Cross-reference tables for DIN aluminium wrought alloys: Part 1


Abstract:
Cross-reference tables between alphanumeric and numeric temper designations for wrought aluminum alloys according to DIN 1788 and DIN 1790 standard specifications are given in this article. It covers sheets and strips with thickness from 0,021 to 0,035mm and aluminium alloy wires.