castings, Carbon, Low Alloy, and Stainless Steel, Heavy-Walled for Steam Turbines
|
|
A367
|
A367-60 (1999)
|
Test Methods of Chill Testing of Cast Iron
|
|
A389
|
A389/A389M-93 (1998)
|
Specification for Steel Castings, Alloy, Specially Heat-Treated, for Pressure-Containing Parts, Suitable for High-Temperature Service
|
|
A395
|
A395/A395M-99
|
Specification for Ferritic Ductile Iron Pressure-Retaining Castings for Use at Elevated Temperatures
|
|
A426
|
A426-92 (1997)
|
Specification for Centrifugally Cast Ferritic Alloy Steel Pipe for High-Temperature Service
|
|
A436
|
A436-84 (1997) e1
|
Specification for Austenitic Gray Iron Castings
|
|
A438
|
A438-80 (1997)
|
Test Method for Transverse Testing of Gray Cast Iron
|
|
A439
|
A439-83 (1999)
|
Specification for Austenitic Ductile Iron Castings
|
|
A447
|
A447/A447M-93 (1998)
|
Specification for Steel Castings, Chromium-Nickel-Iron Alloy (25-12 Class), for High-Temperature Service
|
|
A451
|
A451-93 (1997)
|
Specification for Centrifugally Cast Austenitic Steel Pipe for High-Temperature Service
|
|
A476M
|
A476M-84 (1993)
|
Specification for Ductile Iron Castings for Paper Mill Dryer Rolls [Metric]
|
|
A476
|
A476-90 (1997)
|
Specification for Ductile Iron Castings for Paper Mill Dryer Rolls
|
|
A487
|
A487/A487M-93 (1998)
|
Specification for Steel Castings Suitable for Pressure Service
|
|
A488
|
A488/A488M-99
|
Practice for Steel Castings, Welding, Qualifications of Procedures and Personnel
|
|
A494
|
A494/A494M-00
|
Specification for Castings, Nickel and Nickel Alloy
|
|
A518
|
A518/A518M-99
|
Specification for Corrosion-Resistant High-Silicon Iron Castings
|
|
A532
|
A532/A532M-93a (1999) e1
|
Specification for Abrasion-Resistant Cast Irons
|
|
A536
|
A536-84 (1999) e1
|
Specification for Ductile Iron Castings
|
|
A560
|
A560/A560M-93 (1998)
|
Specification for Castings, Chromium-Nickel Alloy
|
|
A571M
|
A571M-84 (1997)
|
Specification for Austenitic Ductile Iron Castings for Pressure-Containing Parts Suitable for Low-Temperature Service [Metric]
|
|
A571
|
A571-84 (1997)
|
Specification for Austenitic Ductile Iron Castings for Pressure-Containing Parts Suitable for Low-Temperature Service
|
|
A583
|
A583-93 (1999)
|
Specification for Cast Steel Wheels for Railway Service
|
|
A597
|
A597-87 (1999)
|
Specification for Cast Tool Steel
|
|
A602
|
A602-94 (1998)
|
Specification for Automotive Malleable Iron Castings
|
|
A608
|
A608-91a (1998)
|
Specification for Centrifugally Cast Iron-Chromium-Nickel High-Alloy Tubing for Pressure Application at High Temperatures
|
|
A609
|
A609/A609M-91 (1997)
|
Practice for Castings, Carbon, Low-Alloy, and Martensitic Stainless Steel, Ultrasonic Examination Thereof
|
|
A644
|
A644-98
|
Terminology Relating to Iron Castings
|
|
A667
|
A667/A667M-87 (1998)
|
Specification for Centrifugally Cast Dual Metal (Gray and White Cast Iron) Cylinders
|
|
A703
|
A703/A703M-99
|
Specification for Steel Castings, General Requirements, for Pressure-Containing Parts
|
|
A732
|
A732/A732M-98
|
Specification for Castings, Investment, Carbon and Low Alloy Steel for General Application, and Cobalt Alloy for High Strength at Elevated Temperatures
|
|
A743
|
A743/A743M-98ae1
|
Specification for Castings, Iron-Chromium, Iron-Chromium-Nickel, Corrosion Resistant, for General Application
|
|
A744
|
A744/A744M-98a
|
Specification for Castings, Iron-Chromium-Nickel, Corrosion Resistant, for Severe Service
|
|
A747
|
A747/A747M-99
|
Specification for Steel Castings, Stainless, Precipitation Hardening
|
|
A748
|
A748/A748M-87 (1998)
|
Specification for Statically Cast Chilled White Iron-Gray Iron Dual Metal Rolls for Pressure Vessel Use
|
|
A757
|
A757/A757M-00
|
Specification for Steel Castings, Ferritic and Martensitic, for Pressure-Containing and Other Applications, for Low-Temperature Service
|
|
A781
|
A781/A781M-99a
|
Specification for Castings, Steel and Alloy, Common Requirements, for General Industrial Use
|
|
A799
|
A799/A799M-92 (1997)
|
Practice for Steel Castings, Stainless, Instrument Calibration, for Estimating Ferrite Content
|
|
A800
|
A800/A800M-91 (1997) e1
|
Practice for Steel Casting, Austenitic Alloy, Estimating Ferrite Content Thereof
|
|
A802
