Group of ASTM standards for steel plate, sheet, strip and wire |
|
|
|
|
This group of ASTM standards covers the requirements to be met by:
- Steel plate, sheet, and strip used in various applications
- The properties of assorted types of steel wire, e.g., stainless and heat resisting steel wire, drawn galvanized wire for mechanical springs, and alloy steel coarse round wire
- Industrial sizing screens.
STEEL PLATE, SHEET AND STRIP
|
A109
|
A109/A109M-98a
|
Specification for Steel, Strip, Carbon (0.25 Maximum Percent), Cold-Rolled
|
|
A167
|
A167-99
|
Specification for Stainless and Heat-Resisting Chromium-Nickel Steel Plate, Sheet, and Strip
|
|
A176
|
A176-99
|
Specification for Stainless and Heat-Resisting Chromium Steel Plate, Sheet, and Strip
|
|
A240
|
A240/A240M-00
|
Specification for Heat-Resisting Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels
|
|
A262
|
A262-98
|
Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels
|
|
A263
|
A263-94a (1999)
|
Specification for Corrosion-Resisting Chromium Steel-Clad Plate, Sheet, and Strip
|
|
A264
|
A264-94a (1999)
|
Specification for Stainless Chromium-Nickel Steel-Clad Plate, Sheet, and Strip
|
|
A265
|
A265-94a (1999)
|
Specification for Nickel and Nickel-Base Alloy-Clad Steel Plate
|
|
A345
|
A345-98
|
Specification for Flat-Rolled Electrical Steels for Magnetic Applications
|
|
A366
|
A366/A366M-97e1
|
Specification for Commercial Steel (CS) Sheet, Carbon (0.15 Maximum Percent) Cold-Rolled
|
|
A370
|
A370-97a
|
Test Methods and Definitions for Mechanical Testing of Steel Products
|
|
A380
|
A380-99e1
|
Practice for Cleaning, Descaling, and Passivation of Stainless Steel Parts, Equipment, and Systems
|
|
A414
|
A414/A414M-00
|
Specification for Steel, Sheet, Carbon, for Pressure Vessels
|
|
A417
|
A417-93 (1998)
|
Specification for Steel Wire, Cold-Drawn, for Zig-Zag, Square-Formed, and Sinuous-Type Upholstery Spring Units
|
|
A424
|
A424-00
|
Specification for Steel, Sheet, for Porcelain Enameling
|
|
A480
|
A480/A480M-99b
|
Specification for General Requirements for Flat-Rolled Stainless and Heat-Resisting Steel Plate, Sheet, and Strip
|
|
A505
|
A505-00
|
Specification for Steel, Sheet and Strip, Alloy, Hot-Rolled and Cold-Rolled, General Requirements for
|
|
A506
|
A506-93 (1998)
|
Specification for Steel, Sheet and Strip, Alloy, Hot-Rolled and Cold-Rolled, Regular Quality and Structural Quality
|
|
A507
|
A507-93 (1998)
|
Specification for Steel, Sheet and Strip, Alloy, Hot-Rolled and Cold-Rolled, Drawing Quality
|
|
A568
|
A568/A568M-00
|
Specification for Steel, Sheet, Carbon, and High-Strength, Low-Alloy, Hot-Rolled and Cold-Rolled, General Requirements for
|
|
A569
|
A569/A569M-98
|
Specification for Steel, Carbon (0.15 Maximum, Percent), Hot-Rolled Sheet and Strip Commercial Quality
|
|
A570
|
A570/A570M-98
|
Specification for Steel, Sheet and Strip, Carbon, Hot-Rolled, Structural Quality
|
|
A604
|
A604-93 (1998)
|
Test Method for Macroetch Testing of Consumable Electrode Remelted Steel Bars and Billets
|
|
A606
|
A606-98
|
Specification for Steel, Sheet and Strip, High-Strength, Low-Alloy, Hot-Rolled and Cold-Rolled, with Improved Atmospheric Corrosion Resistance
|
|
A607
|
A607-98
|
Specification for Steel, Sheet and Strip, High-Strength, Low-Alloy, Columbium or Vanadium, or Both, Hot-Rolled and Cold-Rolled
|
|
A611
|
A611-97
|
Specification for Structural Steel (SS), Sheet, Carbon, Cold-Rolled
|
|
A620
|
A620/A620M-97
|
Specification for Drawing Steel (DS), Sheet, Carbon, Cold-Rolled
|
|
A622
|
A622/A622M-97
|
Specification for Drawing Steel (DS), Sheet and Strip, Carbon, Hot-Rolled
|
|
A635
|
A635/A635M-98
|
Specification for Steel, Sheet and Strip, Heavy-Thickness Coils, Carbon, Hot-Rolled
|
|
A659
|
A659/A659M-97
|
Specification for Commercial Steel (CS), Sheet and Strip, Carbon (0.16 Maximum to 0.25 Maximum Percent), Hot-Rolled