|
A802/A802M-95 (1996)
|
Practice for Steel Castings, Surface Acceptance Standards, Visual Examination
|
|
A823
|
A823-99
|
Specification for Statically Cast Permanent Mold Gray Iron Castings
|
|
A834
|
A834-95
|
Specification for Common Requirements for Iron Castings for General Industrial Use
|
|
A842
|
A842-85 (1997)
|
Specification for Compacted Graphite Iron Castings
|
|
A872
|
A872-91 (1997)
|
Specification for Centrifugally Cast Ferritic/Austenitic Stainless Steel Pipe for Corrosive Environments
|
|
A874
|
A874/A874M-98
|
Specification for Ferritic Ductile Iron Castings Suitable for Low-Temperature Service
|
|
A888
|
A888-98e1
|
Specification for Hubless Cast Iron Soil Pipe and Fittings for Sanitary and Storm Drain, Waste, and Vent Piping Applications
|
|
A890
|
A890/A890M-99
|
Specification for Castings, Iron-Chromium-Nickel-Molybdenum Corrosion-Resistant, Duplex (Austenitic/Ferritic) for General Application
|
|
A897M
|
A897M-90 (1997)
|
Specification for Austempered Ductile Iron Castings [Metric]
|
|
A897
|
A897-90 (1997)
|
Specification for Austempered Ductile Iron Castings
|
|
A903
|
A903/A903M-99
|
Specification for Steel Castings, Surface Acceptance Standards, Magnetic Particle and Liquid Penetrant Inspection
|
|
A915
|
A915/A915M-93 (1998)
|
Specification for Steel Castings, Carbon, and Alloy, Chemical Requirements Similar to Standard Wrought Grades
|
|
A942
|
A942-95
|
Specification for Centrifugally Cast White Iron/Gray Iron Dual Metal Abrasion- Resistant Roll Shells
|
|
A957
|
A957-96
|
Specification for Investment Castings, Steel and Alloy, Common Requirements, for General Industrial Use
|
|
A958
|
A958-96e1
|
Specification for Steel Castings, Carbon, and Alloy, with Tensile Requirements, Chemical Requirements Similar to Standard Wrought Grades
|
|
A985
|
A985-98a
|
Specification for Steel Investment Casting General Requirements, for Pressure-Containing Parts
|
|
A993
|
A993-98
|
Test Method for Dynamic Tear Testing of Cast Irons to Establish Transition Temperature
|
|
A1002
|
A1002-99
|
Specification for Castings, Nickel-Aluminum Ordered Alloy
|
|
A105
|
A105/A105M-98
|
Specification for Carbon Steel Forgings for Piping Applications
|
|
A181
|
A181/A181M-95b
|
Specification for Carbon Steel Forgings, for General-Purpose Piping
|
|
A182
|
A182/A182M-99
|
Specification for Forged or Rolled Alloy-Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service
|
|
A266
|
A266/A266M-99
|
Specification for Carbon Steel Forgings for Pressure Vessel Components
|
|
A275
|
A275/A275M-98
|
Test Method for Magnetic Particle Examination of Steel Forgings
|
|
A288
|
A288-91 (1998)
|
Specification for Carbon and Alloy Steel Forgings for Magnetic Retaining Rings for Turbine Generators
|
|
A289
|
A289/A289M-97
|
Specification for Alloy Steel Forgings for Nonmagnetic Retaining Rings for Generators
|
|
A290
|
A290-95 (1999)
|
Specification for Carbon and Alloy Steel Forgings for Rings for Reduction Gears
|
|
A291
|
A291-95 (1999)
|
Specification for Steel Forgings, Carbon and Alloy, for Pinions, Gears and Shafts for Reduction Gears
|
|
A314
|
A314-97
|
Specification for Stainless Steel Billets and Bars for Forging
|
|
A336
|
A336/A336M-99
|
Specification for Alloy Steel Forgings for Pressure and High-Temperature Parts
|
|
A350
|
A350/A350M-99
|
Specification for Carbon and Low-Alloy Steel Forgings, Requiring Notch Toughness Testing for Piping Components
|
|
A369
|
A369/A369M-92
|
Specification for Carbon and Ferritic Alloy Steel Forged and Bored Pipe for High-Temperature Service
|
|
A372
|
A372/A372M-99
|
Specification for Carbon and Alloy Steel Forgings for Thin-Walled Pressure Vessels
|
|
A388
|
A388/A388M-95
|
Practice for Ultrasonic Examination of Heavy Steel Forgings
|
|
A418
|
A418-99
|
Test Method for Ultrasonic Examination of Turbine and Generator Steel Rotor Forgings
|
|
A456
|
A456/A456M-99
|
Specification for Magnetic Particle Examination of Large Crankshaft Forgings
|
|
A469
|
A469-94a (1999)
|
Specification for Vacuum-Treated Steel Forgings for Generator Rotors
|
|
A471
|
A471-94 (1999)
|
Specification for Vacuum-Treated Alloy Steel Forgings for Turbine Rotor Disks and Wheels
|
|
A472
|
A472-98
|