|
|
A666
|
A666-00
|
Specification for Annealed or Cold-Worked Austenitic Stainless Steel Sheet, Strip, Plate, and Flat Bar
|
|
A682
|
A682/A682M-98a
|
Specification for Steel, Strip, High-Carbon, Cold-Rolled, General Requirements For
|
|
A684
|
A684/A684M-86 (1998)
|
Specification for Steel, Strip, High-Carbon, Cold-Rolled
|
|
A693
|
A693-93 (1999)
|
Specification for Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip
|
|
A700
|
A700-99
|
Practices for Packaging, Marking, and Loading Methods for Steel Products for Domestic Shipment
|
|
A702
|
A702-89 (1994) e1
|
Specification for Steel Fence Posts and Assemblies, Hot Wrought
|
|
A715
|
A715-98
|
Specification for Steel Sheet and Strip, High-Strength, Low-Alloy, Hot-Rolled, and Steel Sheet, Cold-Rolled, High-Strength, Low-Alloy, with Improved Formability
|
|
A749
|
A749/A749M-97
|
Specification for Steel, Strip, Carbon and High-Strength, Low-Alloy, Hot-Rolled, General Requirements for
|
|
A751
|
A751-96
|
Test Methods, Practices, and Terminology for Chemical Analysis of Steel Products
|
|
A763
|
A763-93 (1999) e1
|
Practices for Detecting Susceptibility to Intergranular Attack in Ferritic Stainless Steels
|
|
A793
|
A793-96
|
Specification for Rolled Floor Plate, Stainless Steel
|
|
A794
|
A794-97
|
Specification for Commercial Steel (CS), Sheet, Carbon (0.16% Maximum to 0.25% Maximum), Cold-Rolled
|
|
A829
|
A829/A829M-95
|
Specification for Alloy Structural Steel Plates
|
STEEL WIRE
|
A227
|
A227/A227M-99
|
Specification for Steel Wire, Cold-Drawn for Mechanical Springs
|
|
A228
|
A228/A228M-93
|
Specification for Steel Wire, Music Spring Quality
|
|
A229
|
A229/A229M-99
|
Specification for Steel Wire, Oil-Tempered for Mechanical Springs
|
|
A230
|
A230/A230M-99
|
Specification for Steel Wire, Oil-Tempered Carbon Valve Spring Quality
|
|
A231
|
A231/A231M-96
|
Specification for Chromium-Vanadium Alloy Steel Spring Wire
|
|
A232
|
A232/A232M-99
|
Specification for Chromium-Vanadium Alloy Steel Valve Spring Quality Wire
|
|
A313
|
A313/A313M-98
|
Specification for Stainless Steel Spring Wire
|
|
A368
|
A368-95a
|
Specification for Stainless Steel Wire Strand
|
|
A401
|
A401/A401M-98
|
Specification for Steel Wire, Chromium-Silicon Alloy
|
|
A407
|
A407-93 (1998)
|
Specification for Steel Wire, Cold-Drawn, for Coiled-Type Springs
|
|
A478
|
A478-97
|
Specification for Chromium-Nickel Stainless Steel Weaving and Knitting Wire
|
|
A492
|
A492-95
|
Specification for Stainless Steel Rope Wire
|
|
A493
|
A493-95
|
Specification for Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging
|
|
A510M
|
A510M-00
|
Specification for General Requirements for Wire Rods and Coarse Round Wire, Carbon Steel [Metric]
|
|
A510
|
A510-00
|
Specification for General Requirements for Wire Rods and Coarse Round Wire, Carbon Steel
|
|
A555
|
A555/A555M-97
|
Specification for General Requirements for Stainless Steel Wire and Wire Rods
|
|
A580
|
A580/A580M-98
|
Specification for Stainless Steel Wire
|
|
A581
|
A581/A581M-95b
|
Specification for Free-Machining Stainless Steel Wire and Wire Rods
|
|
A679
|
A679/A679M-00
|
Specification for Steel Wire, High Tensile Strength, Cold Drawn
|
|
A713
|
A713-93 (1998)
|
Specification for Steel Wire, High-Carbon Spring, for Heat-Treated Components
|
|
A752M
|
A752M-93 (1998)
|
Specification for General Requirements for Wire Rods and Coarse Round Wire, Alloy Steel [Metric]
|
|
A752
|
A752-93 (1998)
|
Specification for General Requirements for Wire Rods and Coarse Round Wire, Alloy Steel
|
|
A764
|
A764-95
|
Specification for Metallic Coated Carbon Steel Wire, Coated at Size and Drawn to Size for Mechanical Springs
|
|
A805
|
A805-93 (1998)
|
Specification for Steel, Flat Wire, Carbon, Cold-Rolled
|
List of Articles - Knowledge Base |
|
|
|