Test Method for Heat Stability of Steam Turbine Shafts and Rotor Forgings
|
|
A473
|
A473-99
|
Specification for Stainless Steel Forgings
|
|
A484
|
A484/A484M-98
|
Specification for General Requirements for Stainless Steel Bars, Billets, and Forgings
|
|
A493
|
A493-95
|
Specification for Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging
|
|
A503
|
A503/A503M-99
|
Specification for Ultrasonic Examination of Large Forged Crankshafts
|
|
A508
|
A508/A508M-95 (1999)
|
Specification for Quenched and Tempered Vacuum-Treated Carbon and Alloy Steel Forgings for Pressure Vessels
|
|
A522
|
A522/A522M-95b
|
Specification for Forged or Rolled 8 and 9% Nickel Alloy Steel Flanges, Fittings, Valves, and Parts for Low-Temperature Service
|
|
A541
|
A541/A541M-95 (1999)
|
Specification for Quenched and Tempered Carbon and Alloy Steel Forgings for Pressure Vessel Components
|
|
A565
|
A565-97
|
Specification for Martensitic Stainless Steel Bars, Forgings, and Forging Stock for High-Temperature Service
|
|
A579
|
A579-99
|
Specification for Superstrength Alloy Steel Forgings
|
|
A592
|
A592/A592M-89 (1999)
|
Specification for High-Strength Quenched and Tempered Low-Alloy Steel Forged Fittings and Parts for Pressure Vessels
|
|
A638
|
A638/A638M-00
|
Specification for Precipitation Hardening Iron Base Superalloy Bars, Forgings, and Forging Stock for High-Temperature Service
|
|
A646
|
A646-95 (1999)
|
Specification for Premium Quality Alloy Steel Blooms and Billets for Aircraft and Aerospace Forgings
|
|
A649
|
A649/A649M-99
|
Specification for Forged Steel Rolls Used for Corrugating Paper Machinery
|
|
A668
|
A668/A668M-96e1
|
Specification for Steel Forgings, Carbon and Alloy, for General Industrial Use
|
|
A694
|
A694/A694M-00
|
Specification for Carbon and Alloy Steel Forgings for Pipe Flanges, Fittings, Valves, and Parts for High-Pressure Transmission Service
|
|
A705
|
A705/A705M-95
|
Specification for Age-Hardening Stainless Steel Forgings
|
|
A707
|
A707/A707M-00
|
Specification for Forged Carbon and Alloy Steel Flanges for Low-Temperature Service
|
|
A711
|
A711-92 (1996) e1
|
Specification for Steel Forging Stock
|
|
A723
|
A723/A723M-94 (1999)
|
Specification for Alloy Steel Forgings for High-Strength Pressure Component Application
|
|
A727
|
A727/A727M-97
|
Specification for Carbon Steel Forgings for Piping Components with Inherent Notch Toughness
|
|
A730
|
A730-93 (1999)
|
Specification for Forgings, Carbon and Alloy Steel, for Railway Use
|
|
A745
|
A745/A745M-94 (1999)
|
Practice for Ultrasonic Examination of Austenitic Steel Forgings
|
|
A765
|
A765/A765M-98a
|
Specification for Carbon Steel and Low-Alloy Steel Pressure-Vessel-Component Forgings with Mandatory Toughness Requirements
|
|
A768
|
A768-95
|
Specification for Vacuum-Treated 12% Chromium Alloy Steel Forgings for Turbine Rotors and Shafts
|
|
A788
|
A788-98a
|
Specification for Steel Forgings, General Requirements
|
|
A831
|
A831/A831M-95
|
Specification for Austenitic and Martensitic Stainless Steel Bars, Billets, and Forgings for Liquid Metal Cooled Reactor Core Components
|
|
A836
|
A836/A836M-95b
|
Specification for Titanium-Stabilized Carbon Steel Forgings for Glass-Lined Piping and Pressure Vessel Service
|
|
A837
|
A837-91 (1996) e1
|
Specification for Steel Forgings, Alloy, for Carburizing Applications
|
|
A859
|
A859/A859M-95 (1999)
|
Specification for Age-Hardening Alloy Steel Forgings for Pressure Vessel Components
|
|
A891
|
A891-98
|
Specification for Precipitation Hardening Iron Base Superalloy Forgings for Turbine Rotor Disks and Wheels
|
|
A909
|
A909-94 (1999)
|
Specification for Steel Forgings, Microalloy, for General Industrial Use
|
|
A921
|
A921/A921M-93 (1999)
|
Specification for Steel Bars, Microalloy, Hot-Wrought, Special Quality, for Subsequent Hot Forging
|
|
A952
|
A952/A952M-98
|
Specification for Forged Grade 80 and Grade 100 Steel Lifting Components and Welded Attachment Links
|
|
A961
|
A961-99
|
Specification for Common Requirements for Steel Flanges, Forged Fittings, Valves, and Parts for Piping Applications
|
|
A965
|
A965/A965M-99
|
Specification for Steel Forgings, Austenitic, for Pressure and High Temperature Parts
|
|
A966
|
A966/A966M-96
|